Abstract

Abstract An image forming process which comprises image-wise exposing a photosensitive material to light, the photosensitive material comprising a support and a substrate with a photopolymerizable material therebetween, and stripping off the support to leave either exposed areas or non-exposed areas of the photopolymerizable material on the substrate, in which the photopolymerizable material is characterized by comprising at least two different photopolymerizable layers which each comprise one or more addition polymerizable monomers, one or more photopolymerization initiators and one or more binders, which photopolymerizable layers are placed adjacent the support and the substrate, wherein at least one of the ingredients or the ratio of the ingredients of the photopolymerizable layers is different in at least the two different photopolymerizable layers, and the photopolymerizable layers have the relationship of C>A>B and C'>B'>A' or C>B>A and C'>A'>B', wherein: A is the adhesive strength between the support and the photopolymerizable layer adjacent thereto; B is the adhesive strength between the substrate and the photopolymerizable layer adjacent thereto; C is the lowest adhesive strength of all the adhesive strengthes between any two photopolymerizable layers among the layers, A' is the adhesive strength between the support and the photopolymerizable layer adjacent thereto after exposure to light, B' is the adhesive strength between the substrate and the photopolymerizable layer adjacent thereto after exposure to light, and C' is the lowest adhesive strength of all the adhesive strengths between any two photopolymerizable layers among the photopolymerizable layers after exposure to light.

Inventors

  • 👤 Keiji Takeda
  • 👤 Masataka Murata
  • 👤 Teppei Ikeda

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-26 00:05
CPC Classifications
G; G03; G03F; G03F7/00; G03F7/004; G03F7/09; G03F7/095; G03F7/0955; H; H05; H05K; H05K3/00; H05K3/0073; H05K3/02; H05K3/06; H05K3/061; H05K3/064

Claims Analysis

Total Claims: 28
Claim 1
Independent Claim 316 words
An image forming process which comprises image-wise exposing a photosensitive material to light, the photosensitive material comprising a support and a substrate with a photopolymerizable material therebetween, where either or both of the support or substrate is transparent and image-wise exposing is through the transparent support and/or substrate, and stripping off the support to leave either exposed areas or non-exposed areas of the photopolymerizable material on the substrate, in which the photopolymerizable material is characterized by comprising at least two different photopolymerizable layers which each comprise one or more addition polymerizable monomers, one or more photopolymerization initiators and one or more binders, which photopolymerizable layers are placed adjacent the transparent support and the substrate, wherein at least one of the ingredients or the ratio of the ingredients of the photopolymerizable layers is different in at least the two different photopolymerizable layers, and the photopolymerizable layers have the relationship of C>A>B and C'>B'>A' or C>B>A and C'>A'>B', wherein: A is the adhesive strength between the support and the photopolymerizable layer adjacent thereto; B is the adhesive strength between the substrate and the photopolymerizable layer adjacent thereto; C is the lowest adhesive strength of all the adhesive strengths between any two photopolymerizable layers among the layers, A' is the adhesive strength between the support and the photopolymerizable layer adjacent thereto after exposure to light, B' is the adhesive strength between the substrate and the photopolymerizable layer adjacent thereto after exposure to light, and C' is the lowest adhesive strength of all the adhesive strengths between any two photopolymerizable layers among the photopolymerizable layers after exposure to light, whereby following image-wise exposure and delamination cohesive failure occurs either (i) at the interface of the support and the photopolymerizable layer adjacent thereto or (ii) at the interface of the substrate and the photopolymerizable layer adjacent thereto, thereby providing negative and positive images in complimentary relationship in accordance with the following:
Claim 2
Dependent Claim 316 words
An image forming process which comprises image-wise exposing a photosensitive material to light, the photosensitive material comprising a support and a substrate with a photopolymerizable material therebetween, where either or both of the support or substrate is transparent and image-wise exposing is through the transparent support and/or substrate, and stripping off the support to leave either exposed areas or non-exposed areas of the photopolymerizable material on the substrate, in which the photopolymerizable material is characterized by comprising at least two different photopolymerizable layers which each comprise one or more addition polymerizable monomers, one or more photopolymerization initiators and one or more binders, which photopolymerizable layers are placed adjacent the transparent support and the substrate, wherein at least one of the ingredients or the ratio of the ingredients of the photopolymerizable layers is different in at least the two different photopolymerizable layers, and the photopolymerizable layers have the relationship of C>A>B and C'>B'>A' or C>B>A and C'>A'>B', wherein: A is the adhesive strength between the support and the photopolymerizable layer adjacent thereto; B is the adhesive strength between the substrate and the photopolymerizable layer adjacent thereto; C is the lowest adhesive strength of all the adhesive strengths between any two photopolymerizable layers among the layers, A' is the adhesive strength between the support and the photopolymerizable layer adjacent thereto after exposure to light, B' is the adhesive strength between the substrate and the photopolymerizable layer adjacent thereto after exposure to light, and C' is the lowest adhesive strength of all the adhesive strengths between any two photopolymerizable layers among the photopolymerizable layers after exposure to light, whereby following image-wise exposure and delamination cohesive failure occurs either (i) at the interface of the support and the photopolymerizable layer adjacent thereto or (ii) at the interface of the substrate and the photopolymerizable layer adjacent thereto, thereby providing negative and positive images in complimentary relationship in accordance with the following:
Claim 3
Dependent Claim 106 words
In the case of cohesive failure as described at (i), the substrate carrying the layer of the photopolymerizable composition adjacent thereto and areas of the photopolymerizable composition originally on the support in correspondence to the image-wise exposure, with the support carrying a complementary image of the photopolymerizable composition originally on the support; or 2. In the case of cohesive failure as described at (ii), the support carrying the layer of the photopolymerizable composition adjacent thereto and areas of the photopolymerizable composition originally on the substrate in correspondence to the image-wise exposure, with the substrate carrying a complementary image of the photopolymerizable composition originally on the substrate.
Claim 4
Dependent Claim 106 words
In the case of cohesive failure as described at (i), the substrate carrying the layer of the photopolymerizable composition adjacent thereto and areas of the photopolymerizable composition originally on the support in correspondence to the image-wise exposure, with the support carrying a complementary image of the photopolymerizable composition originally on the support; or 2. In the case of cohesive failure as described at (ii), the support carrying the layer of the photopolymerizable composition adjacent thereto and areas of the photopolymerizable composition originally on the substrate in correspondence to the image-wise exposure, with the substrate carrying a complementary image of the photopolymerizable composition originally on the substrate.
Claim 5
Dependent Claim 13 words
The process of claim 1, wherein said substrate is a printed circuit substrate.
Claim 6
Dependent Claim 9 words
The process of claim 2, wherein substrate has through-holes.
Claim 7
Dependent Claim 24 words
The process of claim 2, wherein exposed areas remain on the substrate and unexposed areas are removed together with the support from the substrate.
Claim 8
Dependent Claim 12 words
The process of claim 2, wherein said substrate comprises a copper-plastic laminate.
Claim 9
Dependent Claim 12 words
The process of claim 2, wherein said substrate comprises a flexible film.
Claim 10
Dependent Claim 20 words
The process of claim 1, wherein a photopolymerizable layer adjacent the substrate or adjacent the support comprises a chlorinated polyolefin.
Claim 11
Dependent Claim 22 words
The process of claim 7, wherein the chlorinated polyolefin comprises at least 30 weight % of the total binder in that layer.
Claim 12
Dependent Claim 22 words
The process of claim 8, wherein the chlorinated polyolefin comprises at least 50 weight % of the total binder in that layer.
Claim 13
Dependent Claim 55 words
The process of claim 8, wherein one photopolymerizable layer is adjacent the support and wherein one photopolymerizable layer is adjacent the substrate and further wherein at least one additional photopolymerizable layer is intermediate said first two recited layers, which intermediate layer has a molecular weight of more than about 10,000 but less than about 5,000,000.
Claim 14
Dependent Claim 18 words
The process of claim 10, wherein the molecular weight of said intermediate layer is from 100,000 to 2,000,000.
Claim 15
Dependent Claim 33 words
The process of claim 10, wherein the one or more addition polymerizable monomers are selected from the group consisting of acrylates or methacrylates of polyhydric compounds, a polyester acrylate or a polyester methacrylate.
Claim 16
Dependent Claim 11 words
The process of claim 12, wherein the support is polyethylene terephthalate.
Claim 17
Dependent Claim 41 words
The process of claim 12, wherein the one or more photopolymerization initiators include at least one compound represented by the following formula: ##STR6## wherein R 1 is an alkyl group and R 2 is an alkyl group or an aryl group.
Claim 18
Dependent Claim 38 words
The process of claim 12, wherein the one or more photopolymerization initiators include at least one compound represented by the following formula: ##STR7## wherein R 3 and R 4 are alkyl groups of 1 to 5 carbon atoms.
Claim 19
Dependent Claim 22 words
The process of claim 1, wherein said support is transparent and said substrate is metal, image-wise exposure being through said transparent support.
Claim 20
Dependent Claim 92 words
The process of claim 1, wherein said photosensitive material comprises a support and a substrate with a photopolymerizable material therebetween which comprises at least three sublayers, the sublayers which are adjacent to the support and the substrate, respectively, contribute to providing images of good quality by sharply breaking at the interface between exposed and unexposed areas upon stripping development, and any remaining layers intermediate these two sublayers not contributing directly to image quality, but primarily contributing to provide a resist film after image-wise exposure and stripping development which has high mechanical strength.
Claim 21
Dependent Claim 94 words
The process of claim 1, wherein said photosensitive material comprises a support, a substrate and a photopolymerizable material therebetween, said photopolymerizable material comprising at least one sublayer which is adjacent the support and one sublayer which is adjacent the substrate which forms sharp images which do not form a tenting film resistant to etching processing, and at least one sublayer having high film strength therebetween, high film strength being defined as follows: after image-wise exposure to cause photopolymerization, the strength of the layer is sufficient to resist the preseure of etchant during etching spraying.
Claim 22
Dependent Claim 80 words
The process of claim 1, wherein said photosensitive material comprises a support and a substrate with a photopolymerizable material therebetween, said photopolymerizable material comprising sublayers adjacent the support and the substrate, respectively, which sublayers are easily separated at the boundary between exposed and unexposed portions thereof resulting from image-wise exposure by stripping development, and comprising a binder selected from the group consisting of chlorinated polyethylene, chlorinated polypropolene, chlorinated rubbers, and polymers comprising more than 50 mol % of vinylidene chloride.
Claim 23
Dependent Claim 21 words
The process of claim 19, wherein said binders have a molecular weight in the range of about 5,000 to about 100,000.
Claim 24
Dependent Claim 16 words
The process of claim 20, wherein a layer comprising these polymers is adjacent the transparent support.
Claim 25
Dependent Claim 105 words
The process of claim 1, wherein said photosensitive material comprises a support and a substrate with a photopolymerizable material therebetween, the photopolymerizable material comprising at least two sublayers one adjacent to the support and one adjacent to the substrate, each of said sublayers comprising a polymer binder wherein: i. the identity of the monomeric components of the polymer binder of the sublayers differs; or ii. the monomeric components of the polymer binders in each sublayer are identical but the ratio between the monomeric components of the polymer binder in each sublayer differs; or iii. the molecular weight of the polymer binder in each sublayer differs.
Claim 26
Dependent Claim 62 words
The process of claim 1, wherein the photosensitive material comprises a support and a substrate with a photopolymerizable material therebetween, the photopolymerizable material comprising at least two different sublayers adjacent the support and the substrate which comprise at least one polymeric binder and at least one monomer, which binder-monomer combination upon image-wise exposure reverses its adhesion gradient between exposed and unexposed areas.
Claim 27
Dependent Claim 45 words
The process of claim 20, wherein there is present at least one layer intermediate the two sublayers, which layer comprises a polymer binder having a molecular weight in the range of about 10,000 to about 5,000,000, which polymer binder provides high strength to said layer.
Claim 28
Dependent Claim 45 words
The process of claim 1, wherein the ratio by weight of the one or more binders to the monomer is in the range of about 2 to about 0.2, per 100 parts by weight of the one or more binders present in the layer involved.

References Cited (Backward Citations)

US3157505A Cited
US3060026A Cited
US3244519A Cited
US3240600A Cited
US3573918A Cited
US3615435A Cited
US3891441A Cited
US3660088A Cited
US3785817A Cited
US3754920A Cited
US3770438A Cited
US4002478A Cited
US3898086A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1980-09-26 1981-03-28 1981-09-27 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1984-09-26 1985-03-28 1985-09-27 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1988-09-26 1989-03-28 1989-09-27 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag