Patent US4011072A successfully refreshed from Google Patents.
← Back to Patent Explorer
US4011072A Expired / Lapsed US ⏱️ 0.0 years remaining

Flotation of oxidized copper ores

Assignee: Inspiration Consolidated Copper Co
•
Filing: 1975-05-27
•
Granted: 1977-03-08
•
Expires: 1995-05-27
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract Copper is recovered from an aqueous pulp of an ore containing both sulfide minerals and oxidized minerals by continuously monitoring the EMF of the pulp and adding a water-soluble sulfide to the pulp in an amount from 0.05 to 7 pounds of contained sulfur per ton of ore whenever and for so long as the pump EMF is above about -30 millivolts with reference to a standard silver-silver chloride electrode, and discontinuing such addition whenever such EMF in less than about -30 millivolts. Thereafter the pulp is subjected to a froth flotation operation in the presence of a collector for copper sulfide minerals to produce a concentrate containing most of the sulfide minerals and a substantial part of the oxidized minerals of the ore.

Inventors

  • 👤 James B. Holman
  • 👤 John A. Cronin
  • 👤 Bernhard Lamby

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-01 10:20
CPC Classifications
B; B03; B03B; B03B13/00; B03B13/005; B03D; B03D1/00; B03D1/08; B03D1/10

Claims Analysis

Total Claims: 5
Claim 1
Independent Claim 181 words
The method of recovering copper by froth flotation from an aqueous pulp of an ore containing both sulfide and oxidized minerals of copper which comprises subjecting an aqueous pulp of the ore to a first froth flotation operation in the presence of a collector for sulfide copper minerals, thereby producing a concentrate containing a large proportion of the sulfide copper minerals, then subjecting the residual ore pulp to a further operation which comprises continuously monitoring the EMF of the pulp, adding a water-soluble sulfide to the pulp in an amount from 0.05 to 7 pounds contained sulfur per ton of ore whenever and for so long as the pulp EMF rises above about -30 millivolts with reference to a silver-silver chloride standard electrode and discontinuing such addition whenever such EMF becomes less than about -30 millivolts, and thereafter subjecting the pulp to a second froth flotation operation in the presence of a collector for copper sulfide minerals, thereby producing a concentrate containing much of the remaining sulfide copper minerals and a substantial part of the oxidized copper minerals of the ore.
Claim 2
Independent Claim 181 words
The method of recovering copper by froth flotation from an aqueous pulp of an ore containing both sulfide and oxidized minerals of copper which comprises subjecting an aqueous pulp of the ore to a first froth flotation operation in the presence of a collector for sulfide copper minerals, thereby producing a concentrate containing a large proportion of the sulfide copper minerals, then subjecting the residual ore pulp to a further operation which comprises continuously monitoring the EMF of the pulp, adding a water-soluble sulfide to the pulp in an amount from 0.05 to 7 pounds contained sulfur per ton of ore whenever and for so long as the pulp EMF rises above about -30 millivolts with reference to a silver-silver chloride standard electrode and discontinuing such addition whenever such EMF becomes less than about -30 millivolts, and thereafter subjecting the pulp to a second froth flotation operation in the presence of a collector for copper sulfide minerals, thereby producing a concentrate containing much of the remaining sulfide copper minerals and a substantial part of the oxidized copper minerals of the ore.
Claim 3
Dependent Claim 29 words
The method according to claim 1 wherein the pH of the pulp at the time of addition of the soluble sulfide is in the range from 8 to 11.
Claim 4
Dependent Claim 38 words
The method according to claim 1 wherein the water-soluble sulfide is selected from the group consisting of sodium hydrosulfide (NaHS), sodium sulfide (Na 2 S), hydrogen sulfide (H 2 S), and ammonium sulfide ((NH 4 ) 2 S).
Claim 5
Dependent Claim 31 words
The method according to claim 3 wherein the soluble sulfide is sodium hydrosulfide and the amount added to the ore pulp is from 0.1 to 10 pounds per ton of ore.

References Cited (Backward Citations)

US3421850A Cited
US3582317A Cited
US3667690A Cited
US3735931A Cited
US3883421A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1980-03-07 1980-09-06 1981-03-08 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1984-03-07 1984-09-06 1985-03-08 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1988-03-07 1988-09-06 1989-03-08 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag