Electrophotographic liquid developer containing a graft copolymer of a cyclized rubber

Assignee: Iwatsu Electric Co Ltd
•
Filing: 1976-05-20
•
Granted: 1978-04-18
•
Expires: 1996-05-20
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A liquid developer for use in preparing a printing plate for an offset duplicator is provided. The liquid developer comprises a dispersion of image-forming materials comprising finely divided colorant particles and an acrylic or methacrylic acid estergrafted cyclized rubber in a liquid carrier of a high electrical resistivity and a low dielectric constant.

Inventors

  • 👤 Syozo Adachi
  • 👤 Masato Tamori

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-02 08:36
CPC Classifications
G; G03; G03G; G03G9/00; G03G9/08; G03G9/12; G03G9/13; G03G9/133

Claims Analysis

Total Claims: 4
Claim 1
Independent Claim 264 words
A liquid developer for use in preparing a printing plate for an offset duplicator which comprises a dispersion of image-forming materials comprising finely divided colorant particles selected from a group consisting of dyes and pigments in a liquid carrier having an electrical resistivity of not less than 10 8 ohm-cm and a dielectric constant of not more than 3.0, said liquid carrier being at least one hydrocarbon selected from the group consisting of n-paraffinic hydrocarbons, iso-paraffinic hydrocarbons and their mixtures, characterized in that said image-forming material further comprises a graft copolymer of a cyclized rubber prepared from natural rubber onto which an ester of at least one acid selected from acrylic acid and methacrylic acid is grafted, said cyclized rubber having the recurring unit expressed by the structural formula ##STR3## wherein n is an integer such that said cyclized rubber has an average molecular weight of about 9,000 or greater and wherein said cyclized rubber has an average degree of cyclization in the range from about 20 to 80%, said ester being at least one compound selected from the group consisting of butyl acrylate, butyl methacrylate, 2-ethylhexyl acrylate, 2-ethylhexyl methacrylate, lauryl methacrylate, stearyl methacrylate, diethylaminoethyl acrylate and glycidyl methacrylate; and the amount of said graft copolymer being such that the ratio by weight of said graft copolymer to the colorant particles is within the range of 5/3 to 3/5, and the amounts of said ester and said cyclized rubber in the graft copolymer being 20 to 40% by weight and 60 to 80% by weight, respectively, based on the weight of the graft copolymer.
Claim 2
Dependent Claim 264 words
A liquid developer for use in preparing a printing plate for an offset duplicator which comprises a dispersion of image-forming materials comprising finely divided colorant particles selected from a group consisting of dyes and pigments in a liquid carrier having an electrical resistivity of not less than 10 8 ohm-cm and a dielectric constant of not more than 3.0, said liquid carrier being at least one hydrocarbon selected from the group consisting of n-paraffinic hydrocarbons, iso-paraffinic hydrocarbons and their mixtures, characterized in that said image-forming material further comprises a graft copolymer of a cyclized rubber prepared from natural rubber onto which an ester of at least one acid selected from acrylic acid and methacrylic acid is grafted, said cyclized rubber having the recurring unit expressed by the structural formula ##STR3## wherein n is an integer such that said cyclized rubber has an average molecular weight of about 9,000 or greater and wherein said cyclized rubber has an average degree of cyclization in the range from about 20 to 80%, said ester being at least one compound selected from the group consisting of butyl acrylate, butyl methacrylate, 2-ethylhexyl acrylate, 2-ethylhexyl methacrylate, lauryl methacrylate, stearyl methacrylate, diethylaminoethyl acrylate and glycidyl methacrylate; and the amount of said graft copolymer being such that the ratio by weight of said graft copolymer to the colorant particles is within the range of 5/3 to 3/5, and the amounts of said ester and said cyclized rubber in the graft copolymer being 20 to 40% by weight and 60 to 80% by weight, respectively, based on the weight of the graft copolymer.
Claim 3
Dependent Claim 41 words
A liquid developer according to claim 1 wherein said copolymer has a viscosity of V to Z 6 as measured in toluene at a temperature of 25° C and a concentration of 10% by weight by using a Gardner-Holdt bubble viscometer.
Claim 4
Dependent Claim 22 words
A liquid developer according to claim 1, wherein said average degree of cyclization of said cyclized rubber is from 40 to 60%.

References Cited (Backward Citations)

GB788651A Cited
GB797346A Cited
GB893429A Cited
US3432577A Cited
US3510338A Cited
US3629117A Cited
US3639243A Cited
US3639244A Cited
US3585140A Cited
US3640863A Cited
US3729418A Cited
US3657130A Cited
US3674693A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1981-04-17 1981-10-17 1982-04-18 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1985-04-17 1985-10-17 1986-04-18 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1989-04-17 1989-10-17 1990-04-18 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag