Patent US4011909A successfully refreshed from Google Patents.
US4011909A
Expired / Lapsed
US
⏱️ 0.0 years remaining
Method of using cementing composition having improved flow properties
Assignee: ECC SPECIALTY CHEMICALS Inc
•
Filing: 1976-01-29
•
Granted: 1977-03-15
•
Expires: 1996-01-29
Abstract
Abstract Methods of using aqueous hydraulic cement compositions containing polyamido-sulfonic compounds as flow-property-improving and turbulence-inducing additives are disclosed.
Inventors
- 👤 Sally Lee Adams
- 👤 Fred David Martin
- 👤 Michael M. Cook
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-23 13:08
CPC Classifications
C; C09; C09K; C09K8/00; C09K8/42; C09K8/46; C04; C04B; C04B24/00; C04B24/16
Claims Analysis
Total Claims: 12
Claim 1
Independent Claim
211 words
In the method of cementing a well comprising the step of pumping an aqueous hydraulic cement slurry into place in the annular space between the well casing and the well bore-hole, the improvement comprising employing therein an aqueous hydraulic cement slurry composition having improved flow properties comprising hydraulic cement in admixture with from about 0.01 to about 5.0 percent by weight, based on weight of hydraulic cement on a dry basis, of a polyamido-sulfonic compound having recurring units represented by the following formula: ##STR3##wherein R 1 is hydrogen or methyl; R 2 , R 3 , R 4 , and R 5 are each independently selected from the group consisting of hydrogen, phenyl, straight or branched alkyl of from one to twelve carbon atoms, and cycloalkyl of up to six carbon atoms; R 6 is straight or branched alkyl of one to twelve carbon atoms, cycloalkyl of up to six carbon atoms, phenyl, or is absent; A is hydrogen, alkali metal ion or ammonium; and n is an integer of from 2 to about 100, such that the weight average molecular weight of the polyamido-sulfonic compound is from about 200 to about 10,000; and sufficient water to make a pumpable slurry which is capable of setting to form a monolithic solid.
Claim 2
Dependent Claim
211 words
In the method of cementing a well comprising the step of pumping an aqueous hydraulic cement slurry into place in the annular space between the well casing and the well bore-hole, the improvement comprising employing therein an aqueous hydraulic cement slurry composition having improved flow properties comprising hydraulic cement in admixture with from about 0.01 to about 5.0 percent by weight, based on weight of hydraulic cement on a dry basis, of a polyamido-sulfonic compound having recurring units represented by the following formula: ##STR3##wherein R 1 is hydrogen or methyl; R 2 , R 3 , R 4 , and R 5 are each independently selected from the group consisting of hydrogen, phenyl, straight or branched alkyl of from one to twelve carbon atoms, and cycloalkyl of up to six carbon atoms; R 6 is straight or branched alkyl of one to twelve carbon atoms, cycloalkyl of up to six carbon atoms, phenyl, or is absent; A is hydrogen, alkali metal ion or ammonium; and n is an integer of from 2 to about 100, such that the weight average molecular weight of the polyamido-sulfonic compound is from about 200 to about 10,000; and sufficient water to make a pumpable slurry which is capable of setting to form a monolithic solid.
Claim 3
Dependent Claim
28 words
The method of claim 1 wherein the weight average molecular weight of the polyamido-sulfonic compound contained in the composition employed therein is from about 200 to about 1,500.
Claim 4
Dependent Claim
47 words
The method of claim 1 wherein for the said cement slurry composition employed therein, the said polyamido-sulfonic compound is admixed with the hydraulic cement in an amount of from about 0.1 to about 2.0 percent by weight, based on weight of hydraulic cement on a dry basis.
Claim 5
Dependent Claim
41 words
The method of claim 1 wherein for the said cement slurry composition employed therein, the water is present in an amount of from about 25 to about 60 percent by weight, based on weight of hydraulic cement on a dry basis.
Claim 6
Dependent Claim
20 words
The method of claim 1 wherein the polyamido-sulfonic compound is poly-(2-acrylamido-2-methylpropane-1-sulfonic acid) comprising recurring units of the following formula: ##STR4##
Claim 7
Dependent Claim
237 words
In the method of cementing a well, comprising the step of pumping into place in the annular space between the well casing and the well bore-hole an aqueous hydraulic cement slurry which is flowing in turbulence for the purpose of removing any drilling fluid filter cake accumulated on the well bore-hole surface, the improvement comprising employing therein an aqueous hydraulic cement slurry composition being more readily induced to flow in turbulence, comprising hydraulic cement in admixture with from about 0.01 to about 5.0 percent by weight, based on weight of hydraulic cement on a dry basis, of a polyamido-sulfonic compound having recurring units represented by the following formula: wherein R 1 , is hydrogen or methyl; R 2 , R 3 , R 4 , and R 5 are each independently selected from the group consisting of hydrogen, phenyl, straight or branched alkyl of from one to twelve carbon atoms, and cycloalkyl of up to six carbon atoms; R 6 is straight or branched alkyl of one to twelve carbon atoms, cycloalkyl of up to six carbon atoms, phenyl, or is absent; A is hydrogen, alkali metal ion or ammonium; and n is an integer of from 2 to about 100, such that the weight average molecular weight of the polyamido-sulfonic compound is from about 200 to about 10,000; and sufficient water to make a pumpable slurry which is capable of setting to form a monolithic solid.
Claim 8
Dependent Claim
237 words
In the method of cementing a well, comprising the step of pumping into place in the annular space between the well casing and the well bore-hole an aqueous hydraulic cement slurry which is flowing in turbulence for the purpose of removing any drilling fluid filter cake accumulated on the well bore-hole surface, the improvement comprising employing therein an aqueous hydraulic cement slurry composition being more readily induced to flow in turbulence, comprising hydraulic cement in admixture with from about 0.01 to about 5.0 percent by weight, based on weight of hydraulic cement on a dry basis, of a polyamido-sulfonic compound having recurring units represented by the following formula: wherein R 1 , is hydrogen or methyl; R 2 , R 3 , R 4 , and R 5 are each independently selected from the group consisting of hydrogen, phenyl, straight or branched alkyl of from one to twelve carbon atoms, and cycloalkyl of up to six carbon atoms; R 6 is straight or branched alkyl of one to twelve carbon atoms, cycloalkyl of up to six carbon atoms, phenyl, or is absent; A is hydrogen, alkali metal ion or ammonium; and n is an integer of from 2 to about 100, such that the weight average molecular weight of the polyamido-sulfonic compound is from about 200 to about 10,000; and sufficient water to make a pumpable slurry which is capable of setting to form a monolithic solid.
Claim 9
Dependent Claim
28 words
The method of claim 6 wherein the weight average molecular weight of the polyamido-sulfonic compound contained in the composition employed therein is from about 200 to about 1,500.
Claim 10
Dependent Claim
47 words
The method of claim 6 wherein for the said cement slurry composition employed therein, the said polyamido-sulfonic compound is admixed with the hydraulic cement in an amount of from about 0.1 to about 2.0 percent, by weight, based on weight of hydraulic cement on a dry basis.
Claim 11
Dependent Claim
41 words
The method of claim 6 wherein for the said cement slurry composition employed therein, the water is present in an amount of from about 25 to about 60 percent by weight, based on weight of hydraulic cement on a dry basis.
Claim 12
Dependent Claim
21 words
The method of claim 6 wherein the polyamido-sulfonic compound is poly-(2-acrylamido-2-methylpropane-1-sulfonic acid) comprising recurring units represented by the following formula: ##STR5##
References Cited (Backward Citations)
US2582459A
Cited
US2761856A
Cited
US2761834A
Cited
US3024221A
Cited
US3344174A
Cited
US3250736A
Cited
US3332904A
Cited
US3547899A
Cited
US3692673A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1980-03-14 | 1980-09-13 | 1981-03-15 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1984-03-14 | 1984-09-13 | 1985-03-15 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1988-03-14 | 1988-09-13 | 1989-03-15 | $7700.00 | Window Closed / Lapsed |