Patent US3983087A successfully refreshed from Google Patents.
← Back to Patent Explorer
US3983087A Expired / Lapsed US ⏱️ 0.0 years remaining

Novel process of reclaiming polyurethane foam

Assignee: Pharmacia and Upjohn Co
•
Filing: 1975-07-25
•
Granted: 1976-09-28
•
Expires: 1995-07-25
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A process is described for converting scrap flexible polyurethane foam, derived from a polyether polyol, to a homogeneous mixture of polyols which can be used, alone or as a blend with other polyols, in the preparation of polyurethane foams. The process comprises heating the scrap foam with not more than its own weight of an aliphatic diol which has at least one alkyl substituent in the alkylene chain, and which optionally contains an oxygen atom in the alkylene chain. The scrap flexible foam can contain up to about 75 percent of scrap rigid or semi-flexible foam, if desired.

Inventors

  • 👤 Benjamin Tucker
  • 👤 Henri Ulrich

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-28 08:05
CPC Classifications
C; C08; C08J; C08J11/00; C08J11/04; C08J11/10; C08J11/18; C08J11/22; C08J11/24; C08G; C08G18/00; C08G18/06; C08G18/83; C08G18/831; C08J2375/00; C08J2375/04; Y; Y02; Y02W; Y02W30/00; Y02W30/50; Y02W30/62

Claims Analysis

Total Claims: 5
Claim 1
Independent Claim 71 words
A process for converting scrap flexible polyurethane foam, which foam has been derived from a polyether polyol, to a homogeneous mixture of polyols, which process comprises heating, at a temperature in the range of 180° C to 250° C, a mixture of (a) said scrap flexible foam and (b) 1,2-propylene glycol said glycol being present in an amount by weight which does not exceed the total weight of said scrap foam.
Claim 2
Dependent Claim 71 words
A process for converting scrap flexible polyurethane foam, which foam has been derived from a polyether polyol, to a homogeneous mixture of polyols, which process comprises heating, at a temperature in the range of 180° C to 250° C, a mixture of (a) said scrap flexible foam and (b) 1,2-propylene glycol said glycol being present in an amount by weight which does not exceed the total weight of said scrap foam.
Claim 3
Dependent Claim 34 words
The process of claim 1 wherein the said scrap flexible foam is employed in an amount by weight corresponding to from about 1 to about 2 times the amount by weight of said glycol.
Claim 4
Dependent Claim 36 words
The process of claim 1 wherein the said scrap flexible foam is employed in combination with scrap from a foam selected from the class consisting of semi-rigid polyurethane foam, rigid polyurethane foam, and rigid polyisocyanurate foam.
Claim 5
Dependent Claim 31 words
The process of claim 1 wherein the homogeneous polyol recovered from said scrap foam is reacted with an alkylene oxide selected from the group consisting of ethylene oxide and propylene oxide.

References Cited (Backward Citations)

US3632530A Cited
US3738946A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1979-09-28 1980-03-29 1980-09-28 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1983-09-28 1984-03-29 1984-09-28 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1987-09-28 1988-03-29 1988-09-28 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag