Patent US3975407A successfully refreshed from Google Patents.
← Back to Patent Explorer
US3975407A Expired / Lapsed US ⏱️ 0.0 years remaining

Method for producing maleic anhydride

Assignee: Kuraray Co Ltd
•
Filing: 1975-05-14
•
Granted: 1976-08-17
•
Expires: 1995-05-14
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract Maleic anhydride is obtained by oxidizing an unsaturated hydrocarbon having at least 4 carbon atoms in the presence of a catalyst consisting essentially of the oxides of phosphorus and tungsten, with small amounts of a catalyst promoter selected from compounds of alkali metals, alkaline earth metals, copper, zinc, chromium, bismuth and titanium.

Inventors

  • 👤 Ryuhei Ueeda

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-07 13:49
CPC Classifications
C; C07; C07C; C07C51/00; C07C51/16; C07C51/21; C07C51/25; C07C51/252; B; B01; B01J; B01J27/00; B01J27/14; B01J27/186; B01J27/188; B01J37/00; B01J37/28; C07C51/31; C07C51/313

Claims Analysis

Total Claims: 17
Claim 1
Independent Claim 102 words
A method for preparing maleic anhydride which comprises oxidizing a gaseous mixture containing an olefinic hydrocarbon having 4 or 5 carbon atoms or a hydrocarbon mixture thereof and oxygen or an oxygen-containing gas in a reaction zone in the presence of a catalyst consisting essentially of the oxides of tungsten and phosphorus, the atomic ratio of tungsten to phosphorus being less than 30, and at least one catalyst promoter selected from the group consisting of compounds of alkali metals, alkaline earth metals, alkaline earth metals, copper, zinc, chromium, bismuth and titanium at a temperature in the range of from 250°C. to 650°C.
Claim 2
Independent Claim 102 words
A method for preparing maleic anhydride which comprises oxidizing a gaseous mixture containing an olefinic hydrocarbon having 4 or 5 carbon atoms or a hydrocarbon mixture thereof and oxygen or an oxygen-containing gas in a reaction zone in the presence of a catalyst consisting essentially of the oxides of tungsten and phosphorus, the atomic ratio of tungsten to phosphorus being less than 30, and at least one catalyst promoter selected from the group consisting of compounds of alkali metals, alkaline earth metals, alkaline earth metals, copper, zinc, chromium, bismuth and titanium at a temperature in the range of from 250°C. to 650°C.
Claim 3
Dependent Claim 50 words
A method according to claim 1 in which the catalyst promoter is selected from (I) the oxides, hydroxides, nitrates, carbonates, sulfates, halides, acetates, phosphates and tungstates of alkali metals, alkaline earth metals, copper, zinc, chromium, bismuth and titanium, and (II) compounds which are converted to (I) upon calcination in air.
Claim 4
Dependent Claim 71 words
A method according to claim 2 wherein there is introduced into the reaction zone an additional compound selected from the group consisting of phosphine, phosphorus oxides, hydrophosphorous acid, phosphorous acid, diphosphorous acid, hypophosphoric acid, orthophosphoric acid, metaphosphoric acid, salts of phosphorous and phosphoric acid which are decomposed at the reaction temperature, and organophosphorus compounds of the formulae: ##STR2## wherein R is phenyl or lower alkyl and X is hydrogen or R.
Claim 5
Dependent Claim 14 words
A method according to claim 2 wherein the catalyst is supported on a carrier.
Claim 6
Dependent Claim 22 words
A method according to claim 1 wherein the catalyst consists essentially of a complex or a compound of tungsten, phosphorus and oxygen.
Claim 7
Dependent Claim 30 words
A method according to claim 1 wherein the catalyst consists essentially of oxides of tungsten and phosphorus, a complex or a compound of tungsten, phosphorus and oxygen, and mixtures thereof.
Claim 8
Dependent Claim 25 words
A method according to claim 1 wherein oxidation is effected by admixing said olefinic hydrocarbon with an oxidizing agent comprising oxygen or an oxygen-containing gas.
Claim 9
Dependent Claim 23 words
A method according to claim 6 wherein the molar ratio of olefinic hydrocarbon to oxygen is less than 1/10 or more than 1/2.
Claim 10
Dependent Claim 23 words
A method according to claim 1 wherein the gaseous hourly space velocity through the reaction zone ranges from 500 to 15,000 per hour.
Claim 11
Dependent Claim 48 words
A method according to claim 2 in which the catalyst promoter is selected from the group consisting of the oxides, hydroxides, chlorides, carbonates, sulfates, nitrates, phosphates and acetates of an alkali metal, the atomic ratio of the alkali metal to phosphorus ranging from about 0.001 to about 0.4.
Claim 12
Dependent Claim 50 words
A method according to claim 2 in which the catalyst promoter is selected from the group consising of the oxides, hydroxides, chlorides, carbonates, sulfates, nitrates, phosphates and acetates of an alkaline earth metal, the atomic ratio of the alkaline earth metal to phosphorus ranging from about 0.001 to about 100.
Claim 13
Dependent Claim 45 words
A method according to claim 2 in which the catalyst promoter is selected from the group consisting of cupric chloride, cuprous chloride, cupric sulfate, cuprous sulfate, cupric nitrate and cuprous nitrate, the atomic ratio of copper to phosphorus ranging from about 0.001 to about 2.0.
Claim 14
Dependent Claim 41 words
A method according to claim 2 in which the catlayst promoter is selected from the group consisting of zinc oxide, zinc chloride, zinc sulfate and zinc nitrate, the atomic ratio of zinc to phosphorus ranging from about 0.001 to about 1.0.
Claim 15
Dependent Claim 43 words
A method according to claim 1 in which the catalyst promoter is selected from the group consisting of chromium oxide, chromium chloride, chromium phosphate, chromium sulfate and chromic acid, the atomic ratio of chromium to phosphorus ranging from about 0.001 to about 1.0.
Claim 16
Dependent Claim 41 words
A method according to claim 2 in which the catalyst promoter is selected from the group consisting of bismuth nitrate, bismuth oxide, bismuth chloride and bismuth sulfate, the atomic ratio of bismuth to phosphorus ranging from about 0.001 to about 100.
Claim 17
Dependent Claim 43 words
A method according to claim 2 in which the catalyst promoter is selected from the group consisting of titanium dioxide, titanium nitrate, titanium sulfate, titanium trichloride and titanium tetrachloride, the atomic ratio of titanium to phosphorus ranging from about 0.001 to about 100.

References Cited (Backward Citations)

US3906008A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1979-08-17 1980-02-16 1980-08-17 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1983-08-17 1984-02-16 1984-08-17 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1987-08-17 1988-02-16 1988-08-17 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag