Process for polymerizing diolefin copolymers employing a catalyst mixture of hydroperoxides
Assignee: Goodyear Tire and Rubber Co
•
Filing: 1976-06-01
•
Granted: 1977-10-04
•
Expires: 1996-06-01
Abstract
Abstract A method of producing a polymeric material comprised of polymerizing at least one unsaturated organic compound in an aqueous emulsion in the presence of a free radical generating redox catalyst comprised of a reducing component and an oxidizing component. Said oxidizing component is a composite prepared by (A) obtaining the oxidation product of reacting p-diisopropylbenzene with oxygen and (B) removing a major portion of resulting p-diisopropylbenzene hydroperoxide and unreacted monomers therefrom to effect a concentration of the remainder of the byproducts therein.
Inventors
- 👤 Howard K. Foley
- 👤 David A. Hutchings
- 👤 Terry C. Neubert
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-01 12:06
CPC Classifications
C; C08; C08F; C08F236/00; C08F236/02; C08F236/04; C08F236/10
Claims Analysis
Total Claims: 3
Claim 1
Independent Claim
253 words
In a method of producing a polymeric material comprised of polymerizing at least one unsaturated organic compound, selected from a mixture of 1,3-butadiene and styrene or a mixture of isoprene and styrene, in an aqueous emulsion in the presence of a free radical generating redox catalyst comprised of a reducing component and an oxidizing component, said oxidizing component is a composite prepared by (A) obtaining the oxidation product of reacting p-diisopropylbenzene with oxygen under relatively harsh temperature conditions at a temperature in the range of about 100° to about 120° C. comprised of a mixture of p-diisopropylbenzene hydroperoxide and byproducts comprised at least about 90 weight percent of phenols, enols and ketones, and unreacted p-diisopropylbenzene and (B) removing by separation a major portion of said p-diisopropylbenzene dihydroperoxide and unreacted p-diisopropylbenzene and a minor portion of said p-diisopropylbenzene hydroperoxide to effect a concentration of the remainder of the mixture as a distilland having an equivalent monohydroperoxide content by ASTM No. E-298-68 in the range of about 70 to about 90 percent comprised, by weight of about 45 to about 65 percent p-diisopropylbenzene monohydroperoxide about 5 to about 15 percent p-diisopropylbenzene dihydroperoxide and about 10 to about 30 percent said byproducts containing primarily phenols, enols and ketones, where said remainder distilland mixture is enhanced by (C) diluting with at least one alcohol selected from methanol, ethanol and isopropanol, to render the composite a free flowing liquid having hydroperoxide equivalent concentration according to ASTM No. E-298-68 in the range of about 40 to about 60 percent.
Claim 2
Dependent Claim
253 words
In a method of producing a polymeric material comprised of polymerizing at least one unsaturated organic compound, selected from a mixture of 1,3-butadiene and styrene or a mixture of isoprene and styrene, in an aqueous emulsion in the presence of a free radical generating redox catalyst comprised of a reducing component and an oxidizing component, said oxidizing component is a composite prepared by (A) obtaining the oxidation product of reacting p-diisopropylbenzene with oxygen under relatively harsh temperature conditions at a temperature in the range of about 100° to about 120° C. comprised of a mixture of p-diisopropylbenzene hydroperoxide and byproducts comprised at least about 90 weight percent of phenols, enols and ketones, and unreacted p-diisopropylbenzene and (B) removing by separation a major portion of said p-diisopropylbenzene dihydroperoxide and unreacted p-diisopropylbenzene and a minor portion of said p-diisopropylbenzene hydroperoxide to effect a concentration of the remainder of the mixture as a distilland having an equivalent monohydroperoxide content by ASTM No. E-298-68 in the range of about 70 to about 90 percent comprised, by weight of about 45 to about 65 percent p-diisopropylbenzene monohydroperoxide about 5 to about 15 percent p-diisopropylbenzene dihydroperoxide and about 10 to about 30 percent said byproducts containing primarily phenols, enols and ketones, where said remainder distilland mixture is enhanced by (C) diluting with at least one alcohol selected from methanol, ethanol and isopropanol, to render the composite a free flowing liquid having hydroperoxide equivalent concentration according to ASTM No. E-298-68 in the range of about 40 to about 60 percent.
Claim 3
Dependent Claim
64 words
The method of claim 1 where said p-diisopropylbenzene oxidation product is prepared by initially oxidizing p-diisopropylbenzene with oxygen at a temperature of about 112° ± 5° C., removing a major portion of said p-diisopropylbenzene diihydroperoxide by crystallization, removing a major portion of unreacted p-diisopropylbenzene and minor portion of said p-diisopropylbenzene monohydroxide by fractionation as a distillate and recovering said oxidizing component as a distilland.
References Cited (Backward Citations)
US3123590A
Cited
US2569506A
Cited
US2548435A
Cited
US2680138A
Cited
US2932628A
Cited
US3489730A
Cited
US3577376A
Cited
US3607807A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1980-10-03 | 1981-04-04 | 1981-10-04 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1984-10-03 | 1985-04-04 | 1985-10-04 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1988-10-03 | 1989-04-04 | 1989-10-04 | $7700.00 | Window Closed / Lapsed |