Abstract

Abstract A process is provided for melting glass forming ingredients by supplying all, or at least part, of the total heat required for such melting from the combustion of a combustible fuel which is an admixture of particulate coal and oil. The melting operating can be accomplished without any difficulty of temperature control and with no adverse effects on the quality or composition of the final glass. Excellent results are obtained employing, for example, a combustible fuel mixture of about 40% by weight of particulate coal having a particle size less than about 200 mesh and about 60% by weight of Number 2 fuel oil.

Inventors

  • 👤 Valdis R. Daiga

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-09 03:59
CPC Classifications
C; C03; C03B; C03B5/00; C03B5/16; C03B5/235

Claims Analysis

Total Claims: 11
Claim 1
Independent Claim 58 words
In a method of manufacturing glass comprising discharging glass forming ingredients unto a pool of molten glass and burning a combustible fuel above the surface of said pool so as to produce a source of heat to convert said ingredients to a molten glass the improvement wherein said fuel is a preslurried mixture of a coal and oil.
Claim 2
Dependent Claim 58 words
In a method of manufacturing glass comprising discharging glass forming ingredients unto a pool of molten glass and burning a combustible fuel above the surface of said pool so as to produce a source of heat to convert said ingredients to a molten glass the improvement wherein said fuel is a preslurried mixture of a coal and oil.
Claim 3
Dependent Claim 50 words
The improvement of claim 1 and further including flowing a gaseous medium above said pool of glass at a sufficient velocity to pneumatically convey substantially all of the ash residue of the burned coal above said pool and maintain substantially all of said ash in noncontacting relation to said pool.
Claim 4
Dependent Claim 16 words
The improvement of claim 2 wherein said velocity is at least about 12 feet per second.
Claim 5
Dependent Claim 31 words
The improvement of claim 1 wherein said coal has a particle size of less than about 200 mesh and wherein said mixture has a viscosity of less than about 820 centipoise.
Claim 6
Dependent Claim 20 words
The improvement of claim 4 wherein said fuel is about 40 weight percent coal and about 60 weight percent oil.
Claim 7
Dependent Claim 84 words
In a method of manufacturing glass comprising adding glass forming ingredients to a melting chamber, said ingredients being capable of being melted to form a pool of molten glass in said chamber, supplying a combustible fuel to a burner disposed in said chamber above the level of said pool and burning said fuel so as to provide heat to melt said ingredients and form a molten pool of glass, the improvement wherein said fuel comprises a preslurried mixture of particulate coal and fuel oil.
Claim 8
Dependent Claim 84 words
In a method of manufacturing glass comprising adding glass forming ingredients to a melting chamber, said ingredients being capable of being melted to form a pool of molten glass in said chamber, supplying a combustible fuel to a burner disposed in said chamber above the level of said pool and burning said fuel so as to provide heat to melt said ingredients and form a molten pool of glass, the improvement wherein said fuel comprises a preslurried mixture of particulate coal and fuel oil.
Claim 9
Dependent Claim 48 words
The improvement of claim 6 and further including maintaining a gaseous flow in said chamber above said pool of a velocity sufficient to suspend substantially all of the residual ash of the burned coal in said gas flow so as to pneumatically convey said ash from said chamber.
Claim 10
Dependent Claim 38 words
In a method for manufacturing glass comprising burning a combustible fuel so as to produce heat to convert glass forming ingredients to molten glass the improvement wherein said fuel is a preslurried admixture of particulate coal and oil.
Claim 11
Dependent Claim 38 words
In a method for manufacturing glass comprising burning a combustible fuel so as to produce heat to convert glass forming ingredients to molten glass the improvement wherein said fuel is a preslurried admixture of particulate coal and oil.

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1980-02-01 1980-08-02 1981-02-01 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1984-02-01 1984-08-02 1985-02-01 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1988-02-01 1988-08-02 1989-02-01 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag