Patent US4053666A successfully refreshed from Google Patents.
US4053666A
Expired / Lapsed
US
⏱️ 0.0 years remaining
Recoverable, recyclable, and reusable composite container
Assignee: Graham Packaging Plastic Products Inc
•
Filing: 1975-01-16
•
Granted: 1977-10-11
•
Expires: 1995-01-16
Abstract
Abstract There is disclosed a glass based container having at least a portion of its external surface coated after the annealing of the glass with a protective, decorable, water removable, organic polymeric film which can be removed by an aqueous medium such that the annealed glass container base can be recovered, recycled, and reused.
Inventors
- 👤 Lynn J. Taylor
- 👤 Neal Troy
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-26 05:36
CPC Classifications
B; B65; B65D; B65D23/00; B65D23/08; B65D23/0807; B65D23/0814; C; C03; C03C; C03C17/00; C03C17/28; C03C17/32; C03C2218/00; C03C2218/30; C03C2218/355; Y; Y02; Y02W; Y02W30/00; Y02W30/50; Y02W30/80; Y10; Y10S; Y10S215/00; Y10S215/06; Y10T; Y10T428/00; Y10T428/13; Y10T428/131; Y10T428/1317; Y10T428/1321; Y10T428/24; Y10T428/24942; Y10T428/2495; Y10T428/249921; Y10T428/249953; Y10T428/249987; Y10T428/24999; Y10T428/26; Y10T428/263; Y10T428/269; Y10T428/31504; Y10T428/31551; Y10T428/31616; Y10T428/3162; Y10T428/31623; Y10T428/31634; Y10T428/31638; Y10T428/31645; Y10T428/31649
Claims Analysis
Total Claims: 14
Claim 1
Independent Claim
181 words
As an article of manufacture, a previously annealed glass container having at least a portion of its annealed, external surface coated with a protective, decorable film consisting essentially of a water removable, film-forming, thermoplastic organic polymer, said polymer being water soluble or dispersible and being selected from the group consisting of poly(ethylene oxide); poly(propylene oxide); ethylene oxide-propylene oxide copolymers; polyvinylpyrrolidinone; polyethyleneimine; poly(methyl vinyl ether); polyacrylamide; polymethacrylamide; poly(vinyl acetate); polyvinyl formal; poly(alkyl methacrylates); methyl cellulose; ethyl cellulose; hydroxyethyl cellulose; hydroxypropyl cellulose; sodium carboxymethyl cellulose; methyl hydroxypropyl cellulose; poly(acrylic acid) and salts thereof; poly(methacrylic acid) and salts thereof; ethylene-maleic anhydride copolymers; ethylene-vinyl alcohol copolymers, ethylene-acrylic acid copolymers; vinyl acetate-vinyl alcohol copolymers; methyl vinyl ether-maleic anhydride copolymers; and emulsifiable polyurethanes; said polymer being capable of removal by an aqueous medium such that the annealed glass container and polymer can be recovered, recycled, and reused, the film thickness being at least 0.002 inch and sufficient to provide scratch and shatter resistance for the container and to retain broken glass fragments upon fracture of the glass container so as to reduce the incidence of accidental injury.
Claim 2
Dependent Claim
181 words
As an article of manufacture, a previously annealed glass container having at least a portion of its annealed, external surface coated with a protective, decorable film consisting essentially of a water removable, film-forming, thermoplastic organic polymer, said polymer being water soluble or dispersible and being selected from the group consisting of poly(ethylene oxide); poly(propylene oxide); ethylene oxide-propylene oxide copolymers; polyvinylpyrrolidinone; polyethyleneimine; poly(methyl vinyl ether); polyacrylamide; polymethacrylamide; poly(vinyl acetate); polyvinyl formal; poly(alkyl methacrylates); methyl cellulose; ethyl cellulose; hydroxyethyl cellulose; hydroxypropyl cellulose; sodium carboxymethyl cellulose; methyl hydroxypropyl cellulose; poly(acrylic acid) and salts thereof; poly(methacrylic acid) and salts thereof; ethylene-maleic anhydride copolymers; ethylene-vinyl alcohol copolymers, ethylene-acrylic acid copolymers; vinyl acetate-vinyl alcohol copolymers; methyl vinyl ether-maleic anhydride copolymers; and emulsifiable polyurethanes; said polymer being capable of removal by an aqueous medium such that the annealed glass container and polymer can be recovered, recycled, and reused, the film thickness being at least 0.002 inch and sufficient to provide scratch and shatter resistance for the container and to retain broken glass fragments upon fracture of the glass container so as to reduce the incidence of accidental injury.
Claim 3
Dependent Claim
11 words
The invention of claim 1 wherein the polymer is water soluble.
Claim 4
Dependent Claim
11 words
The invention of claim 1 wherein the polymer is water dispersible.
Claim 5
Dependent Claim
18 words
The invention of claim 1 wherein the polymer is loaded with ingredients selected from fillers, pigments, and dyes.
Claim 6
Dependent Claim
13 words
The invention of claim 1 wherein the film has a foamed cellular structure.
Claim 7
Dependent Claim
189 words
In a process for the preparation of a coated glass container, the improvement which comprises applying a film consisting essentially of a water removable thermoplastic organic polymer which is water soluble or dispersible and is selected from the group consisting of poly(ethylene oxide); poly(propylene oxide); ethylene oxide-propylene oxide copolymers; polyvinyl-pyrrolidinone; polyethyleneimine; poly(methyl vinyl ether); polyacrylamide; polymethacrylamide; poly(vinyl acetate); polyvinyl formal; poly(alkyl methacrylates); methyl cellulose; ethyl cellulose; hydroxyethyl cellulose; hydroxypropyl cellulose; sodium carboxymethyl cellulose; methyl hydroxypropyl cellulose; poly(acrylic acid) and salts thereof; poly(methacrylic acid) and salts thereof; ethylene-maleic anhydride copolymers; ethylene-vinyl alcohol copolymers, ethylene-acrylic acid copolymers; vinyl acetate -vinyl alcohol copolymers; methyl vinyl ether-maleic anhydride copolymers; and emulsifiable polyurethanes; to at least a portion of the external surface of a previously annealed glass container, said film having a thickness of at least 0.002 inch and sufficient to provide scratch and shatter resistance for the container and to retain broken glass fragments upon fracture of the glass container so as to reduce the incidence of accidental injury, and being capable of removal by an aqueous medium such that the glass container and the coating film can be recovered, recycled, and reused.
Claim 8
Dependent Claim
189 words
In a process for the preparation of a coated glass container, the improvement which comprises applying a film consisting essentially of a water removable thermoplastic organic polymer which is water soluble or dispersible and is selected from the group consisting of poly(ethylene oxide); poly(propylene oxide); ethylene oxide-propylene oxide copolymers; polyvinyl-pyrrolidinone; polyethyleneimine; poly(methyl vinyl ether); polyacrylamide; polymethacrylamide; poly(vinyl acetate); polyvinyl formal; poly(alkyl methacrylates); methyl cellulose; ethyl cellulose; hydroxyethyl cellulose; hydroxypropyl cellulose; sodium carboxymethyl cellulose; methyl hydroxypropyl cellulose; poly(acrylic acid) and salts thereof; poly(methacrylic acid) and salts thereof; ethylene-maleic anhydride copolymers; ethylene-vinyl alcohol copolymers, ethylene-acrylic acid copolymers; vinyl acetate -vinyl alcohol copolymers; methyl vinyl ether-maleic anhydride copolymers; and emulsifiable polyurethanes; to at least a portion of the external surface of a previously annealed glass container, said film having a thickness of at least 0.002 inch and sufficient to provide scratch and shatter resistance for the container and to retain broken glass fragments upon fracture of the glass container so as to reduce the incidence of accidental injury, and being capable of removal by an aqueous medium such that the glass container and the coating film can be recovered, recycled, and reused.
Claim 9
Dependent Claim
11 words
The invention of claim 6 wherein the polymer is water soluble.
Claim 10
Dependent Claim
11 words
The invention of claim 6 wherein the polymer is water dispersible.
Claim 11
Dependent Claim
20 words
The invention of claim 6 wherein the polymer is loaded with ingredients selected from fillers, pigments, dyes, and blowing agents.
Claim 12
Dependent Claim
54 words
The invention of claim 6 wherein a liquid coating medium is applied to the surface of the container and subsequently dried, said coating medium consisting essentially of a solution or dispersion of 5% to 60% by weight of a water-removable film-forming thermoplastic organic polymer in 40% to 95% by weight of suitable volatile liquid.
Claim 13
Dependent Claim
30 words
The invention of claim 6 wherein the polymer is removed by an aqueous medium selected from water, aqueous acids, aqueous bases, aqueous salt solutions, and aqueous soap or surfactant solutions.
Claim 14
Dependent Claim
20 words
The invention of claim 6 wherein the polymer is removed by a mixture of water and a miscible organic solvent.
References Cited (Backward Citations)
US2761799A
Cited
US3379559A
Cited
US3554787A
Cited
US3498825A
Cited
US3549448A
Cited
US3604584A
Cited
US3577256A
Cited
US3698586A
Cited
US3760968A
Cited
US3868960A
Cited
US3889031A
Cited
US3919440A
Cited
US3920869A
Cited
US3922450A
Cited
US3937853A
Cited
US3922451A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1980-10-10 | 1981-04-11 | 1981-10-11 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1984-10-10 | 1985-04-11 | 1985-10-11 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1988-10-10 | 1989-04-11 | 1989-10-11 | $7700.00 | Window Closed / Lapsed |