Abstract
Abstract A binary or ternary graft-copolymer excellent in both tensile strength and impact resistance is obtained by the process for producing a binary or ternary graft-copolymer consisting essentially of an ethylene-propylene rubber and an aromatic vinyl compound or of an ethylene-propylene rubber, an aromatic vinyl compound, and a vinyl cyanide compound, characterized by subjecting these materials to solution polymerization in a mixed solvent comprising an aliphatic hydrocarbon solvent capable of dissolving the ethylene-propylene rubber and a polar solvent capable of dissolving a poly-(aromatic vinyl compound) or a copolymer of the aromatic vinyl compound and the vinyl cyanide compound.
Inventors
- 👤 Masayoshi Morimoto
- 👤 Tetsutaro Sanjiki
- 👤 Hideki Horiike
- 👤 Takeo Oyamada
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-06 14:06
CPC Classifications
C; C08; C08F; C08F255/00; C08F255/02
Claims Analysis
Total Claims: 2
Claim 1
Independent Claim
304 words
A binary or ternary graft-copolymer obtained by the process for producing a binary or ternary graft-copolymer consisting essentially of an ethylene-propylene rubber and an aromatic vinyl compound or of an ethylene-propylene rubber, an aromatic vinyl compound and a vinyl cyanide compound, the ethylene-propylene rubber comprising ethylene and propylene in a molar ratio of 5 : 1 to 1 : 2 and being selected from the group consisting of two-component polymer comprising ethylene and propylene and ethylene-propylene-diene terpolymer containing as a third component a diene selected from the group consisting of dicyclopentadiene, ethylidenenorbornene, 1,4-hexadiene, 1,3-cycloctadiene, 1,5-hexadiene, 1,7-octadiene or 1,4-pentadiene and a proportion of the diene component being 4 to 50 in terms of iodine value, the aromatic vinyl compound being selected from the group consisting of styrene, α-methylstyrene, α-chlorostyrene, and dimethylstyrene, and the vinyl cyanide compound being selected from the group consisting of acrylonitrile and methacrylonitrile, which comprises subjecting these materials to solution polymerization in the presence of a radical catalyst at a temperature of 50° to 120°C for 5 to 25 hours in a mixed solvent comprising 5 to 95% by weight of an aliphatic hydrocarbon solvent capable of dissolving the ethylene-propylene rubber and 95 to 5% by weight of a polar solvent capable of dissolving a poly-(aromatic vinyl compound) in the case of the binary graft-copolymer, or of dissolving a copolymer of the aromatic vinyl compound and the vinyl cyanide compound in the case of the ternary graft-copolymer, the aliphatic hydrocarbon solvent being selected from the group consisting of paraffins and cycloparaffins having 5 to 10 carbon atoms, cyclopentanes having substituent alkyl groups of 1 to 4 carbon atoms, and cyclohexanes having substituent alkyl groups of 1 to 4 carbon atoms, and the polar solvent being selected from the group consisting of ketones, esters, ethers, chlorine-substituted aliphatic hydrocarbons, nitrogen-containing hydrocarbons, and sulfurcontaining hydrocarbons.
Claim 2
Dependent Claim
304 words
A binary or ternary graft-copolymer obtained by the process for producing a binary or ternary graft-copolymer consisting essentially of an ethylene-propylene rubber and an aromatic vinyl compound or of an ethylene-propylene rubber, an aromatic vinyl compound and a vinyl cyanide compound, the ethylene-propylene rubber comprising ethylene and propylene in a molar ratio of 5 : 1 to 1 : 2 and being selected from the group consisting of two-component polymer comprising ethylene and propylene and ethylene-propylene-diene terpolymer containing as a third component a diene selected from the group consisting of dicyclopentadiene, ethylidenenorbornene, 1,4-hexadiene, 1,3-cycloctadiene, 1,5-hexadiene, 1,7-octadiene or 1,4-pentadiene and a proportion of the diene component being 4 to 50 in terms of iodine value, the aromatic vinyl compound being selected from the group consisting of styrene, α-methylstyrene, α-chlorostyrene, and dimethylstyrene, and the vinyl cyanide compound being selected from the group consisting of acrylonitrile and methacrylonitrile, which comprises subjecting these materials to solution polymerization in the presence of a radical catalyst at a temperature of 50° to 120°C for 5 to 25 hours in a mixed solvent comprising 5 to 95% by weight of an aliphatic hydrocarbon solvent capable of dissolving the ethylene-propylene rubber and 95 to 5% by weight of a polar solvent capable of dissolving a poly-(aromatic vinyl compound) in the case of the binary graft-copolymer, or of dissolving a copolymer of the aromatic vinyl compound and the vinyl cyanide compound in the case of the ternary graft-copolymer, the aliphatic hydrocarbon solvent being selected from the group consisting of paraffins and cycloparaffins having 5 to 10 carbon atoms, cyclopentanes having substituent alkyl groups of 1 to 4 carbon atoms, and cyclohexanes having substituent alkyl groups of 1 to 4 carbon atoms, and the polar solvent being selected from the group consisting of ketones, esters, ethers, chlorine-substituted aliphatic hydrocarbons, nitrogen-containing hydrocarbons, and sulfurcontaining hydrocarbons.
References Cited (Backward Citations)
US3538191A
Cited
US3538190A
Cited
US3538193A
Cited
US3538192A
Cited
US3642950A
Cited
US3683050A
Cited
US3671608A
Cited
US3657395A
Cited
US3819795A
Cited
US3876730A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1979-10-05 | 1980-04-05 | 1980-10-05 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1983-10-05 | 1984-04-05 | 1984-10-05 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1987-10-05 | 1988-04-05 | 1988-10-05 | $7700.00 | Window Closed / Lapsed |