Patent US4376565A successfully refreshed from Google Patents.
Patent US4051282A successfully refreshed from Google Patents.
← Back to Patent Explorer
US4051282A Expired / Lapsed US ⏱️ 0.0 years remaining

Production of treated wood having easy penetrability

Assignee: Hickson Corp
•
Filing: 1976-06-14
•
Granted: 1977-09-27
•
Expires: 1996-06-14
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract Production of treated wood with improved penetrability by projectiles is accomplished in an improved pressure treatment with an improved treating solution. The wood is impregnated in a pressure treatment process with a treating solution containing an impregnant, an aliphatic hydrocarbon or halogenated hydrocarbon liquid carrier, a cosolvent if the solubility of the impregnant in the liquid carrier is inadequate, and an effective amount of lubricating oil. After the treating solution has impregnated the wood, the liquid carrier is evaporated leaving treated wood containing an impregnant with internal lubrication due to the oil and possibly some cosolvent.

Inventors

  • 👤 Dan L. Davies

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-24 05:13
CPC Classifications
B; B27; B27K; B27K3/00; B27K3/34; B27K3/50; B27K3/02; B27K3/08; B27K3/36; B27K3/38; B27K3/40; B27K3/44; B27K3/48; B27K2240/00; B27K2240/30

Claims Analysis

Total Claims: 13
Claim 1
Independent Claim 150 words
In a pressure treating process for wood wherein wood is impregnated with a treating solution containing one or more impregnants selected from the group of preservatives and fire retardants and a liquid carrier selected from the group consisting of aliphatic hydrocarbons and halogenated aliphatic hydrocarbons that are liquids at elevated pressures and that have boiling points below 130° C. at atmospheric pressure and wherein the impregnated wood is treated to evaporate the liquid carrier, the improvement which comprises: adding to the treating solution an effective lubricating amount of an oil having a kinematic viscosity of not less than 2.5 centistokes at 100° F. and not more than 5.8 centistokes at 100° F. and having a distillation range such that not more than about 50 percent of the volume distills below or about 450° F. and not more than about 90 percent of the volume distills below or about 550° F.
Claim 2
Dependent Claim 150 words
In a pressure treating process for wood wherein wood is impregnated with a treating solution containing one or more impregnants selected from the group of preservatives and fire retardants and a liquid carrier selected from the group consisting of aliphatic hydrocarbons and halogenated aliphatic hydrocarbons that are liquids at elevated pressures and that have boiling points below 130° C. at atmospheric pressure and wherein the impregnated wood is treated to evaporate the liquid carrier, the improvement which comprises: adding to the treating solution an effective lubricating amount of an oil having a kinematic viscosity of not less than 2.5 centistokes at 100° F. and not more than 5.8 centistokes at 100° F. and having a distillation range such that not more than about 50 percent of the volume distills below or about 450° F. and not more than about 90 percent of the volume distills below or about 550° F.
Claim 3
Dependent Claim 32 words
Process according to claim 1 wherein an amount of oil in the range of around 1.5 percent to around 15 percent of the total treating solution is added to the treating solution.
Claim 4
Dependent Claim 46 words
Process according to claim 1 wherein the aliphatic hydrocarbon is selected from the group consisting of propane, n-butane, isobutane, and mixtures thereof and the impregnant is one or more preservatives selected from the group consisting of polychlorinated phenols, copper quinolinolate, tributyl tin oxide and copper naphthenate.
Claim 5
Dependent Claim 36 words
Process according to claim 1 wherein a cosolvent in which the impregnant is substantially soluble and which is substantially soluble in the liquid carrier is used to aid in solubilizing the impregnant in the liquid carrier.
Claim 6
Dependent Claim 13 words
Process according to claim 1 wherein the halogenated aliphatic hydrocarbon is methylene chloride.
Claim 7
Dependent Claim 14 words
Process according to claim 1 wherein the oil is a No. 2 fuel oil.
Claim 8
Dependent Claim 232 words
In a process for the impregnation of wood with a liquid preservative comprising: A. immersing the wood in a treating solution at pressures above ambient pressure, 1. said treating solution comprising: a. an aliphatic hydrocarbon which is selected from the group consisting of propane, n-butane, isobutane, n-pentane, isopentane, and mixtures thereof and which is in the liquid state; b. a preservative selected from the group consisting of copper quinolinolate and pentachlorophenol; and c. a cosolvent, differing in its molecular structure from said aliphatic hydrocarbon, that has less than 10% water solubility, that has at least 25% solubility for the preservative, and that is soluble in the hydrocarbon to form a treating solution containing at least 2% by weight preservative, said treating solution containing at least 2% by weight of said cosolvent. B. separating said treating solution from the wood, and C. evaporating the aliphatic hydrocarbon from the impregnated wood autogenously whereby the preservative remains in the wood, the improvement comprising: adding to said treating solution an effective lubricating amount of an oil having a kinematic viscosity of not less than 2.5 centistokes at 100° F. and not more than 5.8 centistokes at 100° F. and having a distillation range such that not more than about 50 percent of the volume distills below or about 450° F. and not more than about 90 percent of the volume distills below or about 550° F.
Claim 9
Dependent Claim 232 words
In a process for the impregnation of wood with a liquid preservative comprising: A. immersing the wood in a treating solution at pressures above ambient pressure, 1. said treating solution comprising: a. an aliphatic hydrocarbon which is selected from the group consisting of propane, n-butane, isobutane, n-pentane, isopentane, and mixtures thereof and which is in the liquid state; b. a preservative selected from the group consisting of copper quinolinolate and pentachlorophenol; and c. a cosolvent, differing in its molecular structure from said aliphatic hydrocarbon, that has less than 10% water solubility, that has at least 25% solubility for the preservative, and that is soluble in the hydrocarbon to form a treating solution containing at least 2% by weight preservative, said treating solution containing at least 2% by weight of said cosolvent. B. separating said treating solution from the wood, and C. evaporating the aliphatic hydrocarbon from the impregnated wood autogenously whereby the preservative remains in the wood, the improvement comprising: adding to said treating solution an effective lubricating amount of an oil having a kinematic viscosity of not less than 2.5 centistokes at 100° F. and not more than 5.8 centistokes at 100° F. and having a distillation range such that not more than about 50 percent of the volume distills below or about 450° F. and not more than about 90 percent of the volume distills below or about 550° F.
Claim 10
Dependent Claim 29 words
Process according to claim 5 wherein the effective lubricating amount of oil is in the range of around 1.5 percent to around 15 percent of the total treating solution.
Claim 11
Dependent Claim 128 words
An improved wood treating solution useful in pressurized wood treating processes wherein the treating solution containing pentachlorophenol, isopropyl ether, and liquefied petroleum gas impregnates the wood, and the liquefied petroleum gas is evaporated from the treated wood, the improvement comprising: having a treating solution containing: 2 to 7.5 percent pentachlorophenol, 3 to 12 percent isopropyl ether, 65 to 93 percent liquefied petroleum gas, and 1.5 to 15 percent of an oil having a kinematic viscosity of not less than 2.5 centistokes at 100° F. and not more than 5.8 centistokes at 100° F. and having a distillation range such that about 50 percent of the volume distills below or about 450° F. and not more than about 90 percent of the volume distills below or about 550° F.
Claim 12
Dependent Claim 128 words
An improved wood treating solution useful in pressurized wood treating processes wherein the treating solution containing pentachlorophenol, isopropyl ether, and liquefied petroleum gas impregnates the wood, and the liquefied petroleum gas is evaporated from the treated wood, the improvement comprising: having a treating solution containing: 2 to 7.5 percent pentachlorophenol, 3 to 12 percent isopropyl ether, 65 to 93 percent liquefied petroleum gas, and 1.5 to 15 percent of an oil having a kinematic viscosity of not less than 2.5 centistokes at 100° F. and not more than 5.8 centistokes at 100° F. and having a distillation range such that about 50 percent of the volume distills below or about 450° F. and not more than about 90 percent of the volume distills below or about 550° F.
Claim 13
Dependent Claim 15 words
An improved treating solution of claim 9 wherein the oil is No. 2 fuel oil.

References Cited (Backward Citations)

GB228119A Cited
US2799597A Cited
US3200003A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1980-09-26 1981-03-28 1981-09-27 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1984-09-26 1985-03-28 1985-09-27 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1988-09-26 1989-03-28 1989-09-27 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag