← Back to Patent Explorer
US4099117A Expired / Lapsed US ⏱️ 0.0 years remaining

Method and apparatus for measuring the quality of insulation on a buried pipeline and the quantity of metal oxide present at breaks in the insulation

Assignee: Individual
•
Filing: 1976-04-26
•
Granted: 1978-07-04
•
Expires: 1996-04-26
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract The invention disclosed comprises a method of and apparatus for inspecting a pipeline in situ. An alternating voltage is impressed between the pipeline and a ground bed. Spaced electrodes are positioned transverse the pipeline at spaced locations along the pipeline. At each location, the current flowing between the electrodes is used to indicate the condition of the coating on the pipeline. In one aspect of the invention, the current flowing between electrodes is obtained by measuring the resistance of the medium in which the pipeline is buried, such as the ground, and the voltage, and then dividing the voltage by the resistance. In another aspect of the invention, the ratio of the resistive and reactive components of the current flowing between the pipeline and the ground bed is used to indicate the quality of the pipeline coating. In yet another aspect of the invention, the third harmonic content of the voltage is measured to obtain an indication of the presence of iron oxide. The amount of third harmonic present when compared with current flow indicates the quantity of oxide.

Inventors

  • 👤 Louis W. Erath

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-25 16:57
CPC Classifications
G; G01; G01R; G01R31/00; G01N; G01N27/00; G01N27/02; G01N27/04; G01N27/20; G01N27/205

Claims Analysis

Total Claims: 16
Claim 1
Independent Claim 119 words
A method of inspecting in situ an externally coated metal pipeline that is buried in an electrically conductive medium, such as the ground, comprising connecting the pipeline to a source of alternating electrical voltage, connecting the voltage source to a ground bed located in the medium, and measuring along the pipeline the flow of electrical current through the medium between the ground bed and the pipeline to locate breaks in the coating of the pipeline by changes in the current flow, and measuring one of the harmonics in the signal that is produced by an oxide of the metal of the pipeline to obtain an indication of the amount of metal oxide formed at the break in the coating.
Claim 2
Independent Claim 119 words
A method of inspecting in situ an externally coated metal pipeline that is buried in an electrically conductive medium, such as the ground, comprising connecting the pipeline to a source of alternating electrical voltage, connecting the voltage source to a ground bed located in the medium, and measuring along the pipeline the flow of electrical current through the medium between the ground bed and the pipeline to locate breaks in the coating of the pipeline by changes in the current flow, and measuring one of the harmonics in the signal that is produced by an oxide of the metal of the pipeline to obtain an indication of the amount of metal oxide formed at the break in the coating.
Claim 3
Dependent Claim 27 words
The method of claim 1 in which the third harmonic is measured to obtain an indication of the iron oxide formed at the break in the coating.
Claim 4
Independent Claim 94 words
The method of determining the presence of a selected metal oxide formed on a buried pipeline comprising connecting the pipeline to a source of alternating voltage, filtering the harmonic from the alternating voltage that is produced by the selected metal oxide, connecting such source to a ground bed, and measuring the oxide produced harmonic content of the alternating voltage flowing through the ground between the pipeline and the ground bed at selected locations to obtain an indication of the presence of the selected metal oxide from the oxide produced harmonic content of the voltage.
Claim 5
Independent Claim 94 words
The method of determining the presence of a selected metal oxide formed on a buried pipeline comprising connecting the pipeline to a source of alternating voltage, filtering the harmonic from the alternating voltage that is produced by the selected metal oxide, connecting such source to a ground bed, and measuring the oxide produced harmonic content of the alternating voltage flowing through the ground between the pipeline and the ground bed at selected locations to obtain an indication of the presence of the selected metal oxide from the oxide produced harmonic content of the voltage.
Claim 6
Independent Claim 126 words
A method of inspecting an externally coated pipeline made of an iron containing metal that is buried in an electrically conductive medium, such as the ground, comprising connecting the pipeline to a source of alternating electrical voltage, connecting the voltage source to a ground bed located in the medium, and measuring the flow of electrical current through the medium between the ground bed and the pipeline along the path of the pipeline to locate breaks in the coating of the pipeline by changes in the current flow, and measuring the third harmonic content of the voltage that is produced by an oxide of the metal of the pipeline to obtain an indication of the amount of iron oxide present at each break located in the coating.
Claim 7
Independent Claim 126 words
A method of inspecting an externally coated pipeline made of an iron containing metal that is buried in an electrically conductive medium, such as the ground, comprising connecting the pipeline to a source of alternating electrical voltage, connecting the voltage source to a ground bed located in the medium, and measuring the flow of electrical current through the medium between the ground bed and the pipeline along the path of the pipeline to locate breaks in the coating of the pipeline by changes in the current flow, and measuring the third harmonic content of the voltage that is produced by an oxide of the metal of the pipeline to obtain an indication of the amount of iron oxide present at each break located in the coating.
Claim 8
Independent Claim 186 words
A method of inspecting for breaks in the external protective coating of a buried metal pipeline comprising connecting the pipeline at a selected point to a source of alternating electrical voltage, connecting the electrical voltage source to a ground bed spaced from the pipeline, inserting a plurality of spaced electrodes into the ground above the pipeline at spaced locations along a line transverse the longitudinal axis of the pipeline, and at each location measuring the resistivity of the ground between the electrodes, measuring the voltage between adjacent electrodes, calculating the current flow between adjacent electrodes from the ground resistivity and the voltage and comparing the current measured at each location to determine if the current flow at any location is such as would indicate a break in the coating adjacent such location, and measuring at each location one of the harmonics in signal that is produced by an oxide of the metal of the pipeline and comparing the value of such signal with the amount of current flow to get an indication of the amount of metal oxide formed at any break indicated in the coating.
Claim 9
Independent Claim 186 words
A method of inspecting for breaks in the external protective coating of a buried metal pipeline comprising connecting the pipeline at a selected point to a source of alternating electrical voltage, connecting the electrical voltage source to a ground bed spaced from the pipeline, inserting a plurality of spaced electrodes into the ground above the pipeline at spaced locations along a line transverse the longitudinal axis of the pipeline, and at each location measuring the resistivity of the ground between the electrodes, measuring the voltage between adjacent electrodes, calculating the current flow between adjacent electrodes from the ground resistivity and the voltage and comparing the current measured at each location to determine if the current flow at any location is such as would indicate a break in the coating adjacent such location, and measuring at each location one of the harmonics in signal that is produced by an oxide of the metal of the pipeline and comparing the value of such signal with the amount of current flow to get an indication of the amount of metal oxide formed at any break indicated in the coating.
Claim 10
Dependent Claim 25 words
The method of claim 5 in which the third harmonic frequency is measured to determine the amount of iron oxide formed at any break indicated.
Claim 11
Dependent Claim 164 words
Apparatus for inspecting in situ an externally coated pipeline made of an iron containing metal that is located in an electrically conductive medium such as the ground or along the bottom of the ocean, comprising a sinusoidal alternating electrical voltage connected between the pipeline and a ground bed in the medium, a plurality of electrodes spaced along a line transverse the direction of the longitudinal axis of the pipeline for positioning in the medium at selected locations along the direction of the pipeline, means for measuring the current flowing between the electrodes at each location to obtain indications of changes in resistance that indicate a break in the coating on the pipeline, means for detecting the voltage signal between two of said electrodes, and means for measuring the third harmonic component of said signal that is produced by iron oxide to determine the presence of iron oxide and for comparing the component with the current flow to indicate the amount of iron oxide present.
Claim 12
Dependent Claim 164 words
Apparatus for inspecting in situ an externally coated pipeline made of an iron containing metal that is located in an electrically conductive medium such as the ground or along the bottom of the ocean, comprising a sinusoidal alternating electrical voltage connected between the pipeline and a ground bed in the medium, a plurality of electrodes spaced along a line transverse the direction of the longitudinal axis of the pipeline for positioning in the medium at selected locations along the direction of the pipeline, means for measuring the current flowing between the electrodes at each location to obtain indications of changes in resistance that indicate a break in the coating on the pipeline, means for detecting the voltage signal between two of said electrodes, and means for measuring the third harmonic component of said signal that is produced by iron oxide to determine the presence of iron oxide and for comparing the component with the current flow to indicate the amount of iron oxide present.
Claim 13
Dependent Claim 73 words
The apparatus of claim 7 in which at least three electrodes are used with the center electrode located approximately over the pipeline and the means for measuring the amount of current flowing between each electrode includes means for placing a known voltage between the intermost electrodes, means for measuring the voltage between adjacent electrodes, and means for determining the resistance of the medium between adjacent electrodes based on the current flow and voltage.
Claim 14
Independent Claim 96 words
A method of inspecting the external coating of a pipeline buried in an electrically conductive medium comprising the steps of impressing an alternating voltage between the pipeline and ground, measuring the voltage between selected points in the medium along a line transverse the longitudinal axis of the pipeline, resolving the measured voltage into its resistive component and its reactive component, and obtaining a signal proportional to the ratio of the resistive component to the reactive component which indicates the quality of the external coating of the pipeline and is independent of the resistivity of the medium.
Claim 15
Independent Claim 96 words
A method of inspecting the external coating of a pipeline buried in an electrically conductive medium comprising the steps of impressing an alternating voltage between the pipeline and ground, measuring the voltage between selected points in the medium along a line transverse the longitudinal axis of the pipeline, resolving the measured voltage into its resistive component and its reactive component, and obtaining a signal proportional to the ratio of the resistive component to the reactive component which indicates the quality of the external coating of the pipeline and is independent of the resistivity of the medium.
Claim 16
Dependent Claim 41 words
The method of claim 9 further including measuring the harmonic content of the voltage that is produced by oxides of the metal of the pipeline to obtain an indication of the presence of and the quantity of oxide on the pipeline.

References Cited (Backward Citations)

US2378440A Cited
US3299351A Cited
US3526831A Cited
US3862491A Cited
US3792350A Cited
US3866117A Cited
US3991363A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1981-07-03 1982-01-02 1982-07-04 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1985-07-03 1986-01-02 1986-07-04 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1989-07-03 1990-01-02 1990-07-04 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag