US4060888A
Expired / Lapsed
US
⏱️ 0.0 years remaining
Method of improving ohmic contact through high-resistance oxide film
Assignee: K & L MICROWAVE Inc A DE CORP
•
Filing: 1976-06-29
•
Granted: 1977-12-06
•
Expires: 1996-06-29
Abstract
Abstract A novel method is described for improving the ohmic contact through a relatively high electrical-resistance oxide film formed on at least one of two materials joined together to provide a low-resistance electrical junction. A current pulse of sufficient magnitude and duration is directed through the junction so that the oxide film breaks down and so that normal operating currents can then pass through the junction between the two materials.
Inventors
- 👤 Virgil E. Bottom
- 👤 Robert E. Christian
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-28 14:56
CPC Classifications
H; H01; H01R; H01R43/00; H01R43/02; Y; Y10; Y10T; Y10T29/00; Y10T29/42; Y10T29/49; Y10T29/49002; Y10T29/49117; Y10T29/49169
Claims Analysis
Total Claims: 7
Claim 1
Independent Claim
84 words
A method of making improved ohmic contact between at least one aluminum contact of a quartz crystal resonator and an electrically-conductive material comprising the steps of: forming an aluminum oxide coating on said aluminum contact; coupling a wire lead to said contact with said electrically-conductive material; and discharging a current pulse of a predetermined magnitude and duration through said electrically-conductive material and said aluminum oxide coating so as to form a low electrical resistance ohmic path between said aluminum contact and said electrically-conductive material.
Claim 2
Independent Claim
84 words
A method of making improved ohmic contact between at least one aluminum contact of a quartz crystal resonator and an electrically-conductive material comprising the steps of: forming an aluminum oxide coating on said aluminum contact; coupling a wire lead to said contact with said electrically-conductive material; and discharging a current pulse of a predetermined magnitude and duration through said electrically-conductive material and said aluminum oxide coating so as to form a low electrical resistance ohmic path between said aluminum contact and said electrically-conductive material.
Claim 3
Dependent Claim
35 words
A method in accordance with claim 1, wherein said electrically-conductive material is an electrically-conductive cement and said step of coupling includes the steps of cementing said wire lead to said contact and curing said cement.
Claim 4
Dependent Claim
40 words
A method in accordance with claim 1 wherein the step of discharging an electrical current pulse includes the steps of charging a capacitor with an electrical charge and discharging said capacitor through said electrically-conductive material and said aluminum oxide coating.
Claim 5
Dependent Claim
45 words
A method in accordance with claim 1 wherein said step of discharging a current pulse includes the steps of contacting either said electrically-conductive material or said aluminum contact with a needle like pointed end of an electrode and discharging said current pulse through said electrode.
Claim 6
Independent Claim
98 words
A method of making an improved ohmic contact through an aluminum oxide film formed between each aluminum contact of a quartz crystal resonator and a corresponding channeled end of a wire lead of an integrated base assembly supporting said resonator, said method comprising the steps of: mounting said resonator to said integrated base so that said resonator is received by and conductively secured to the channeled end of said wire lead; discharging a current pulse through said aluminum oxide film so as to form a low electrical resistance ohmic path between said aluminum contact and said wire lead.
Claim 7
Independent Claim
98 words
A method of making an improved ohmic contact through an aluminum oxide film formed between each aluminum contact of a quartz crystal resonator and a corresponding channeled end of a wire lead of an integrated base assembly supporting said resonator, said method comprising the steps of: mounting said resonator to said integrated base so that said resonator is received by and conductively secured to the channeled end of said wire lead; discharging a current pulse through said aluminum oxide film so as to form a low electrical resistance ohmic path between said aluminum contact and said wire lead.
References Cited (Backward Citations)
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1980-12-05 | 1981-06-06 | 1981-12-06 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1984-12-05 | 1985-06-06 | 1985-12-06 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1988-12-05 | 1989-06-06 | 1989-12-06 | $7700.00 | Window Closed / Lapsed |