Polymerized titanium dioxide for ultraviolet coatings
Assignee: Celanese Corp
•
Filing: 1975-02-18
•
Granted: 1977-08-16
•
Expires: 1995-02-18
Abstract
Abstract There is disclosed a process for utilizing titanium dioxide pigments in ultraviolet coating compositions. Basically, the process involves forming a vinyl aqueous emulsion in the presence of titanium dioxide pigments; precipitating and drying the titanium dioxide-polymeric emulsion and adding the dried precipitate as pigment to an ultraviolet curable coating composition.
Inventors
- 👤 George L. Collins
- 👤 John R. Costanza
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-26 01:51
CPC Classifications
C; C08; C08F; C08F291/00; C08F291/18; C08K; C08K3/00; C08K3/18; C08K3/20; C08K3/22; C09; C09D; C09D4/00
Claims Analysis
Total Claims: 10
Claim 1
Independent Claim
192 words
A process for ultraviolet coating which comprises: a. forming an aqueous polymer emulsion of alpha beta ethylenically unsaturated vinyl polymerizable monomers utilizing a free radical initiator and up to about 20 percent, by weight, based on the solids content of the formed emulsion, of titanium dioxide; b. precipitating the resulting polymer emulsion utilizing an organic solvent having a boiling point of less than about 70° C.; c. removing water and solvent from the precipitate; d. mixing the dried precipitate with an ultraviolet curable binder in the precipitate to binder ratio, by weight, of about 2-1 to 1-5, wherein said binder contains about 40 to about 100 percent, by weight, of an alpha beta ethylenically unsaturated vinyl polymerizable compound containing at least two sites of alpha beta ethylenic unsaturation and up to about 60 percent, by weight, of an alpha beta ethylenically unsaturated vinyl polymerizable monomer containing no more than one site of alpha beta ethylenic unsaturation, and about 0.1 to about 15 percent, by weight, based upon the ultraviolet curable components, of an ultraviolet photoinitiator; e. applying a coating of the ultraviolet curable mixture; and f. subjecting the coating to ultraviolet light.
Claim 2
Dependent Claim
192 words
A process for ultraviolet coating which comprises: a. forming an aqueous polymer emulsion of alpha beta ethylenically unsaturated vinyl polymerizable monomers utilizing a free radical initiator and up to about 20 percent, by weight, based on the solids content of the formed emulsion, of titanium dioxide; b. precipitating the resulting polymer emulsion utilizing an organic solvent having a boiling point of less than about 70° C.; c. removing water and solvent from the precipitate; d. mixing the dried precipitate with an ultraviolet curable binder in the precipitate to binder ratio, by weight, of about 2-1 to 1-5, wherein said binder contains about 40 to about 100 percent, by weight, of an alpha beta ethylenically unsaturated vinyl polymerizable compound containing at least two sites of alpha beta ethylenic unsaturation and up to about 60 percent, by weight, of an alpha beta ethylenically unsaturated vinyl polymerizable monomer containing no more than one site of alpha beta ethylenic unsaturation, and about 0.1 to about 15 percent, by weight, based upon the ultraviolet curable components, of an ultraviolet photoinitiator; e. applying a coating of the ultraviolet curable mixture; and f. subjecting the coating to ultraviolet light.
Claim 3
Dependent Claim
24 words
The process of claim 1 wherein the titanium dioxide pigment has a particle size in the range of about 0.05 to about 10 microns.
Claim 4
Dependent Claim
18 words
The process of claim 1 wherein the polymer emulsion is prepared at temperatures ranging up to 250° F.
Claim 5
Dependent Claim
20 words
The process of claim 1 wherein the emulsion is prepared utilizing a stabilizing surfactant, which is nonionic, anionic or cationic.
Claim 6
Dependent Claim
28 words
The process of claim 4 wherein the surfactant is added at a weight range of up to about 10 percent, by weight, based on the vinyl polymerizable monomers.
Claim 7
Dependent Claim
19 words
The process of claim 1 wherein said polymer emulsion is formed in the presence of a protective colloid-forming substance.
Claim 8
Dependent Claim
16 words
The process of claim 1 wherein the organic solvent is a C 1 -C 5 alcohol.
Claim 9
Dependent Claim
10 words
The process of claim 7 wherein the alcohol is propanol.
Claim 10
Dependent Claim
23 words
The process of claim 1 wherein up to about 500 percent, by weight, based upon the photoinitiator, of an organic amine is utilized.
References Cited (Backward Citations)
US3393165A
Cited
US3759807A
Cited
US3887450A
Cited
US3887450B1
Cited
US3827958A
Cited
US3884871A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1980-08-15 | 1981-02-14 | 1981-08-16 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1984-08-15 | 1985-02-14 | 1985-08-16 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1988-08-15 | 1989-02-14 | 1989-08-16 | $7700.00 | Window Closed / Lapsed |