← Back to Patent Explorer
US4071577A Expired / Lapsed US ⏱️ 0.0 years remaining

Toughened mercaptosiloxane modified emulsion polymerized vinylic polymers

Assignee: Dow Silicones Corp
•
Filing: 1976-04-23
•
Granted: 1978-01-31
•
Expires: 1996-04-23
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract The impact strength of certain thermoplastic vinylic polymers is improved by polymerizing the corresponding monomers in an emulsion of a diorganosiloxane containing units of the formula HSR'SiR n O 3-n/2 . For example a styrene acrylonitrile copolymer containing 20 percent by weight of a dimethylsiloxane-3-mercaptopropylsiloxane copolymer having 1 mol percent mercaptosiloxane has an Izod notched impact strength of 10.8 foot pounds per inch.

Inventors

  • 👤 James R. Falender
  • 👤 Claudia M. Mettler
  • 👤 John C. Saam

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-26 09:51
CPC Classifications
C; C08; C08F; C08F283/00; C08F283/12; C08F283/122

Claims Analysis

Total Claims: 8
Claim 1
Independent Claim 252 words
A thermoplastic vinylic polymer having improved impact strength made by the method which comprises polymerizing (1) a vinylic monomer selected from the group consisting of styrenic monomers, methyl methacrylate, mixtures of major amounts of styrenic monomers and minor amounts of monomers selected from the group consisting of acrylic monomers, alpha-methylstyrene, vinyl halide monomers, vinyl acetate, butadiene monomers and acrylonitrile monomers and mixtures of major amounts of methyl methacrylate and minor amounts of monomers selected from the group consisting of other acrylic monomers, styrenic monomers, butadiene monomers, vinyl halide monomers, vinyl acetate, alpha-methylstyrene, and acrylonitrile monomers, in an aqueous emulsion of (2) a copolymer of dimethylsiloxane, from 0.3 to 10 mol percent mercaptosiloxane of the unit formula HSR'SiR n O 3-n/2 in which R' is a divalent or trivalent saturated aliphatic hydrocarbon radical of 1 to 18 carbon atoms, two valences of R' being attached to the same silicon atom when R' is trivalent, R is a monovalent hydrocarbon radical free of aliphatic unsaturation of 1 to 6 carbon atoms and n is 0 to 2 and sufficient R"SiO 3/2 or SiO 2 units to give a percent volume swell of the copolymer of 500 to 1,600 percent in benzene, R" being of the group HSR'-- and R groups, in the presence of a free radical generator, whereby a thermoplastic matrix having dispersed therein particles of (2) is obtained, the proportions of (1) and (2) being from 1 to 40 percent by weight (2) based on the combined weights of (1) and (2).
Claim 2
Dependent Claim 252 words
A thermoplastic vinylic polymer having improved impact strength made by the method which comprises polymerizing (1) a vinylic monomer selected from the group consisting of styrenic monomers, methyl methacrylate, mixtures of major amounts of styrenic monomers and minor amounts of monomers selected from the group consisting of acrylic monomers, alpha-methylstyrene, vinyl halide monomers, vinyl acetate, butadiene monomers and acrylonitrile monomers and mixtures of major amounts of methyl methacrylate and minor amounts of monomers selected from the group consisting of other acrylic monomers, styrenic monomers, butadiene monomers, vinyl halide monomers, vinyl acetate, alpha-methylstyrene, and acrylonitrile monomers, in an aqueous emulsion of (2) a copolymer of dimethylsiloxane, from 0.3 to 10 mol percent mercaptosiloxane of the unit formula HSR'SiR n O 3-n/2 in which R' is a divalent or trivalent saturated aliphatic hydrocarbon radical of 1 to 18 carbon atoms, two valences of R' being attached to the same silicon atom when R' is trivalent, R is a monovalent hydrocarbon radical free of aliphatic unsaturation of 1 to 6 carbon atoms and n is 0 to 2 and sufficient R"SiO 3/2 or SiO 2 units to give a percent volume swell of the copolymer of 500 to 1,600 percent in benzene, R" being of the group HSR'-- and R groups, in the presence of a free radical generator, whereby a thermoplastic matrix having dispersed therein particles of (2) is obtained, the proportions of (1) and (2) being from 1 to 40 percent by weight (2) based on the combined weights of (1) and (2).
Claim 3
Dependent Claim 25 words
The polymer according to claim 1 in which (1) is a copolymer of styrene and acrylonitrile and (2) is a copolymer of dimethylsiloxane and mercaptopropylsiloxane.
Claim 4
Dependent Claim 28 words
The polymer in accordance with claim 2 in which (1) is a copolymer of styrene and acrylonitrile and (2) is a copolymer of dimethylsiloxane, mercaptopropylmethylsiloxane and ethyl orthosilicate.
Claim 5
Dependent Claim 13 words
The polymer in accordance with claim 1 in which (1) is methyl methacrylate.
Claim 6
Dependent Claim 12 words
The polymer in accordance with claim 1 in which (1) is styrene.
Claim 7
Dependent Claim 37 words
The polymer of claim 1 in which (1) is a copolymer of styrene and acrylonitrile and (2) is present in amount of 10 to 30 percent by weight based on the combined weights of (1) and (2).
Claim 8
Dependent Claim 28 words
The polymer of claim 5 in which (2) is present in amount of from 1 to 5 weight percent based on the combined weights of (1) and (2).

References Cited (Backward Citations)

US2965593A Cited
US3382196A Cited
US3445415A Cited
US3532729A Cited
US3898300A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1981-01-30 1981-08-01 1982-01-31 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1985-01-30 1985-08-01 1986-01-31 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1989-01-30 1989-08-01 1990-01-31 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag