Film-lined foam plastic receptacles and laminated materials and methods for making the same

Assignee: OI Glass Inc
•
Filing: 1976-04-02
•
Granted: 1977-07-19
•
Expires: 1996-04-02
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A low-cost, throw-away receptacle such as a cup, picnic plate, or container, and closures for such receptacles, are made from foamed plastic material, preferably foamed polystyrene, which is lined on one or both sides with unoriented polyolefin film, preferably polypropylene. The film is secured to the foamed plastic base material using as a heat-sensitive adhesive a vinylic polymer or polyamide resin. Preferred vinylic polymers are based on vinyl acetate, and include polyvinyl acetate maleate copolymer. The film is coated with the initially wet adhesive which is dispersed in an emulsion or solvent carrier, and dried before laminating the film to the foam material. Laminating is done by heating the foam material to a temperature of from 250°-275° F., preheating the coated film to from 100°-180° F., and pressing the coated film surface against the heated foam using a cold platen or roller for from 10 to 15 seconds. The adhesive may be pigmented, and imprinted or applied over decorative printing on the transparent polyolefin film liner material, to provide colorful designs or printing appearing through the film and thus shielded by the liner material from scuffing or marring. The hard, glossy polyolefin film liner which provides the surface of such receptacles is strong to resist puncture, yet the foamed plastic base material provides both heat resistance and lightness, and does not absorb water or grease. Continuous processes and apparatus for making such laminated material and receptacles are disclosed.

Inventors

  • 👤 Stephen W. Amberg
  • 👤 Frank S. Landers

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-05 22:43
CPC Classifications
B; B32; B32B; B32B27/00; B32B27/06; B32B27/065; B29; B29C; B29C43/00; B29C43/22; B29C43/30; B29C43/305; B29C51/00; B29C51/14; B32B27/08; B32B27/32; B32B37/00; B32B37/10; B32B37/12; B32B37/1207; B32B38/00; B32B38/0036; B65; B65D; B65D1/00; B65D1/22; B65D1/26; B65D1/28; B29K; B29K2023/00; B29K2023/10; B29K2023/12; B29K2025/00; B29K2105/00; B29K2105/04; B29L; B29L2031/00; B29L2031/712; B29L2031/7132; B32B2266/00; B32B2266/02; B32B2266/0214; B32B2266/0221; B32B2266/0228; B32B2307/00; B32B2307/30; B32B2307/306; B32B2307/40; B32B2307/406; B32B2307/70; B32B2307/726; B32B2307/7265; B32B2323/00; B32B2323/10; B32B2439/00; Y; Y10; Y10T; Y10T428/00; Y10T428/249921; Y10T428/249953; Y10T428/249982; Y10T428/249985; Y10T428/249987; Y10T428/249991; Y10T428/249992; Y10T428/249993

Claims Analysis

Total Claims: 24
Claim 1
Independent Claim 100 words
A method of laminating a polyolefin plastic film to a surface of a foamed plastic material comprising the steps of applying an initially wet coating of a heat-sensitive plastic resin adhesive on a surface of substantially unoriented polyolefin film and drying said coating, and thereafter heating said dried adhesive to a temperature above its softening point but below the softening points of said film and said foamed plastic material while holding said coated film surface and said foamed plastic material surface against each other, and thereafter cooling the laminated material to a temperature below said softening point of the adhesive.
Claim 2
Independent Claim 100 words
A method of laminating a polyolefin plastic film to a surface of a foamed plastic material comprising the steps of applying an initially wet coating of a heat-sensitive plastic resin adhesive on a surface of substantially unoriented polyolefin film and drying said coating, and thereafter heating said dried adhesive to a temperature above its softening point but below the softening points of said film and said foamed plastic material while holding said coated film surface and said foamed plastic material surface against each other, and thereafter cooling the laminated material to a temperature below said softening point of the adhesive.
Claim 3
Dependent Claim 23 words
A method according to claim 1 wherein said cooling is effected by pressing and holding said laminated material against a relatively cold surface.
Claim 4
Dependent Claim 19 words
A method according to claim 2 wherein said pressing for cooling said laminated material is effected by fluid pressure.
Claim 5
Dependent Claim 41 words
A method according to claim 1 wherein said foamed plastic material is heated to said temperature above the softening point of said adhesive before said coated film surface and said foamed plastic material surface are placed in contact with each other.
Claim 6
Dependent Claim 22 words
A method according to claim 4 wherein said film is placed against said foamed plastic material using a relatively cold pressing means.
Claim 7
Dependent Claim 53 words
A method according to claim 5 wherein said coated surface of the film is preheated to a temperature of from substantially 100° F. to substantially 180° F. by a stream of heated air directed against said film surface prior to said placing of said film and said foamed plastic material against each other.
Claim 8
Dependent Claim 54 words
A method according to claim 5 wherein said foamed plastic material is polystyrene, and said polystyrene foam is heated to a temperature within the range of from about 250° F. to about 275° F., and the temperature of said pressing means for placing said film against said foamed plastic material is below 150° F.
Claim 9
Dependent Claim 12 words
A method according to claim 7 wherein said polyolefin film is polypropylene.
Claim 10
Dependent Claim 21 words
A method according to claim 7 wherein said polyolefin is polyethylene, and said polystyrene foam is heated to substantially 250° F.
Claim 11
Dependent Claim 15 words
A method according to claim 7 wherein said pressing means is a relatively cold roller.
Claim 12
Dependent Claim 29 words
A method according to claim 10 wherein said cooling of the laminated material is effected by using fluid pressure to press said laminated material against a relatively cold surface.
Claim 13
Dependent Claim 15 words
A method according to claim 11 wherein said relatively cold surface is a receptacle mold.
Claim 14
Dependent Claim 19 words
A method according to claim 7 wherein said plastic resin adhesive is a solvent solution of a polyamide resin.
Claim 15
Dependent Claim 15 words
A method according to claim 7 wherein said plastic resin adhesive is a vinylic polymer.
Claim 16
Dependent Claim 17 words
A method according to claim 14 wherein said vinylic polymer is a polymer based on vinyl acetate.
Claim 17
Dependent Claim 18 words
A method according to claim 15 wherein said vinylic polymer is a copolymer of ethylene and vinyl acetate.
Claim 18
Dependent Claim 16 words
A method according to claim 16 wherein said copolymer is a polyvinyl acetate maleate copolymer emulsion.
Claim 19
Dependent Claim 21 words
A method according to claim 16 wherein said polyolefin film and said ethylene-vinyl acetate are coextruded to form said coated film.
Claim 20
Dependent Claim 22 words
A method according to claim 15 wherein said vinylic polymer is a blend of polyvinyl acetate and a polyvinyl acetate acrylic copolymer.
Claim 21
Dependent Claim 109 words
A process for manufacturing receptacles from a sheet of cellular polystyrene foam material coated with a film of polyolefin material secured to the foam by a plastic resin adhesive comprising the steps of applying said adhesive to one side of a substantially unoriented polyolefin film and allowing the adhesive to dry, heating both said foam and the adhesive coated film to a temperature of substantially 260° F. while pressing the adhesive coated side of said film against said foam to form a laminate, and vacuum-forming said laminate into the form of a receptacle by drawing said laminate into a cold mold while said foam and said film are heated.
Claim 22
Dependent Claim 109 words
A process for manufacturing receptacles from a sheet of cellular polystyrene foam material coated with a film of polyolefin material secured to the foam by a plastic resin adhesive comprising the steps of applying said adhesive to one side of a substantially unoriented polyolefin film and allowing the adhesive to dry, heating both said foam and the adhesive coated film to a temperature of substantially 260° F. while pressing the adhesive coated side of said film against said foam to form a laminate, and vacuum-forming said laminate into the form of a receptacle by drawing said laminate into a cold mold while said foam and said film are heated.
Claim 23
Dependent Claim 10 words
The process of claim 20 wherein said polyolefin is polypropylene.
Claim 24
Dependent Claim 25 words
The process of claim 20 which further comprises similarly applying adhesive coated film to both sides of said foam material prior to said forming step.

References Cited (Backward Citations)

US3234065A Cited
US3220902A Cited
US3483076A Cited
US3617419A Cited
US3619344A Cited
US3654069A Cited
US3919033A Cited
US3933762A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1980-07-18 1981-01-17 1981-07-19 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1984-07-18 1985-01-17 1985-07-19 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1988-07-18 1989-01-17 1989-07-19 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag