US4069053A Expired / Lapsed US ⏱️ 0.0 years remaining

Photographic films

Assignee: Konica Minolta Inc
•
Filing: 1977-03-31
•
Granted: 1978-01-17
•
Expires: 1997-03-31
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A photographic film comprising a plastic support having first and second layers therein in that order, the first layer comprising a cellulose acetate together with a matting agent composed mainly of silicon dioxide of less than 1 μ in particle size, the second layer comprising a phosphoric acid ester, or an amine salt thereof of a C 8 to C 22 -higher alkyl alcohol. A light-sensitive emulsion layer is carried on the other side of the support.

Inventors

  • 👤 Masayoshi Mayama
  • 👤 Tohru Kobayashi
  • 👤 Masahide Tamura

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-27 18:53
CPC Classifications
G; G03; G03C; G03C1/00; G03C1/76; G03C1/95; G03C1/85; G03C1/856; Y; Y10; Y10S; Y10S430/00; Y10S430/151

Claims Analysis

Total Claims: 12
Claim 1
Independent Claim 78 words
In a photographic film having a plastic support; a first layer comprising cellulose acetate and a matting agent comprising silicon dioxide less than 1μ in particle size; a second layer comprising a phosphoric acid ester of a C 8 to C 22 -higher alkyl alcohol, or an amine salt thereof, said first and second layers being carried in that order on one side of the support; and a light-sensitive emulsion layer on the other side of the support.
Claim 2
Dependent Claim 78 words
In a photographic film having a plastic support; a first layer comprising cellulose acetate and a matting agent comprising silicon dioxide less than 1μ in particle size; a second layer comprising a phosphoric acid ester of a C 8 to C 22 -higher alkyl alcohol, or an amine salt thereof, said first and second layers being carried in that order on one side of the support; and a light-sensitive emulsion layer on the other side of the support.
Claim 3
Dependent Claim 27 words
A photographic film as claimed in claim 1, wherein said matting agent further comprises up to 25% of at least one of aluminum oxide and magnesium oxide.
Claim 4
Dependent Claim 19 words
A photographic film as claimed in claim 2, wherein said silicon dioxide is modified by treatment with methyl chloride.
Claim 5
Dependent Claim 26 words
A photographic film as claimed in claim 1, wherein said first layer further comprises at least one of a plasticizer, a colorant or a defoaming agent.
Claim 6
Dependent Claim 26 words
A photographic film as claimed in claim 1, wherein said second layer further comprises at least one of a plasticizer, a colorant or a defoaming agent.
Claim 7
Dependent Claim 35 words
A photographic film as claimed in claim 1, wherein said emulsion layer is a light-sensitive gelatino-silver halide photographic emulsion layer and is coated on a sub layer applied to the other side of the support.
Claim 8
Dependent Claim 21 words
A photographic film as claimed in claim 1, wherein the plastic support is a film of cellulose triacetate or polyethylene terephthalate.
Claim 9
Dependent Claim 136 words
A photographic film which is stain-resistant to developing solutions containing an organic solvent, said film comprising a plastic support of cellulose triacetate or polyethylene terephthalate; a first layer comprising cellulose acetate in an amount of 10-500 mg. per square meter of the layer, and a matting agent of silicon dioxide less than 1μ in particle size in an amount of 0.1 to 0.5 part per part of cellulose acetate; a second layer comprising a phosphoric acid ester of a C 8 to C 22 -higher alkyl alcohol, or an amine salt thereof, in an amount of 6-20 mg. per square meter of said second layer, said first and second layers being carried in that order on one side of said support; and a light-sensitive gelatino-silver halide photographic emulsion layer on the other side of said support.
Claim 10
Dependent Claim 136 words
A photographic film which is stain-resistant to developing solutions containing an organic solvent, said film comprising a plastic support of cellulose triacetate or polyethylene terephthalate; a first layer comprising cellulose acetate in an amount of 10-500 mg. per square meter of the layer, and a matting agent of silicon dioxide less than 1μ in particle size in an amount of 0.1 to 0.5 part per part of cellulose acetate; a second layer comprising a phosphoric acid ester of a C 8 to C 22 -higher alkyl alcohol, or an amine salt thereof, in an amount of 6-20 mg. per square meter of said second layer, said first and second layers being carried in that order on one side of said support; and a light-sensitive gelatino-silver halide photographic emulsion layer on the other side of said support.
Claim 11
Independent Claim 144 words
A method of producing a photographic film which is stain-resistant to developing solutions containing an organic solvent, said method comprising forming a plastic support of cellulose triacetate or polyethylene terephthalate, depositing a first layer on one side of the support, said first layer comprising cellulose acetate in an amount of 10-500 mg. per square meter of the layer, and a matting agent of silicon dioxide less than 1μ in particle size in an amount of 0.1 to 0.5 part per part of cellulose acetate, depositing a second layer on the first layer, said second layer comprising a phosphoric acid ester of a C 8 to C 22 -higher alkyl alcohol, or an amine salt thereof, in an amount of 6-20 mg. per square meter of said second layer, and depositing a light-sensitive gelatino-silver halide photographic emulsion layer on the other side of said support.
Claim 12
Independent Claim 144 words
A method of producing a photographic film which is stain-resistant to developing solutions containing an organic solvent, said method comprising forming a plastic support of cellulose triacetate or polyethylene terephthalate, depositing a first layer on one side of the support, said first layer comprising cellulose acetate in an amount of 10-500 mg. per square meter of the layer, and a matting agent of silicon dioxide less than 1μ in particle size in an amount of 0.1 to 0.5 part per part of cellulose acetate, depositing a second layer on the first layer, said second layer comprising a phosphoric acid ester of a C 8 to C 22 -higher alkyl alcohol, or an amine salt thereof, in an amount of 6-20 mg. per square meter of said second layer, and depositing a light-sensitive gelatino-silver halide photographic emulsion layer on the other side of said support.

References Cited (Backward Citations)

US2801191A Cited
US3053662A Cited
US3159487A Cited
US3514291A Cited
US3525621A Cited
US3658573A Cited
US3630740A Cited
US3635714A Cited
US3656950A Cited
US3775124A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1981-01-16 1981-07-18 1982-01-17 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1985-01-16 1985-07-18 1986-01-17 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1989-01-16 1989-07-18 1990-01-17 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag