Patent US4030988A successfully refreshed from Google Patents.
US4030988A
Expired / Lapsed
US
⏱️ 0.0 years remaining
Process for producing halogen and metal hydroxides with cation exchange membranes of improved permselectivity
Assignee: EIDP Inc
•
Filing: 1976-04-27
•
Granted: 1977-06-21
•
Expires: 1996-04-27
Abstract
Abstract Fluorinated cation exchange polymers are obtained from intermediate fluorinated polymers containing pendant sulfonyl halide groups which are reacted with a di- or polyamine and subjected to elevated temperature of the order of 170° to 300° C. The polymers are desirably employed with pendant side groups in the salt form. The polymers possess permselectivity giving desirable performance in electrolytic cells such as chlor-alkali cells as well as membrane ion exchanger and reverse osmosis devices.
Inventors
- 👤 Walther Gustav Grot
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-25 12:33
CPC Classifications
B; B01; B01D; B01D71/00; B01D71/06; B01D71/30; B01D71/32; B01D67/00; B01D67/0081; B01D67/0083; C; C08; C08F; C08F8/00; C08J; C08J5/00; C08J5/20; C08J5/22; C08J2327/00; C08J2327/02; C08J2327/12
Claims Analysis
Total Claims: 3
Claim 1
Independent Claim
235 words
In a process of production of halogen and metal hydroxide of an alkali or alkaline earth metal, or combination thereof, by electrolysis of a halide of said metal employing anode and cathode sections separated by an ion exchange film, said improvement comprising passing ions of said metal through a fluorinated ion exchange polymer film comprising a. a first surface formed from an intermediate fluorinated polymer containing pendant sulfonyl halide groups attached to carbon atoms which have at least one fluorine atom connected thereto in which i. at least 40% of the sulfonyl halide groups to a depth of at least one micron in the intermediate polymer have been reacted with a di- or poly-amine comprising at least two groups with one primary amine group and a second amino group either primary or secondary, said first surface facing the cathode section; and ii. the polymer of (i) has been subjected to an elevated temperature of between 170° C. and the degradation temperature of the reacted polymer for a period of time to increase permselectivity; b. a second surface containing pendant sulfonyl groups attached to carbon atoms which have at least one fluorine atom connected thereto with at least a majority of the sulfonyl groups present as --(SO 2 NH) m Q, or --(SO 3 ) n Me wherein Q and Me represent ions of said metal, and m and n represent the valence of said metal.
Claim 2
Dependent Claim
235 words
In a process of production of halogen and metal hydroxide of an alkali or alkaline earth metal, or combination thereof, by electrolysis of a halide of said metal employing anode and cathode sections separated by an ion exchange film, said improvement comprising passing ions of said metal through a fluorinated ion exchange polymer film comprising a. a first surface formed from an intermediate fluorinated polymer containing pendant sulfonyl halide groups attached to carbon atoms which have at least one fluorine atom connected thereto in which i. at least 40% of the sulfonyl halide groups to a depth of at least one micron in the intermediate polymer have been reacted with a di- or poly-amine comprising at least two groups with one primary amine group and a second amino group either primary or secondary, said first surface facing the cathode section; and ii. the polymer of (i) has been subjected to an elevated temperature of between 170° C. and the degradation temperature of the reacted polymer for a period of time to increase permselectivity; b. a second surface containing pendant sulfonyl groups attached to carbon atoms which have at least one fluorine atom connected thereto with at least a majority of the sulfonyl groups present as --(SO 2 NH) m Q, or --(SO 3 ) n Me wherein Q and Me represent ions of said metal, and m and n represent the valence of said metal.
Claim 3
Dependent Claim
24 words
The process of claim 1 wherein said film is formed from an intermediate polymer which is a copolymer of tetrafluoroethylene and perfluoro(3, 6-dioxa-4-methyl-7-octenesulfonyl fluoride).
References Cited (Backward Citations)
US3969285A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1980-06-20 | 1980-12-20 | 1981-06-21 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1984-06-20 | 1984-12-20 | 1985-06-21 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1988-06-20 | 1988-12-20 | 1989-06-21 | $7700.00 | Window Closed / Lapsed |