Patent US4043943A successfully refreshed from Google Patents.
← Back to Patent Explorer
US4043943A Expired / Lapsed US ⏱️ 0.0 years remaining

Process for producing a mixed oxide of vanadium and phosphorus having an improved intrinsic surface area

Assignee: Chevron USA Inc
•
Filing: 1975-09-12
•
Granted: 1977-08-23
•
Expires: 1995-09-12
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A solid vanadium (IV) phosphate having an improved intrinsic surface area is prepared by precipitating the solid from an essentially organic liquid medium at a temperature in the range 0° C. to 200° C.

Inventors

  • 👤 Ronald A. Schneider

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-28 05:58
CPC Classifications
B; B01; B01J; B01J27/00; B01J27/14; B01J27/186; B01J27/195; B01J27/198; C; C07; C07C; C07C51/00; C07C51/16; C07C51/21; C07C51/215

Claims Analysis

Total Claims: 3
Claim 1
Independent Claim 157 words
A process for preparing a catalyst for catalayzing maleic anhydride production by oxidation of a hydrocarbon and which has an intrinsic surface area in excess of 5 m 2 /g, which preparation process comprises: a. forming a solution containing a vanadium compound and a phosphorus compound in an organic liquid medium, the medium containing less than 20 volume percent water and at least 15 volume percent oxygen-containing organic compounds selected from the group consisting of alcohols, carboxylic acids, ethers, esters, amides, and ketones, said medium and said vanadium and phosphorus compounds being effective so as to form a vanadium phosphate compound wherein the average valence of vanadium is between +3.8 and +4.6; b. precipitating said vanadium phosphate compound in said solution; c. removing liquid medium from the solution to obtain said vanadium phosphate compound; and d. calcining the vanadium phosphate compound to obtain said catalyst having an intrinsic surface area in excess of 5 m 2 /g.--
Claim 2
Dependent Claim 157 words
A process for preparing a catalyst for catalayzing maleic anhydride production by oxidation of a hydrocarbon and which has an intrinsic surface area in excess of 5 m 2 /g, which preparation process comprises: a. forming a solution containing a vanadium compound and a phosphorus compound in an organic liquid medium, the medium containing less than 20 volume percent water and at least 15 volume percent oxygen-containing organic compounds selected from the group consisting of alcohols, carboxylic acids, ethers, esters, amides, and ketones, said medium and said vanadium and phosphorus compounds being effective so as to form a vanadium phosphate compound wherein the average valence of vanadium is between +3.8 and +4.6; b. precipitating said vanadium phosphate compound in said solution; c. removing liquid medium from the solution to obtain said vanadium phosphate compound; and d. calcining the vanadium phosphate compound to obtain said catalyst having an intrinsic surface area in excess of 5 m 2 /g.--
Claim 3
Dependent Claim 19 words
A process in accordance with claim 1 wherein the intrinsic surface area is at least 10 M 2 /g.

References Cited (Backward Citations)

US3156706A Cited
US3156707A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1980-08-22 1981-02-21 1981-08-23 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1984-08-22 1985-02-21 1985-08-23 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1988-08-22 1989-02-21 1989-08-23 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag