Patent US4079158A successfully refreshed from Google Patents.
US4079158A
Expired / Lapsed
US
⏱️ 0.0 years remaining
Asphalt impregnated felt building materials
Assignee: Petro Canada Inc
•
Filing: 1975-10-07
•
Granted: 1978-03-14
•
Expires: 1995-10-07
Abstract
Abstract The disclosure describes asphalt saturated felt building materials, optionally having a mineral filled asphalt base coating thereon, in which the asphalt saturating the felt and/or the asphalt in any mineral filled coating is a blend of 10-55% sulfur dispersed in the asphalt. The materials are used in the conventional manner as roofing felt, roofing shingles, and in built-up roofing, to obtain improved fire resistance.
Inventors
- 👤 Gerhard J. A. Kennepohl
- 👤 Laverne J. Miller
- 👤 David C. Bean
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-05 17:29
CPC Classifications
D; D06; D06N; D06N5/00; E; E04; E04D; E04D5/00; E04D5/02; Y; Y10; Y10S; Y10S428/00; Y10S428/92; Y10S428/921; Y10T; Y10T428/00; Y10T428/24; Y10T428/24355; Y10T428/24372; Y10T428/2438; Y10T428/31504; Y10T428/31815; Y10T428/31819; Y10T428/31823; Y10T442/00; Y10T442/20; Y10T442/2762
Claims Analysis
Total Claims: 12
Claim 1
Independent Claim
104 words
A saturated felt building material comprising a web of paper felt, said web having been (1) saturated at a temperature in the range 240° F-350° F (115° C-176° C) in a uniform dispersed composition of from 10 to 55% sulfur dispersed in 90 to 45% saturant asphalt, with any of the sulfur in the composition which is not dissolved in the asphalt being dispersed as finely divided particles in the size range below 50 microns, then (2) pressed to remove saturant on the surface of the web and leave in the web residual saturant of at least 140% by weight of the unsaturated felt.
Claim 2
Dependent Claim
104 words
A saturated felt building material comprising a web of paper felt, said web having been (1) saturated at a temperature in the range 240° F-350° F (115° C-176° C) in a uniform dispersed composition of from 10 to 55% sulfur dispersed in 90 to 45% saturant asphalt, with any of the sulfur in the composition which is not dissolved in the asphalt being dispersed as finely divided particles in the size range below 50 microns, then (2) pressed to remove saturant on the surface of the web and leave in the web residual saturant of at least 140% by weight of the unsaturated felt.
Claim 3
Dependent Claim
25 words
A saturated felt building material as claimed in claim 1 in which the saturant is between 160 and 260% by weight of the unsaturated felt.
Claim 4
Dependent Claim
80 words
An asphalt roofing shingle comprising (1) felt backing saturated with an asphalt based saturant and (2) a mineral filler binder mixture coated thereon, the binder for the mineral filler being a uniform sulfur asphalt dispersed composition containing from 10 to 55% by weight of sulfur dispersed in 90 to 45% coating asphalt, with any of the sulfur in the composition which is not dissolved in the asphalt being dispersed as finely divided particles in the size range below 50 microns.
Claim 5
Dependent Claim
80 words
An asphalt roofing shingle comprising (1) felt backing saturated with an asphalt based saturant and (2) a mineral filler binder mixture coated thereon, the binder for the mineral filler being a uniform sulfur asphalt dispersed composition containing from 10 to 55% by weight of sulfur dispersed in 90 to 45% coating asphalt, with any of the sulfur in the composition which is not dissolved in the asphalt being dispersed as finely divided particles in the size range below 50 microns.
Claim 6
Dependent Claim
37 words
An asphalt roofing shingle as claimed in claim 3 in which the saturant in the felt is a uniform sulfur asphalt blend containing from 10 to 55% by weight of sulfur and 90 to 45% saturant asphalt.
Claim 7
Dependent Claim
22 words
An asphalt shingle as claimed in claim 3 in which the felt backing is a saturated felt as claimed in claim 1.
Claim 8
Dependent Claim
85 words
A saturated felt building material having an asphalt base saturant therein and optionally having a mineral filler asphalt base binder mixture coated thereon, wherein at least one of the asphalt base saturant in the felt and the asphalt base binder is a uniform dispersed composition of from 10 to 55% sulfur dispersed in 90 to 45% asphalt, with any of the sulfur in the composition which is not dissolved in the asphalt being dispersed as finely divided particles in the size range below 50 microns.
Claim 9
Dependent Claim
85 words
A saturated felt building material having an asphalt base saturant therein and optionally having a mineral filler asphalt base binder mixture coated thereon, wherein at least one of the asphalt base saturant in the felt and the asphalt base binder is a uniform dispersed composition of from 10 to 55% sulfur dispersed in 90 to 45% asphalt, with any of the sulfur in the composition which is not dissolved in the asphalt being dispersed as finely divided particles in the size range below 50 microns.
Claim 10
Dependent Claim
29 words
A saturated felt building material as claimed in claim 1 in which the dispersed composition contains between substantially 25 and 55% sulfur dispersed in substantially 75 to 45% asphalt.
Claim 11
Dependent Claim
28 words
An asphalt roofing shingle as claimed in claim 3, wherein the sulfur asphalt dispersed composition contains from 25 to 55% sulfur dispersed in 75 to 45% coating asphalt.
Claim 12
Dependent Claim
28 words
A saturated felt building material as claimed in claim 6 in which the uniform dispersed composition contains from 25 to 55% sulfur dispersed in 75 to 45% asphalt.
References Cited (Backward Citations)
US95576A
Cited
US256368A
Cited
US1026855A
Cited
US1264932A
Cited
US1765778A
Cited
US1846186A
Cited
US2804833A
Cited
US3810857A
Cited
US3738853A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1981-03-13 | 1981-09-12 | 1982-03-14 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1985-03-13 | 1985-09-12 | 1986-03-14 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1989-03-13 | 1989-09-12 | 1990-03-14 | $7700.00 | Window Closed / Lapsed |