Abstract

Abstract In a process for preparing a pure phosphoric acid whereby phosphate rock is treated with sulfuric acid or hydrochloric acid to prepare a crude phosphoric acid, and wherein said crude acid is solvent extracted with an organic solvent to prepare an extracted aqueous phosphoric acid solution which is then concentrated, the improvement which comprises adding a fluorine compound to said extracted aqueous phosphoric acid solution, and concentrating the mixture under a reduced pressure and thereafter, contacting the concentrated phosphoric acid solution with steam or hot air.

Inventors

  • 👤 Itaru Toshimitsu
  • 👤 Sakumi Fujii
  • 👤 Masao Uchida
  • 👤 Yoshio Fujii

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-07 22:49
CPC Classifications
C; C01; C01B; C01B25/00; C01B25/16; C01B25/18; C01B25/234; C01B25/2343

Claims Analysis

Total Claims: 12
Claim 1
Independent Claim 203 words
In a process for preparing and purifying phosphoric acid whereby phosphate rock containing silica impurities is treated with sulfuric acid or hydrochloric acid to prepare a crude phosphoric acid containing silica, fluorine and chlorine impurities and wherein said crude acid is solvent extracted with an organic solvent to prepare an extracted aqueous phosphoric acid solution reduced in fluorine and silica impurites but whose residual fluorine/silicon content ratio is also decreased, which is then concentrated, the improvement which comprises: mixing a fluorine compound with said extracted aqueous phosphoric acid solution of a form such that it reacts with said SiO 2 in the extracted phosphoric acid solution and in an amount such that the atomic ratio of F/Si is greater than 4, thereby converting said silica to SiF 4 , and concentrating the mixture by evaporating water under a reduced pressure whereby significant quantities of Si, F and Cl impurities are vaporized; contacting the concentrated phosphoric acid solution with steam or hot air to vaporize the remaining Si, F and Cl impurities such that the concentration levels of Si, F and Cl remaining in the acid are less than 20 ppm, 5 ppm and 1 ppm, respectively, thereby obtaining a purified phosphoric acid solution.
Claim 2
Dependent Claim 203 words
In a process for preparing and purifying phosphoric acid whereby phosphate rock containing silica impurities is treated with sulfuric acid or hydrochloric acid to prepare a crude phosphoric acid containing silica, fluorine and chlorine impurities and wherein said crude acid is solvent extracted with an organic solvent to prepare an extracted aqueous phosphoric acid solution reduced in fluorine and silica impurites but whose residual fluorine/silicon content ratio is also decreased, which is then concentrated, the improvement which comprises: mixing a fluorine compound with said extracted aqueous phosphoric acid solution of a form such that it reacts with said SiO 2 in the extracted phosphoric acid solution and in an amount such that the atomic ratio of F/Si is greater than 4, thereby converting said silica to SiF 4 , and concentrating the mixture by evaporating water under a reduced pressure whereby significant quantities of Si, F and Cl impurities are vaporized; contacting the concentrated phosphoric acid solution with steam or hot air to vaporize the remaining Si, F and Cl impurities such that the concentration levels of Si, F and Cl remaining in the acid are less than 20 ppm, 5 ppm and 1 ppm, respectively, thereby obtaining a purified phosphoric acid solution.
Claim 3
Dependent Claim 33 words
The process of claim 1, wherein said extracted aqueous phosphoric acid solution contains 15-40% by weight of P 2 O 5 , and concentration is conducted under a pressure of less than-650 mmHg.
Claim 4
Dependent Claim 24 words
The process of claim 1, wherein said concentrated phosphoric acid is contacted with steam or hot air in a plate tower or packed tower.
Claim 5
Dependent Claim 18 words
The process of claim 3, wherein said plate is a bubble cap tower, or a sieve tray tower.
Claim 6
Dependent Claim 26 words
The process of claim 1, wherein the step of contacting steam or hot air with the phosphoric acid solution is performed in a multiple effect evaporator.
Claim 7
Dependent Claim 32 words
The process of claim 1, wherein said fluorine compound is added to said extracted aqueous phosphoric acid solution so as to give an atomic ratio of F/Si of 6-8 in said solution.
Claim 8
Dependent Claim 16 words
The process of claim 1, wherein the fluorine compound is hydrofluoric acid or a salt thereof.
Claim 9
Dependent Claim 35 words
The process of claim 1, wherein a small amount of the fluorine compound is added to said concentrated phosphoric acid solution to give an atomic ratio of F/Si of higher than 4 in said solution.
Claim 10
Dependent Claim 19 words
The process of claim 2, wherein the concentration of P 2 O 5 after the concentration step is 54-69%.
Claim 11
Dependent Claim 216 words
In a process for preparing and purifying phosphoric acid whereby phosphate rock containing silica impurities is treated with sulfuric acid or hydrochloric acid to prepare a crude phosphoric acid containing silica, fluorine and chlorine impurities, and wherein said crude acid is solvent extracted with an organic solvent to prepared an extracted aqueous phosphoric acid solution reduced in fluorine and silica impurities but whose residual fluorine/silicon content ratio is also decreased, which is then concentrated, the improvement which comprises: mixing a fluorine compound with said extracted aqueous phosphoric acid solution of a form such that it reacts with said SiO 2 in the extracted phosphoric acid solution and in an amount such that the atomic ratio of F/Si is 6-8 in said solution, thereby converting said silica to SiF 4 , and concentrating the mixture by evaporating water under a reduced pressure of -650 mmHg whereby significant quantities of Si, F and Cl impurities are vaporized; contacting the concentrated phosphoric acid solution with at least one of steam or hot air in a bubble cap tower to vaporize the remaining Si, F and Cl impurities such that the concentration levels of Si, F and Cl remaining in the acid are less than 20 ppm, 5 ppm, and 1 ppm, respectively thereby obtaining a purified phosphoric acid solution.
Claim 12
Dependent Claim 216 words
In a process for preparing and purifying phosphoric acid whereby phosphate rock containing silica impurities is treated with sulfuric acid or hydrochloric acid to prepare a crude phosphoric acid containing silica, fluorine and chlorine impurities, and wherein said crude acid is solvent extracted with an organic solvent to prepared an extracted aqueous phosphoric acid solution reduced in fluorine and silica impurities but whose residual fluorine/silicon content ratio is also decreased, which is then concentrated, the improvement which comprises: mixing a fluorine compound with said extracted aqueous phosphoric acid solution of a form such that it reacts with said SiO 2 in the extracted phosphoric acid solution and in an amount such that the atomic ratio of F/Si is 6-8 in said solution, thereby converting said silica to SiF 4 , and concentrating the mixture by evaporating water under a reduced pressure of -650 mmHg whereby significant quantities of Si, F and Cl impurities are vaporized; contacting the concentrated phosphoric acid solution with at least one of steam or hot air in a bubble cap tower to vaporize the remaining Si, F and Cl impurities such that the concentration levels of Si, F and Cl remaining in the acid are less than 20 ppm, 5 ppm, and 1 ppm, respectively thereby obtaining a purified phosphoric acid solution.

References Cited (Backward Citations)

US2165100A Cited
US2987376A Cited
US3386892A Cited
US3151941A Cited
US3193351A Cited
US3314756A Cited
US3366448A Cited
US3397123A Cited
US3544269A Cited
US3615195A Cited
US3723606A Cited
US3718729A Cited
US3764658A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1981-04-10 1981-10-10 1982-04-11 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1985-04-10 1985-10-10 1986-04-11 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1989-04-10 1989-10-10 1990-04-11 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag