Abstract

Abstract Disclosed are novel aminopolyamide-acrylamide-glyoxal resins useful as a sizing agent for paper having low water absorption, a desirable property for sized paper. The products are water dispersible and/or soluble and also find utility in printing inks, textile treatment and cosmetic or beauty aid compositions. The aminopolyamide is the condensation product of a polymeric fat acid and polyalkylene polyamine.

Inventors

  • 👤 Don E. Floyd
  • 👤 Demetri Potente

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-03 18:51
CPC Classifications
C; C08; C08G; C08G69/00; C08G69/48; D; D21; D21H; D21H17/00; D21H17/20; D21H17/33; D21H17/46; D21H17/54; D21H17/55

Claims Analysis

Total Claims: 10
Claim 1
Independent Claim 83 words
An aminopolyamide-acrylamide-glyoxal resin prepared by reacting a. a polymeric fat acid aminopolyamide having an amide number of about 150 to 600 b. an amount of an unsaturated amide sufficient to react with substantially all the amine groups in the aminopolyamide, said unsaturated amide having the formula ##STR3## where R'is hydrogen or an alkyl group containing up to 6 carbon atoms and c. reacting the resulting aminopolyamideunsaturated amide adduct with about 0.3 to 1.5 moles of glyoxal per amide group present in said adduct.
Claim 2
Dependent Claim 83 words
An aminopolyamide-acrylamide-glyoxal resin prepared by reacting a. a polymeric fat acid aminopolyamide having an amide number of about 150 to 600 b. an amount of an unsaturated amide sufficient to react with substantially all the amine groups in the aminopolyamide, said unsaturated amide having the formula ##STR3## where R'is hydrogen or an alkyl group containing up to 6 carbon atoms and c. reacting the resulting aminopolyamideunsaturated amide adduct with about 0.3 to 1.5 moles of glyoxal per amide group present in said adduct.
Claim 3
Dependent Claim 62 words
A resin as defined in claim 1 wherein said aminopolyamide is the reaction product at a temperature in the range of about 100 to 300° C. of a polymeric fat acid and a polyamine of the formula H.sub.2 NR(NHR).sub.ρ NH.sub.2 where R is an alkylene radical containing about 2 to 6 carbon atoms and p is a positive integer less than 6.
Claim 4
Dependent Claim 24 words
A resin as defined in claim 2 wherein said polymeric fat acid is a polymerized monocarboxylic aliphatic acid containing 16 to 20 carbon atoms.
Claim 5
Dependent Claim 20 words
A resin as defined in claim 2 wherein said polymerized fat acid is a polymerized C 18 monocarboxylic aliphatic acid.
Claim 6
Dependent Claim 18 words
A resin as defined in claim 2 wherein said polymeric fat acid is polymerized tall oil fatty acids.
Claim 7
Dependent Claim 13 words
A resin as defined in claim 1 wherein said unsaturated amide is acrylamide.
Claim 8
Dependent Claim 91 words
A process of preparing an aminopolyamide-acrylamide-polyaldehyde resin which comprises the steps of reacting a. a polymeric fat acid aminopolyamide having an amine number of about 150 to 600 b. an amount of an unsaturated amide sufficient to react with substantially all the amine groups in the aminopolyamide, said unsaturated amide having the formula ##STR4## where R' is hydrogen or an alkyl group containing up to 6 carbon atoms and c. reacting the resulting aminopolyamideunsaturated amide adduct with about 0.3 to 1.5 moles of glyoxal per amide group present in said adduct.
Claim 9
Dependent Claim 91 words
A process of preparing an aminopolyamide-acrylamide-polyaldehyde resin which comprises the steps of reacting a. a polymeric fat acid aminopolyamide having an amine number of about 150 to 600 b. an amount of an unsaturated amide sufficient to react with substantially all the amine groups in the aminopolyamide, said unsaturated amide having the formula ##STR4## where R' is hydrogen or an alkyl group containing up to 6 carbon atoms and c. reacting the resulting aminopolyamideunsaturated amide adduct with about 0.3 to 1.5 moles of glyoxal per amide group present in said adduct.
Claim 10
Dependent Claim 25 words
A sized paper treated with about 0.03 to 5 percent by weight based on the weight of paper of the resin defined in claim 1.

References Cited (Backward Citations)

US3127365A Cited
US3607622A Cited
US3728215A Cited
US3728214A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1980-11-28 1981-05-30 1981-11-29 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1984-11-28 1985-05-30 1985-11-29 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1988-11-28 1989-05-30 1989-11-29 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag