Abstract

Abstract A method of making toothed power transmission belting having preferably an elastomer-free sprocket-engaging toothed surface is described. A temperature sensitive tackifier is applied to a toothed mold surface and the belt face cover is stitched to the tacky surface, and then preferably further immobilized by winding tensile cord circumferentially about the mold. Elastomeric material is introduced into the tooth and body portions of the belt and the belting is cured. The temperature is elevated at some point during the process, whereby the tackifier loses its adherence to the mold, permitting easy demolding of the product.

Inventors

  • 👤 John D. Redmond, Jr.

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-29 17:10
CPC Classifications
B; B29; B29D; B29D29/00; B29D29/08

Claims Analysis

Total Claims: 14
Claim 1
Independent Claim 171 words
In the manufacture of power transmission belting having an elastomeric body and spaced teeth disposed along the inner surface thereof, the teeth including an outermost face cover portion, a method of affixing the face cover into intimate conformance to the surface of the teeth, comprising the steps of: a. applying a temperature sensitive tackifier, adherable to the face cover at the joining temperature under step b) and separable with respect to the face cover at a temperature elevated a predetermined amount above the joining temperature, directly or indirectly to the surface of a notched mold; b. stitchingly joining the face cover into conformance with the notched surface of the mold; c. disposing elastomeric material against the face cover and within the notches of the mold; d. elevating the temperature of the tackifier, either prior to or after step e), at least said predetermined amount above the joining temperature whereby the tackifier loses its tackiness and the face cover becomes readily movable with respect to the mold; and e. curing the belting.
Claim 2
Dependent Claim 171 words
In the manufacture of power transmission belting having an elastomeric body and spaced teeth disposed along the inner surface thereof, the teeth including an outermost face cover portion, a method of affixing the face cover into intimate conformance to the surface of the teeth, comprising the steps of: a. applying a temperature sensitive tackifier, adherable to the face cover at the joining temperature under step b) and separable with respect to the face cover at a temperature elevated a predetermined amount above the joining temperature, directly or indirectly to the surface of a notched mold; b. stitchingly joining the face cover into conformance with the notched surface of the mold; c. disposing elastomeric material against the face cover and within the notches of the mold; d. elevating the temperature of the tackifier, either prior to or after step e), at least said predetermined amount above the joining temperature whereby the tackifier loses its tackiness and the face cover becomes readily movable with respect to the mold; and e. curing the belting.
Claim 3
Dependent Claim 24 words
The method of claim 1 wherein the tackifier comprises a thermoplastic polymeric material having a melting point above the joining temperature under step b).
Claim 4
Dependent Claim 14 words
The method of claim 2 wherein the tackifier is disposed in a carrier solvent.
Claim 5
Dependent Claim 43 words
The method of claim 1 wherein the face cover is formed of a heat shrinkable material, and is joined to the surface of the notched mold in such a manner that excess face cover material is provided notches in the form of loops.
Claim 6
Dependent Claim 39 words
The method of claim 1 wherein step c) is accomplished by casting a liquid elastomeric within an annular cavity defined between the mold, wrapped with face cover, and an outwardly disposed mold shell spaced uniformly from the tensile band.
Claim 7
Dependent Claim 47 words
The method of claim 1 including the additional step, after step b) and prior to step c), of: positioning a tensile band generally transversely to the disposition of the notches of the mold and adjacent the face cover to substantially immobilize the face cover against the notches.
Claim 8
Dependent Claim 55 words
The method of claim 6 wherein subsequent to the step of positioning the tensile band but prior to step c), the perform comprising face cover and adjacently disposed tensile band are heated sufficiently to shrink the excess face cover material and conform it intimately against the land portions of the mold defined between the notches.
Claim 9
Dependent Claim 97 words
In a method of making toothed elastomeric power transmission belting having a body and teeth attached thereto and having a face cover formed on the outer surface of the teeth, the steps comprising: adhering the face cover to a notched mold surface with a temperature sensitive tackifier; applying a tensile member outwardly of the face cover and generally transversely of the notches of the mold; elevating the temperature of the tackifier sufficiently to break adherence between the face cover and notched mold surface; introducing elastomeric material into the mold and curing the belting into a unitary member.
Claim 10
Dependent Claim 97 words
In a method of making toothed elastomeric power transmission belting having a body and teeth attached thereto and having a face cover formed on the outer surface of the teeth, the steps comprising: adhering the face cover to a notched mold surface with a temperature sensitive tackifier; applying a tensile member outwardly of the face cover and generally transversely of the notches of the mold; elevating the temperature of the tackifier sufficiently to break adherence between the face cover and notched mold surface; introducing elastomeric material into the mold and curing the belting into a unitary member.
Claim 11
Dependent Claim 47 words
The method of claim 8 wherein the tackifier maintains tack and adheres the face cover and notched mold surface together through the step of introduction of elastomeric material, and yet loses tack at an elevated temperature which is below the temperature at which the belting is cured.
Claim 12
Independent Claim 93 words
A method for manufacturing toothed elastomeric power transmission belting having a body and teeth attached thereto, and having a face cover formed on the outer surface of the teeth and substantially free of the elastomer, comprising: bonding the face cover temporarily to a notched mold surface with a temperature sensitive tackifier; elevating the temperature of the tackifier, sufficiently to cause the bond between the face cover and notched mold surface to be at least partially broken; introducing elastomeric material into the notches of the mold and curing the belting into a unitary member.
Claim 13
Independent Claim 93 words
A method for manufacturing toothed elastomeric power transmission belting having a body and teeth attached thereto, and having a face cover formed on the outer surface of the teeth and substantially free of the elastomer, comprising: bonding the face cover temporarily to a notched mold surface with a temperature sensitive tackifier; elevating the temperature of the tackifier, sufficiently to cause the bond between the face cover and notched mold surface to be at least partially broken; introducing elastomeric material into the notches of the mold and curing the belting into a unitary member.
Claim 14
Dependent Claim 46 words
The method of claim 10 wherein the tackifier comprises a thermoplastic polymeric material dispersed in a solvent phase, and the bond between the face cover and mold is broken by heating the tackifier to cause solvent to flash off thereby reducing the tackiness of the tackifier.

References Cited (Backward Citations)

US3138962A Cited
US3418186A Cited
US3580767A Cited
US3897291A Cited
US3964328A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1981-01-02 1981-07-04 1982-01-03 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1985-01-02 1985-07-04 1986-01-03 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1989-01-02 1989-07-04 1990-01-03 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag