US4071577A
Expired / Lapsed
US
⏱️ 0.0 years remaining
Toughened mercaptosiloxane modified emulsion polymerized vinylic polymers
Assignee: Dow Silicones Corp
•
Filing: 1976-04-23
•
Granted: 1978-01-31
•
Expires: 1996-04-23
Abstract
Abstract The impact strength of certain thermoplastic vinylic polymers is improved by polymerizing the corresponding monomers in an emulsion of a diorganosiloxane containing units of the formula HSR'SiR n O 3-n/2 . For example a styrene acrylonitrile copolymer containing 20 percent by weight of a dimethylsiloxane-3-mercaptopropylsiloxane copolymer having 1 mol percent mercaptosiloxane has an Izod notched impact strength of 10.8 foot pounds per inch.
Inventors
- 👤 James R. Falender
- 👤 Claudia M. Mettler
- 👤 John C. Saam
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-26 16:54
CPC Classifications
C; C08; C08F; C08F283/00; C08F283/12; C08F283/122
Claims Analysis
Total Claims: 8
Claim 1
Independent Claim
252 words
A thermoplastic vinylic polymer having improved impact strength made by the method which comprises polymerizing (1) a vinylic monomer selected from the group consisting of styrenic monomers, methyl methacrylate, mixtures of major amounts of styrenic monomers and minor amounts of monomers selected from the group consisting of acrylic monomers, alpha-methylstyrene, vinyl halide monomers, vinyl acetate, butadiene monomers and acrylonitrile monomers and mixtures of major amounts of methyl methacrylate and minor amounts of monomers selected from the group consisting of other acrylic monomers, styrenic monomers, butadiene monomers, vinyl halide monomers, vinyl acetate, alpha-methylstyrene, and acrylonitrile monomers, in an aqueous emulsion of (2) a copolymer of dimethylsiloxane, from 0.3 to 10 mol percent mercaptosiloxane of the unit formula HSR'SiR n O 3-n/2 in which R' is a divalent or trivalent saturated aliphatic hydrocarbon radical of 1 to 18 carbon atoms, two valences of R' being attached to the same silicon atom when R' is trivalent, R is a monovalent hydrocarbon radical free of aliphatic unsaturation of 1 to 6 carbon atoms and n is 0 to 2 and sufficient R"SiO 3/2 or SiO 2 units to give a percent volume swell of the copolymer of 500 to 1,600 percent in benzene, R" being of the group HSR'-- and R groups, in the presence of a free radical generator, whereby a thermoplastic matrix having dispersed therein particles of (2) is obtained, the proportions of (1) and (2) being from 1 to 40 percent by weight (2) based on the combined weights of (1) and (2).
Claim 2
Dependent Claim
252 words
A thermoplastic vinylic polymer having improved impact strength made by the method which comprises polymerizing (1) a vinylic monomer selected from the group consisting of styrenic monomers, methyl methacrylate, mixtures of major amounts of styrenic monomers and minor amounts of monomers selected from the group consisting of acrylic monomers, alpha-methylstyrene, vinyl halide monomers, vinyl acetate, butadiene monomers and acrylonitrile monomers and mixtures of major amounts of methyl methacrylate and minor amounts of monomers selected from the group consisting of other acrylic monomers, styrenic monomers, butadiene monomers, vinyl halide monomers, vinyl acetate, alpha-methylstyrene, and acrylonitrile monomers, in an aqueous emulsion of (2) a copolymer of dimethylsiloxane, from 0.3 to 10 mol percent mercaptosiloxane of the unit formula HSR'SiR n O 3-n/2 in which R' is a divalent or trivalent saturated aliphatic hydrocarbon radical of 1 to 18 carbon atoms, two valences of R' being attached to the same silicon atom when R' is trivalent, R is a monovalent hydrocarbon radical free of aliphatic unsaturation of 1 to 6 carbon atoms and n is 0 to 2 and sufficient R"SiO 3/2 or SiO 2 units to give a percent volume swell of the copolymer of 500 to 1,600 percent in benzene, R" being of the group HSR'-- and R groups, in the presence of a free radical generator, whereby a thermoplastic matrix having dispersed therein particles of (2) is obtained, the proportions of (1) and (2) being from 1 to 40 percent by weight (2) based on the combined weights of (1) and (2).
Claim 3
Dependent Claim
25 words
The polymer according to claim 1 in which (1) is a copolymer of styrene and acrylonitrile and (2) is a copolymer of dimethylsiloxane and mercaptopropylsiloxane.
Claim 4
Dependent Claim
28 words
The polymer in accordance with claim 2 in which (1) is a copolymer of styrene and acrylonitrile and (2) is a copolymer of dimethylsiloxane, mercaptopropylmethylsiloxane and ethyl orthosilicate.
Claim 5
Dependent Claim
13 words
The polymer in accordance with claim 1 in which (1) is methyl methacrylate.
Claim 6
Dependent Claim
12 words
The polymer in accordance with claim 1 in which (1) is styrene.
Claim 7
Dependent Claim
37 words
The polymer of claim 1 in which (1) is a copolymer of styrene and acrylonitrile and (2) is present in amount of 10 to 30 percent by weight based on the combined weights of (1) and (2).
Claim 8
Dependent Claim
28 words
The polymer of claim 5 in which (2) is present in amount of from 1 to 5 weight percent based on the combined weights of (1) and (2).
References Cited (Backward Citations)
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1981-01-30 | 1981-08-01 | 1982-01-31 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1985-01-30 | 1985-08-01 | 1986-01-31 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1989-01-30 | 1989-08-01 | 1990-01-31 | $7700.00 | Window Closed / Lapsed |