US4058883A Expired / Lapsed US ⏱️ 0.0 years remaining

Fabrication of panel structures having thin skin plate in vehicles, water craft, buildings, and the like

Assignee: Kawasaki Motors Ltd
•
Filing: 1976-01-22
•
Granted: 1977-11-22
•
Expires: 1996-01-22
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A panel structure is fabricated by stretching a skin plate with a tensile stress below the elastic limit stress thereof, securing this plate onto a framework with the plate under a constraining tensile stress and with portions thereof to which the constraining stress is not being fully applied being heated thereby to cause thermal expansion thereof, removing the constraining stress, and permitting the plate to cool and thereby to undergo thermal contraction and deformation, thereby producing tensile residual stress within the plate, whereby occurrence of welding deformations in the plate on the finished panel is prevented. Depending on the necessity, the skin plate may be prestretched with a stress exceeding the yield point thereof before the above described panel fabrication.

Inventors

  • 👤 Toshio Yoshida
  • 👤 Kiyoshi Terai
  • 👤 Shigetomo Matsui
  • 👤 Tsuneo Kinoshita
  • 👤 Akira Hoshi
  • 👤 Toru Tohmoto

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-05 17:48
CPC Classifications
B; B61; B61D; B61D17/00; B61D17/04; B61D17/12; B61D17/043; Y; Y10; Y10T; Y10T29/00; Y10T29/49; Y10T29/49826; Y10T29/49863; Y10T29/49867

Claims Analysis

Total Claims: 10
Claim 1
Independent Claim 164 words
A method of fabricating a panel structure of the type having a skeletal framework and a skin plate secured to the framework comprising the steps of: subjecting the skin plate to tensile stretching within the geometric surface thereof to produce a constraining tensile stress in the skin plate not exceeding the tensile elastic limit of the skin plate, the tensile stress being adequately applicable to at least a portion thereof; concurrently heating the skin plate locally at portions thereof to which the constraining tension cannot be adequately applied to a temperature above room temperature to induce thermal expansion of the skin plate within its geometric surface; welding the stressed and locally heated skin plate to the framework; simultaneously maintaining the stressed and heated condition of the skin plate; and thereafter releasing the skin plate from the tensile stretching and from the heating so as to leave a tensile residual stress in the skin plate to prevent undesirable deformation thereof in the fabricated panel structure.
Claim 2
Independent Claim 164 words
A method of fabricating a panel structure of the type having a skeletal framework and a skin plate secured to the framework comprising the steps of: subjecting the skin plate to tensile stretching within the geometric surface thereof to produce a constraining tensile stress in the skin plate not exceeding the tensile elastic limit of the skin plate, the tensile stress being adequately applicable to at least a portion thereof; concurrently heating the skin plate locally at portions thereof to which the constraining tension cannot be adequately applied to a temperature above room temperature to induce thermal expansion of the skin plate within its geometric surface; welding the stressed and locally heated skin plate to the framework; simultaneously maintaining the stressed and heated condition of the skin plate; and thereafter releasing the skin plate from the tensile stretching and from the heating so as to leave a tensile residual stress in the skin plate to prevent undesirable deformation thereof in the fabricated panel structure.
Claim 3
Dependent Claim 25 words
A method of fabricating a panel structure as set forth in claim 1 in which the heated portions are end parts of the skin plate.
Claim 4
Dependent Claim 24 words
A method of fabricating a panel structure as set forth in claim 1 in which the temperature is of the order of 100° C.
Claim 5
Dependent Claim 49 words
A method of fabricating a panel structure as set forth in claim 1, further comprising the step of overstretching the skin plate to apply thereto a tensile stress exceeding the tensile yield point stress thereof, prior to the step of subjecting the skin plate to tensile stretching and heating.
Claim 6
Independent Claim 170 words
A method of fabricating a panel structure of the type having a skeletal framework and a skin plate secured to the framework and having openings therein comprising the steps of: subjecting the skin plate to a tensile stretching within the geometric surface thereof to produce a constraining tensile stress in the skin plate not exceeding the tensile elastic limit of the skin plate, a complete tensile constraining distribution being obtainable in at least a portion thereof, concurrently heating the skin plate at portions thereof in which the complete tensile constraining stress distribution is not obtainable by the constraining tensile force, to a temperature above room temperature to induce thermal expansion of the skin plate within its geometric surface; welding the stressed and locally heated skin plate to the framework; simultaneously maintaining the stressed and heated condition; and thereafter releasing the skin plate from the tensile stretching and heating so as to leave a tensile residual stress in the skin plate to prevent undesirable deformation thereof in the fabricated panel structure.
Claim 7
Independent Claim 170 words
A method of fabricating a panel structure of the type having a skeletal framework and a skin plate secured to the framework and having openings therein comprising the steps of: subjecting the skin plate to a tensile stretching within the geometric surface thereof to produce a constraining tensile stress in the skin plate not exceeding the tensile elastic limit of the skin plate, a complete tensile constraining distribution being obtainable in at least a portion thereof, concurrently heating the skin plate at portions thereof in which the complete tensile constraining stress distribution is not obtainable by the constraining tensile force, to a temperature above room temperature to induce thermal expansion of the skin plate within its geometric surface; welding the stressed and locally heated skin plate to the framework; simultaneously maintaining the stressed and heated condition; and thereafter releasing the skin plate from the tensile stretching and heating so as to leave a tensile residual stress in the skin plate to prevent undesirable deformation thereof in the fabricated panel structure.
Claim 8
Dependent Claim 31 words
A method of fabricating a panel structure as set forth in claim 1 in which the heating is carried out by hot plates pressed against the surface of the skin plate.
Claim 9
Dependent Claim 26 words
A method of fabricating a panel structure as set forth in claim 1 in which the skin plate comprises a plurality of plate elements joined edge-to-edge.
Claim 10
Dependent Claim 23 words
A method of fabricating a panel structure as set forth in claim 1 in which the skin plate is a sheet of metal.

References Cited (Backward Citations)

US2110752A Cited
US2342025A Cited
US2441858A Cited
US2685263A Cited
US3082519A Cited
US3322190A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1980-11-21 1981-05-23 1981-11-22 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1984-11-21 1985-05-23 1985-11-22 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1988-11-21 1989-05-23 1989-11-22 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag