Coupling of alkali metal-terminated polymers

Assignee: Phillips Petroleum Co
•
Filing: 1976-04-19
•
Granted: 1977-08-02
•
Expires: 1996-04-19
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract Alkali metal-terminated polymers of one or more alkadienes and of one or more vinyl-substituted aromatic monomers are effectively coupled by a di-, tri-, or tetra carboxylic acid halide of substituted or unsubstituted benzene.

Inventors

  • 👤 Robert P. Zelinski

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-27 21:25
CPC Classifications
C; C08; C08G; C08G81/00; C08G81/02; C08G81/021; C08C; C08C19/00; C08C19/30; C08C19/42; C08C19/44

Claims Analysis

Total Claims: 14
Claim 1
Independent Claim 145 words
A process for the production of a polymer comprising reacting a living alkali metal-terminated polymer having the formula M--Z wherein M represents an alkali metal and Z is selected from a group consisting of polymer chains of one or more alkadienes having 4-12 carbon atoms and copolymer chains of one or more alkadienes having 4-12 carbon atoms and one or more monovinylarenes of 8-18 carbon atoms, having the vinyl radical attached to an arene ring carbon atom, with a coupling agent having the formula A(COX).sub.n R.sub.6.sub.-n wherein A is a benzene ring, the radicals X, which can be the same or different, are halogen, n is 2, 3 or 4, the radicals R which can be the same or different, are hydrogen or hydrocarbyl radicals of 1-6 carbon atoms, the total number of carbon atoms in all radicals R being between 0 and about 10.
Claim 2
Dependent Claim 145 words
A process for the production of a polymer comprising reacting a living alkali metal-terminated polymer having the formula M--Z wherein M represents an alkali metal and Z is selected from a group consisting of polymer chains of one or more alkadienes having 4-12 carbon atoms and copolymer chains of one or more alkadienes having 4-12 carbon atoms and one or more monovinylarenes of 8-18 carbon atoms, having the vinyl radical attached to an arene ring carbon atom, with a coupling agent having the formula A(COX).sub.n R.sub.6.sub.-n wherein A is a benzene ring, the radicals X, which can be the same or different, are halogen, n is 2, 3 or 4, the radicals R which can be the same or different, are hydrogen or hydrocarbyl radicals of 1-6 carbon atoms, the total number of carbon atoms in all radicals R being between 0 and about 10.
Claim 3
Dependent Claim 11 words
A process in accordance with claim 1 wherein M is lithium.
Claim 4
Dependent Claim 36 words
A process in accordance with claim 1 wherein the coupling agent is employed in such a quantity that about 0.1 to 1.5 atoms of X are present per atom of M in the coupling reaction mixture.
Claim 5
Dependent Claim 18 words
A process in accordance with claim 1 wherein the coupling agent used is a 1,3,5-benzene tricarboxylic acid trihalide.
Claim 6
Dependent Claim 55 words
A process in accordance with claim 1 wherein an alkali metal terminated polymer having the structure M--B'--A' is used, in which M is an alkali metal, A' is a polystyrene block, and B' is a rubbery block obtained by polymerizing or copolymerizing an alkadiene selected from the group consisting of butadiene, isoprene and mixtures thereof.
Claim 7
Dependent Claim 110 words
A process in accordance with claim 1 comprising a. polymerizing under polymerization conditions in a hydrocarbon diluent and in contact with a monofunctional alkali metal polymerization initiator system, at least one alkadiene monomer having 4-12 carbon atoms or at least one alkadiene monomer having 4-12 carbon atoms and at least one monovinyl-substituted arene, the vinyl substituent being attached to a ring carbon atom of the arene ring, to obtain a solution containing a living polymer having the structure M--Z. b. mixing this solution and the coupling agent such as to produce a solution containing a coupled polymer, and c. recovering a coupled polymer from the reaction mixture of step (b).
Claim 8
Dependent Claim 34 words
A process in accordance with claim 6 wherein said alkadiene monomer is selected from the group consisting of butadiene, isoprene, piperylene and mixtures thereof, and wherein said monovinyl-substituted arene is styrene or a methylstyrene.
Claim 9
Dependent Claim 44 words
A process in accordance with claim 6 wherein the alkali metal terminated polymer M--Z is produced by incremental addition of at least two different monomers such as to form a living block copolymer of at least two polymer blocks in the polymer chain Z.
Claim 10
Dependent Claim 138 words
A process in accordance with claim 8 wherein styrene is first polymerized with said monofunctional alkali metal initiator system to form a living polystyrene block in a first polymer mixture, wherein an alkadiene monomer selected from the group consisting of butadiene, isoprene and mixtures thereof, alone or in admixture with a monovinylarene selected from the group consisting of styrene, the methylstyrenes and mixtures thereof is blended with said first polymer mixture to form a second polymer mixture consisting of a living polymer having a rubbery block attached to said styrene block, said alkali metal M being attached to the rubbery block, and wherein the second polymer mixture thereafter is blended with said coupling agent such as to form a third polymer mixture comprising a coupled polymer with polystyrene blocks at the free ends of the coupled polymer chains.
Claim 11
Dependent Claim 35 words
A process in accordance with claim 6 wherein the monofunctional alkali metal initiator system comprises a lithium compound having the formula R'"Li wherein R'" is a hydrocarbyl radical of 1 to about 20 carbon atoms.
Claim 12
Dependent Claim 24 words
A process in accordance with claim 6 wherein said diluent is selected from the group consisting of n-hexane, cyclohexane, n-heptane, 2,2,4-trimethylpentane, benzene and toluene.
Claim 13
Dependent Claim 28 words
A process in accordance with claim 6 wherein about 0.1 to about 100 gram millimoles of monofunctional alkali metal initiator are used per 100 grams of total monomers.
Claim 14
Dependent Claim 67 words
A process in accordance with claim 6 further comprising the steps of a. reacting the mixture obtained during the coupling step and before carrying out the recovering step in the presence of a hydrogenation catalyst and in the presence of free hydrogen to obtain an at least partially hydrogenated polymer, and b. recovering the thus obtained at least partially hydrogenated polymer as the product of the process.

References Cited (Backward Citations)

US3135716A Cited
US3177190A Cited
US3281383A Cited
US3506639A Cited
US3668279A Cited
US3810877A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1980-08-01 1981-01-31 1981-08-02 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1984-08-01 1985-01-31 1985-08-02 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1988-08-01 1989-01-31 1989-08-02 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag