Electroconductive resins and intermediates and electroconductive coated paper
Assignee: Dow Chemical Co
•
Filing: 1978-01-03
•
Granted: 1978-12-19
•
Expires: 1998-01-03
Abstract
Abstract This invention relates a relatively low molecular weight polystyrene having a narrow molecular weight distribution range in combination with a 1 to 3-aromatic hydrocarbon ring compound, chloromethylated derivatives thereof, quaternary amine derivatives of said chloromethylated derivatives and the use of such amines as electroconductive resins for the preparation of electroconductive coated papers useful for electrographic printing.
Inventors
- 👤 Joseph L. Garner
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-28 01:44
CPC Classifications
G; G03; G03G; G03G5/00; G03G5/10; G03G5/101; C; C09; C09D; C09D125/00; C09D125/02; C09D125/04; C09D125/06; C09D5/00; C09D5/24; Y; Y10; Y10T; Y10T428/00; Y10T428/27; Y10T428/273; Y10T428/277; Y10T428/31504; Y10T428/31855; Y10T428/3188; Y10T428/31895; Y10T428/31899; Y10T428/31902; Y10T428/31906
Claims Analysis
Total Claims: 10
Claim 1
Independent Claim
236 words
A process for producing an electroconductive coated paper comprising coating a copying paper base with about 0.1 to about 3 pounds of an electroconductive composition per 3,000 square feet per side of the copying paper base said electroconductive composition having been prepared by chloromethylating or bromomethylating a first composition which comprises, by weight, Component (A) from about 85 to about 95 parts of a polystyrene characterized by a weight average molecular weight, M w , of about 5,000 to about 45,000 and an average molecular weight distribution, M w /M n , of about 2 to about 6; and Component (B) from about 15 to about 5 parts of a cyclic hydrocarbon of from 9 to about 25 carbon atoms which may contain up to two hetero-oxygen atoms, comprising 1 to 3 benzoaromatic rings; thereby introducing chloromethyl or bromomethyl groups on about 70 to 90 percent of the aromatic rings of said first composition and obtaining as a result thereof a chloromethylated or bromomethylated second composition and thereafter reacting the second composition with a tertiary amine of the formula ##STR3## wherein --R 1 , --R 2 and --R 3 are independently --CH 2 CH 2 OH, --CH 2 CHOHCH 3 , --CH 2 CHOHCH 2 OH, alkyl, aryl, cycloalkyl or aralkyl, in an amount sufficient to convert at least about 90 percent of the chloromethyl or bromomethyl groups of the second composition to quaternary ammonium groups.
Claim 2
Dependent Claim
236 words
A process for producing an electroconductive coated paper comprising coating a copying paper base with about 0.1 to about 3 pounds of an electroconductive composition per 3,000 square feet per side of the copying paper base said electroconductive composition having been prepared by chloromethylating or bromomethylating a first composition which comprises, by weight, Component (A) from about 85 to about 95 parts of a polystyrene characterized by a weight average molecular weight, M w , of about 5,000 to about 45,000 and an average molecular weight distribution, M w /M n , of about 2 to about 6; and Component (B) from about 15 to about 5 parts of a cyclic hydrocarbon of from 9 to about 25 carbon atoms which may contain up to two hetero-oxygen atoms, comprising 1 to 3 benzoaromatic rings; thereby introducing chloromethyl or bromomethyl groups on about 70 to 90 percent of the aromatic rings of said first composition and obtaining as a result thereof a chloromethylated or bromomethylated second composition and thereafter reacting the second composition with a tertiary amine of the formula ##STR3## wherein --R 1 , --R 2 and --R 3 are independently --CH 2 CH 2 OH, --CH 2 CHOHCH 3 , --CH 2 CHOHCH 2 OH, alkyl, aryl, cycloalkyl or aralkyl, in an amount sufficient to convert at least about 90 percent of the chloromethyl or bromomethyl groups of the second composition to quaternary ammonium groups.
Claim 3
Dependent Claim
21 words
The process of claim 1 wherein Component B, prior to chloromethylation or bromomethylation of the first composition, is biphenyl or naphthalene.
Claim 4
Dependent Claim
29 words
The process of claim 2 wherein Component A, prior to chloromethylation or bromomethylation of the first composition, is characterized by a M w of about 10,000 to about 30,000.
Claim 5
Dependent Claim
37 words
The process of claim 3 wherein, prior to chloromethylation or bromomethylation, the first composition comprises about 88 to about 92 parts of Component A and about 8 to about 12 parts of Component B which is biphenyl.
Claim 6
Dependent Claim
58 words
The process of claim 1 wherein, prior to chloromethylation or bromomethylation of the first composition Component A is characterized by a M w of about 13,000 to about 21,000, a M w /M n of about 5, and Component B is biphenyl; and R 1 , R 2 and R 3 of the tertiary amine are methyl groups.
Claim 7
Dependent Claim
28 words
The process of claim 1 wherein M w /M n of Component A of the first composition prior to chloromethylation or bromomethylation is about 3 to about 5.
Claim 8
Dependent Claim
21 words
The process of claim 1 wherein R 1 , R 2 and R 3 of the tertiary amine are methyl groups.
Claim 9
Dependent Claim
11 words
The process of claim 1 wherein the tertiary amine is trimethylamine.
Claim 10
Dependent Claim
12 words
An electroconductive coated paper produced according to the process of claim 1.
References Cited (Backward Citations)
US4071666A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1981-12-18 | 1982-06-19 | 1982-12-19 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1985-12-18 | 1986-06-19 | 1986-12-19 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1989-12-18 | 1990-06-19 | 1990-12-19 | $7700.00 | Window Closed / Lapsed |