Abstract

Abstract Coatings having a matt finish are made by applying a powder varnish composition to a substrate and thereafter reacting the varnish at a temperature of 100° to 240° C to form the matt finish coating. The powder varnish composition is a finely divided, particulate mixture of I. a 1,2-epoxy compound having a melting point greater than 40° C and containing at least one 1,2-epoxy group; and Ii. a salt of a polycarboxylic acid (such as pyromellite acid) containing three or more carboxyl groups and a cyclic amidine (such as 2-phenylimidazoline).

Inventors

  • 👤 Felix Schulde
  • 👤 Johann Obendorf
  • 👤 Kurt Neubold
  • 👤 Gunter Dormann

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-09 20:47
CPC Classifications
B; B05; B05D; B05D5/00; B05D5/02; C; C08; C08G; C08G59/00; C08G59/18; C08G59/40; C08G59/50; C08G59/5093; C08K; C08K5/00; C08K5/04; C08K5/09; B05D2401/00; B05D2401/30; B05D2401/32; Y; Y10; Y10S; Y10S525/00; Y10S525/934

Claims Analysis

Total Claims: 8
Claim 1
Independent Claim 150 words
Method for making matt finish coatings which comprises a. applying a powder varnish to a substrate, said powder varnish comprising a finely divided mixture of i. a 1,2-epoxy compound having at least one 1,2-epoxy group in the molecule and a lower melting point greater than 40° C; and ii. a salt of a polycarboxylic acid having three or more carboxyl groups; and a cyclic amidine having the formula ##STR3## wherein R is H, alkyl or aryl; R' is the same as R and in addition cycloalkyl, or a heterocycloalkyl radical obtained by substituting one or more --N--, --S--, and/or --O-- atoms in a cycloalkyl ring; R" is alkyl and aryl substituted alkylene or arylene; and X hydrogen or the radical ##STR4## wherein R and R" are as defined previously; and b. thereafter reacting said powder varnish at a temperature of 100° to 240° C to form a matt finish coating.
Claim 2
Dependent Claim 150 words
Method for making matt finish coatings which comprises a. applying a powder varnish to a substrate, said powder varnish comprising a finely divided mixture of i. a 1,2-epoxy compound having at least one 1,2-epoxy group in the molecule and a lower melting point greater than 40° C; and ii. a salt of a polycarboxylic acid having three or more carboxyl groups; and a cyclic amidine having the formula ##STR3## wherein R is H, alkyl or aryl; R' is the same as R and in addition cycloalkyl, or a heterocycloalkyl radical obtained by substituting one or more --N--, --S--, and/or --O-- atoms in a cycloalkyl ring; R" is alkyl and aryl substituted alkylene or arylene; and X hydrogen or the radical ##STR4## wherein R and R" are as defined previously; and b. thereafter reacting said powder varnish at a temperature of 100° to 240° C to form a matt finish coating.
Claim 3
Dependent Claim 22 words
Method of claim 1 wherein said salt is present in amounts of 2 to 15 weight percent, based on the epoxy compound.
Claim 4
Dependent Claim 25 words
Method of claim 1 wherein the polycarboxylic acid and the cyclic amidine are in a molar ratio of 1 : 1 to 1 : 4.
Claim 5
Dependent Claim 24 words
Method of claim 1 wherein the polycarboxylic acid is selected from the group of trimellite acid, pyromellite acid, butane tetracarboxylic acid and cyclo-pentanetetracarboxylic acid.
Claim 6
Dependent Claim 10 words
Method of claim 1 wherein the cyclic amidine is 2-phenylimidazoline.
Claim 7
Dependent Claim 14 words
Method of claim 1 wherein the salt of pyromellite acid and 2-phenylimidazoline is used.
Claim 8
Dependent Claim 24 words
Method of claim 1 wherein the salt is the reaction product of 1 mole of pyromellite acid with 2 or 4 moles 2-phenylimidazoline used.

References Cited (Backward Citations)

US3324198A Cited
US3549592A Cited
US3746686A Cited
US3842035A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1980-02-08 1980-08-09 1981-02-08 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1984-02-08 1984-08-09 1985-02-08 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1988-02-08 1988-08-09 1989-02-08 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag