Patent US4125465A successfully refreshed from Google Patents.
← Back to Patent Explorer
US4125465A Expired / Lapsed US ⏱️ 0.0 years remaining

Method of effluent sludge treatment

Assignee: Individual
•
Filing: 1976-10-18
•
Granted: 1978-11-14
•
Expires: 1996-10-18
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A method of treating effluent sludge, which comprises coagulating sludge with mineral coagulants, thereafter subjecting the sludge to mechanical dehydration. The dehydrated sludge is dried to a moisture content of from 10 to 50 percent with the aid of a gaseous heat carrier having an initial temperature of from 600° to 800° C under backflow and air-gushing conditions. Dried sludge is introduced into the raw sludge at the coagulation stage at a rate so as to provide for a concentration of the resultant sludge mixture of from 50 to 120 g/lit.

Inventors

  • 👤 Izrail S. Turovsky
  • 👤 Leonic L. Goldfarb
  • 👤 Leonid V. Zamoschin
  • 👤 Alexandr I. Zhukov

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-30 07:06
CPC Classifications
C; C02; C02F; C02F1/00; C02F1/52; C02F1/5236; C02F11/00; C02F11/12; C02F11/13

Claims Analysis

Total Claims: 7
Claim 1
Independent Claim 90 words
A method of treating effluent sludge, which comprises treating sludge with mineral coagulants so as to coagulate the sludge; mechanically dehydrating the resulting sludge; drying the dehydrated sludge to a moisture content of from 10 to 50 percent by means of a gaseous heat carrier having an initial temperature of from 600° to 800° C. under counter-jet and air-gushing conditions; introducing at the coagulation stage dried sludge into the starting sludge at a rate so that a concentration of the sludge mixture thus obtained is from 50 to 120 g/lit.
Claim 2
Independent Claim 90 words
A method of treating effluent sludge, which comprises treating sludge with mineral coagulants so as to coagulate the sludge; mechanically dehydrating the resulting sludge; drying the dehydrated sludge to a moisture content of from 10 to 50 percent by means of a gaseous heat carrier having an initial temperature of from 600° to 800° C. under counter-jet and air-gushing conditions; introducing at the coagulation stage dried sludge into the starting sludge at a rate so that a concentration of the sludge mixture thus obtained is from 50 to 120 g/lit.
Claim 3
Dependent Claim 31 words
A method as set forth in claim 1, wherein said dried sludge introduced into the starting sludge at the coagulation stage has a moisture content of from 10 to 30 percent.
Claim 4
Dependent Claim 56 words
A method as set forth in claim 1, wherein the starting sludge is divided into two portions; one portion of the starting sludge is coagulated with the aid of mineral coagulants, and the other portion of the starting sludge is coagulated with the aid of dried sludge obtained in the treatment of a former sludge portion,
Claim 5
Dependent Claim 38 words
A method as set forth in claim 1, wherein the starting sludge is coagulated alternately with the aid of mineral coagulants and dried sludge obtained in the treatment of the starting sludge with the aid of mineral coagulants.
Claim 6
Independent Claim 99 words
A method of effluent sludge treatment, which comprises treating sludge with at least one mineral coagulant selected from the group consisting of ferric chloride, ferric sulfate and calcium oxide; mechanically dehydrating the sludge; drying the dehydrated sludge to a moisture content of from 10 to 50 percent by means of a gaseous heat carrier having an initial temperature of from 600° to 800° C. under counter-jet and air-gushing conditions; introducing at the coagulation stage, dried sludge into the starting sludge at a rate so that the concentration of the sludge mixture thus obtained is from 50 to 120 g/lit.
Claim 7
Independent Claim 99 words
A method of effluent sludge treatment, which comprises treating sludge with at least one mineral coagulant selected from the group consisting of ferric chloride, ferric sulfate and calcium oxide; mechanically dehydrating the sludge; drying the dehydrated sludge to a moisture content of from 10 to 50 percent by means of a gaseous heat carrier having an initial temperature of from 600° to 800° C. under counter-jet and air-gushing conditions; introducing at the coagulation stage, dried sludge into the starting sludge at a rate so that the concentration of the sludge mixture thus obtained is from 50 to 120 g/lit.

References Cited (Backward Citations)

US3342731A Cited
US3440166A Cited
US3963470A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1981-11-13 1982-05-15 1982-11-14 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1985-11-13 1986-05-15 1986-11-14 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1989-11-13 1990-05-15 1990-11-14 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag