Abstract

Abstract In a method of treating clay-containing phosphate rock comprising at least mining the phosphate rock, reducing the phosphate rock to a predetermined size range, adding water to the phosphate rock, and storing the admixture containing at least the phosphate rock and water; the improvement characterized by adding to the admixture an amount effective to control problems associated with the swelling of residual clays of a chemical treatment selected from the class consisting of aliphatic hydroxy acids containing 2-6 carbon atoms, inclusive, of which citric acid and tartaric acid are members; the aliphatic hydroxy acid salts, and effective blends of the aliphatic hydroxy acid or the aliphatic hydroxy acid salts with a strong caustic, or base. The chemical treatment prevents a build up of viscosity such that the admixture remains pumpable even with a concentration of solids in excess of 66 percent by weight. Moreover, in phosphoric acid production, the equality of the calcium sulfate crystals is improved such that they are more readily removable by filtering. An effective amount of chemical treatment, preferably, is, for example, one pound per ton of phosphate rock and no more than about six pounds per ton (0.05-0.3 percent by weight).

Inventors

  • 👤 Herbert L. Rice
  • 👤 Roy A. Wilkins

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-05 23:57
CPC Classifications
F; F17; F17D; F17D1/00; F17D1/08; F17D1/16

Claims Analysis

Total Claims: 26
Claim 1
Independent Claim 152 words
In a process for treating clay-containing phosphate rock that includes the hydraulic transportation of finely divided phosphate rock wherein the phosphate rock is prepared in the form of an admixture of the phosphate rock in an aqueous slurry for handling; the improvement comprising the step of adding to said admixture a chemical selected from the class consisting of an aliphatic hydroxy acid containing 2-6 carbon atoms, inclusive; a water-soluble, inorganic salt of said aliphatic acid; and a blend of one of said aliphatic hydroxy acid and said salt of said aliphatic hydroxy acid with an alkali metal hydroxide; said chemical being added in at least an amount effective to reduce viscosity of said admixture at a predetermined time interval after addition below the viscosity of said admixture alone and such that said admixture can be pumped after 4 hours storage at concentrations of solids therein in excess of 65 percent by weight.
Claim 2
Dependent Claim 152 words
In a process for treating clay-containing phosphate rock that includes the hydraulic transportation of finely divided phosphate rock wherein the phosphate rock is prepared in the form of an admixture of the phosphate rock in an aqueous slurry for handling; the improvement comprising the step of adding to said admixture a chemical selected from the class consisting of an aliphatic hydroxy acid containing 2-6 carbon atoms, inclusive; a water-soluble, inorganic salt of said aliphatic acid; and a blend of one of said aliphatic hydroxy acid and said salt of said aliphatic hydroxy acid with an alkali metal hydroxide; said chemical being added in at least an amount effective to reduce viscosity of said admixture at a predetermined time interval after addition below the viscosity of said admixture alone and such that said admixture can be pumped after 4 hours storage at concentrations of solids therein in excess of 65 percent by weight.
Claim 3
Dependent Claim 34 words
The process of claim 1 wherein said aliphatic hydroxy acid is selected from the class consisting of glycolic acid, lactic acid, hydroxybutyric acid, glyceric acid, malic acid, tartaric acid, citric acid, and gluconic acid.
Claim 4
Dependent Claim 24 words
The process of claim 1 wherein said aliphatic hydroxy acid is selected from the class consisting of lactic acid, citric acid, and gluconic acid.
Claim 5
Dependent Claim 13 words
The process of claim 3 wherein said aliphatic hydroxy acid is citric acid.
Claim 6
Dependent Claim 31 words
The process of claim 1 wherein said chemical comprises a blend of said alkali metal hydroxide and at least 10 percent by weight of said salt of said aliphatic hydroxy acid.
Claim 7
Dependent Claim 28 words
The process of claim 5 wherein the concentration of said salt of said aliphatic hydroxy acid is within the range of 10-50 percent by weight of said blend.
Claim 8
Dependent Claim 25 words
The process of claim 6 wherein the concentration of said salt of said aliphatic hydroxy acid is about 30 percent by weight of said blend.
Claim 9
Dependent Claim 63 words
The process of claim 1 including the further steps of: a. adding sulfuric acid to said phosphate rock admixture; b. allowing a predetermined time interval for digestion of said rock by said acid to take place and form a liquor and a precipitate comprising gypsum calcium sulfate; and c. filtering said liquor and precipitate to remove said calcium sulfate crystals from said liquor.
Claim 10
Dependent Claim 37 words
The process of claim 8 wherein said chemical is added simultaneously with said water to said phosphate rock and the resulting admixture is stored for a period of up to 4 hours before said acid is added.
Claim 11
Dependent Claim 90 words
The process of claim 9 wherein said water is added to said phosphate rock before the phosphate rock is reduced to a predetermined size range; the resulting slurry formed by grinding said phosphate rock in said water is stored for a period of up to 4 hours before said acid is added; and the filtrate from the first part of the step of filtering of step (c) of claim 8 to remove said calcium sulfate crystals is recycled as acid to be added to said phosphate rock in step (a).
Claim 12
Dependent Claim 33 words
The process of claim 8 wherein said chemical is also added in an amount effective to provide improved crystal growth of gypsum calcium sulfate crystals that are more readily filterable from said liquor.
Claim 13
Dependent Claim 38 words
The process of claim 11 wherein said chemical is present in said admixture in a proportion of at least one pound per ton of phosphate rock and no more than about 10 pounds per ton of phosphate rock.
Claim 14
Dependent Claim 24 words
The process of claim 12 wherein said chemical is present in an amount within the range of 2-6 pounds per ton of phosphate rock.
Claim 15
Dependent Claim 28 words
The process of claim 8 wherein said water, said acid and said chemical are added simultaneously to phosphate rock that has been reduced to a predetermined size range.
Claim 16
Dependent Claim 30 words
The process of claim 14 wherein filtrate from the step of filtering in step (c) of claim 8 is recycled to be admixed with said phosphate rock in step (a).
Claim 17
Dependent Claim 28 words
The process of claim 14 wherein said chemical is present in a proportion of at least one and no more than 10 pounds per ton of phosphate rock.
Claim 18
Dependent Claim 21 words
The process of claim 16 wherein said chemical is present in the range of 2-6 pounds per ton of phosphate rock.
Claim 19
Dependent Claim 29 words
The process of claim 1 wherein said phosphate rock is beneficiated prior to the preparation of said phosphate rock slurry so as to increase the proportion of phosphate therein.
Claim 20
Dependent Claim 20 words
The process of claim 1 wherein said chemical is added in an amount of at least 0.05 percent by weight.
Claim 21
Dependent Claim 38 words
The process of claim 1 wherein said chemical is present in said admixture in a proportion of at least 1 pound per ton of phosphate rock and no more than about 10 pounds per ton of phosphate rock.
Claim 22
Dependent Claim 24 words
The process of claim 20 wherein said chemical is present in an amount within a range of 2-6 pounds per ton of phosphate rock.
Claim 23
Dependent Claim 175 words
In a process for treating clay-containing phosphate rock that has been comminuted and that includes the steps of: a. adding sulfuric acid to said phosphate rock; b. allowing a predetermined time interval for digestion of said rock by said acid to take place and form a liquor and a precipitate comprising calcium sulfate; and c. filtering said liquor and precipitate to remove said calcium sulfate crystals from said liquor; the improvement comprising adding to said phosphate rock and acid a chemical selected from the class consisting of an aliphatic hydroxy acid containing 2-6 carbon atoms, inclusive; a water-soluble, inorganic salt of said aliphatic hydroxy acid; and a blend of one of said aliphatic hydroxy acid and said salt of said aliphatic acid with an alkali metal hydroxide; said chemical being added in an amount sufficient to improve the crystals of calcium sulfate that are formed so they are more readily removed by filtering as compared to calcium sulfate crystals that are formed by said phosphate rock and sulfuric acid alone and without said chemical treatment.
Claim 24
Dependent Claim 175 words
In a process for treating clay-containing phosphate rock that has been comminuted and that includes the steps of: a. adding sulfuric acid to said phosphate rock; b. allowing a predetermined time interval for digestion of said rock by said acid to take place and form a liquor and a precipitate comprising calcium sulfate; and c. filtering said liquor and precipitate to remove said calcium sulfate crystals from said liquor; the improvement comprising adding to said phosphate rock and acid a chemical selected from the class consisting of an aliphatic hydroxy acid containing 2-6 carbon atoms, inclusive; a water-soluble, inorganic salt of said aliphatic hydroxy acid; and a blend of one of said aliphatic hydroxy acid and said salt of said aliphatic acid with an alkali metal hydroxide; said chemical being added in an amount sufficient to improve the crystals of calcium sulfate that are formed so they are more readily removed by filtering as compared to calcium sulfate crystals that are formed by said phosphate rock and sulfuric acid alone and without said chemical treatment.
Claim 25
Dependent Claim 91 words
In a process for treating clay-containing phosphate rock that has been comminuted and includes the step of adding an aqueous medium to said phosphate rock for handling, the improvement comprising adding a concentration within the range of 0.05-0.5 percent by weight of a chemical selected from the class consisting of an aliphatic hydroxy acid containing 2-6 carbon atoms, inclusive; a water-soluble, inorganic salt of said aliphatic hydroxy acid; and a blend of one of said aliphatic hydroxy acid and said salt of said aliphatic hydroxy acid with an alkali metal hydroxide.
Claim 26
Dependent Claim 91 words
In a process for treating clay-containing phosphate rock that has been comminuted and includes the step of adding an aqueous medium to said phosphate rock for handling, the improvement comprising adding a concentration within the range of 0.05-0.5 percent by weight of a chemical selected from the class consisting of an aliphatic hydroxy acid containing 2-6 carbon atoms, inclusive; a water-soluble, inorganic salt of said aliphatic hydroxy acid; and a blend of one of said aliphatic hydroxy acid and said salt of said aliphatic hydroxy acid with an alkali metal hydroxide.

References Cited (Backward Citations)

CA621067A Cited
US1979469A Cited
US2437297A Cited
US3035867A Cited
US3423172A Cited
JPS4421414Y1 Cited
US3594123A Cited
GB1202083A Cited
US3928551A Cited
US3843524A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1980-08-15 1981-02-14 1981-08-16 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1984-08-15 1985-02-14 1985-08-16 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1988-08-15 1989-02-14 1989-08-16 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag