Abstract

Abstract A catalyst containing metallic copper, especially a low temperature shift catalyst containing also zinc oxide, is made from a corresponding catalyst precursor by reduction in two stages. In the first stage a steam and/or CO2-diluted reducing gas is used and in the second a more strongly reducing gas mixture such as ammonia synthesis gas or even 100% hydrogen. The resulting catalyst is substantially more active than one reduced according to previous one-stage steam-reduction practice and similar to catalyst made by the less convenient dry-reduction using nitrogen or natural gas as diluent.

Inventors

  • 👤 Paul Snowden

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-07 09:50
CPC Classifications
B; B01; B01J; B01J37/00; B01J37/16; B01J37/18; B01J23/00; B01J23/70; B01J23/76; B01J23/80; C; C01; C01B; C01B3/00; C01B3/02; C01B3/06; C01B3/12; C01B3/16; Y; Y02; Y02P; Y02P20/00; Y02P20/50; Y02P20/52

Claims Analysis

Total Claims: 7
Claim 1
Independent Claim 181 words
A method of making a catalyst containing active metallic copper from a corresponding catalyst precursor containing copper oxide and zinc oxide in which the molar ratio of zinc oxide to copper oxide is 0.5-3:1, which comprises treating at a temperature of 275° C. or less the precursor with a reducing gas mixture containing steam, carbon dioxide or steam and carbon dioxide totaling at least 50% v/v of the mixture and a reducing gas selected from the group consisting of hydrogen, carbon monoxide and compounds that react readily to give hydrogen and/or carbon oxides the content of reducing gas, calculated as equivalent hydrogen, being less than 3% v/v, until a substantial part of the copper oxide has been reduced to metallic copper and thereafter treating it at a temperature of 275° C. or less with a more strongly reducing gas mixture consisting essentially of a reducing gas selected from the group consisting of hydrogen, carbon monoxide and compounds that react readily to give hydrogen and/or carbon oxides and less than 25% by volume of steam, carbon dioxide or carbon dioxide and steam.
Claim 2
Independent Claim 181 words
A method of making a catalyst containing active metallic copper from a corresponding catalyst precursor containing copper oxide and zinc oxide in which the molar ratio of zinc oxide to copper oxide is 0.5-3:1, which comprises treating at a temperature of 275° C. or less the precursor with a reducing gas mixture containing steam, carbon dioxide or steam and carbon dioxide totaling at least 50% v/v of the mixture and a reducing gas selected from the group consisting of hydrogen, carbon monoxide and compounds that react readily to give hydrogen and/or carbon oxides the content of reducing gas, calculated as equivalent hydrogen, being less than 3% v/v, until a substantial part of the copper oxide has been reduced to metallic copper and thereafter treating it at a temperature of 275° C. or less with a more strongly reducing gas mixture consisting essentially of a reducing gas selected from the group consisting of hydrogen, carbon monoxide and compounds that react readily to give hydrogen and/or carbon oxides and less than 25% by volume of steam, carbon dioxide or carbon dioxide and steam.
Claim 3
Dependent Claim 78 words
A method according to claim 1 in which the catalyst precursor is present in an uncooled bed and the content of reducing gas, calculated as equivalent hydrogen, in the mixture with at least 50% v/v of steam and/or carbon dioxide is under 3% v/v at the start of reduction, is maintained or increased to 3-10% v/v as the reduction proceeds, and is controlled during the reduction so that the temperature does not exceed 275° C. in the bed.
Claim 4
Dependent Claim 24 words
A method according to claim 1 in which the more strongly reducing gas mixture contains less than 5% v/v of steam and carbon dioxide.
Claim 5
Dependent Claim 51 words
A method according to claim 1 in which the product of the first stage of reduction is cooled, dried and, if necessary, stabilised by dilute oxygen, to give a pre-reduced catalyst, and the second stage of reduction is carried out in the reactor in which the catalyst is to be used.
Claim 6
Dependent Claim 32 words
A method according to claim 1 in which the catalyst precursor additionally contains 2.5 to 20% of alumina or 2.5 to 30% w/w of chromium oxide as Cr 2 O 3 .
Claim 7
Dependent Claim 30 words
A method according to claim 1 wherein said compounds that react readily to give hydrogen and/or carbon oxides are selected from the group consisting of methanol, dimethylether, methylformate and ammonia.

References Cited (Backward Citations)

US3514261A Cited
US3390102A Cited
US3388972A Cited
US3546140A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1981-12-11 1982-06-12 1982-12-12 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1985-12-11 1986-06-12 1986-12-12 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1989-12-11 1990-06-12 1990-12-12 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag