US4029557A Expired / Lapsed US ⏱️ 0.0 years remaining

Treatment of water containing cyanide

Assignee: ATK Launch Systems LLC
•
Filing: 1975-10-15
•
Granted: 1977-06-14
•
Expires: 1995-10-15
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract Sodium chloride is added to water which is then passed through at least one electrolytic cell. There, electrolysis of the sodium chloride produces chlorine molecules and sodium hydroxide. The water is then flowed into the presence of metal-cyanide contaminants. The chlorine and caustic immediately react with the metal-cyanide compounds to produce metal hydroxide precipitates, while the cyanide is decomposed and liberated from the water in carbon dioxide and gaseous nitrogen. As part of this reaction, the sodium chloride is reformed, so that the same brine can be recycled and the process repeated without further additives. The optimum pH of between 7 and 8 may be maintained as needed by addition of small amounts of hydrochloric acid to the system.

Inventors

  • 👤 Wendell N. Christensen
  • 👤 Larry W. Poulter

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-27 20:33
CPC Classifications
C; C02; C02F; C02F9/00; C02F1/00; C02F1/46; C02F1/461; C02F1/46104; C02F1/46109; C02F1/467; C02F1/4672; C02F1/4674; C02F1/72; C02F1/76; C02F2001/46152; C02F2101/00; C02F2101/10; C02F2101/16; C02F2101/18; Y; Y10; Y10S; Y10S210/00; Y10S210/902; Y10S210/903; Y10S210/904

Claims Analysis

Total Claims: 4
Claim 1
Independent Claim 104 words
The process for destroying cyanide in water containing a metal-cyanide compound, comprising the steps of: adding 1 to 6% by weight of sodium chloride to water; passing the water through at least one energized electrolytic cell, wherein the sodium chloride and water are electrolyzed to produce chlorine and sodium hydroxide; mixing this water with that containing the metal-cyanide compound; allowing the chlorine and sodium hydroxide to react with the metalcyanide compound, wherein the cyanide is released in harmless gaseous products, the metal is precipitated, and the sodium chloride is reformed; and recycling the resulting water containing the sodium chloride for repetition of the process.
Claim 2
Dependent Claim 104 words
The process for destroying cyanide in water containing a metal-cyanide compound, comprising the steps of: adding 1 to 6% by weight of sodium chloride to water; passing the water through at least one energized electrolytic cell, wherein the sodium chloride and water are electrolyzed to produce chlorine and sodium hydroxide; mixing this water with that containing the metal-cyanide compound; allowing the chlorine and sodium hydroxide to react with the metalcyanide compound, wherein the cyanide is released in harmless gaseous products, the metal is precipitated, and the sodium chloride is reformed; and recycling the resulting water containing the sodium chloride for repetition of the process.
Claim 3
Dependent Claim 30 words
the process of claim 1 including addition of 0.05% to 1.0% of magnesium chloride (Mg Cl 2 ) to the water to prevent deposits of calcium on the electrolytic cell.
Claim 4
Dependent Claim 21 words
The process of claim 1 wherein the pH is controlled to be between 7 and 8 by addition of hydrochloric acid.

References Cited (Backward Citations)

US892486A Cited
US2737298A Cited
US3361663A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1980-06-13 1980-12-13 1981-06-14 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1984-06-13 1984-12-13 1985-06-14 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1988-06-13 1988-12-13 1989-06-14 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag