Abstract

Abstract The condensation product of oxalyl dihydrazide and a mono-ortho-hydroxy aryl ketone is found to be an effective metal deactivator in saturated hydrocarbon polymers. The stabilizer is usefully incorporated in primary insulation, for example in polyethylene insulation on copper wire.

Inventors

  • 👤 Ray Lawson Hartless
  • 👤 Anthony Marion Trozzolo

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-30 23:31
CPC Classifications
C; C08; C08K; C08K5/00; C08K5/16; C08K5/29; C08K5/30; Y; Y10; Y10T; Y10T428/00; Y10T428/31504; Y10T428/31678; Y10T428/31692

Claims Analysis

Total Claims: 8
Claim 1
Independent Claim 208 words
Article including at least one metallic portion in intimate contact with a plastic portion, said metallic portion including at least one element which accelerates the oxidative degradation of at least a component of the said plastic portion, the said plastic portion including a polymeric composition which is at least 90 percent by weight nominally ethylenically saturated polymer, exclusive of filler, the said plastic portion containing a metal deactivator to lessen the acceleration of oxidation degradation due to the said metallic portion said metal deactivator being contained within the range of from 0.01 percent to 5.0 percent by weight based on the said polymeric composition; characterized in that the said metal deactivator is of the structure ##EQU4## in which R is a methyl grouping or higher homologue alkyl grouping, in which Ar is a single aryl ring or fused aryl ring structure, in which the indicated hydroxy substituent is in a position ortho to the ##EQU5## grouping and is the only hydroxy substituent ortho to the said ##EQU6## grouping, in which there are permitted additional substituents on any ring position of the said Ar grouping other than that occupied by the said hydroxy grouping provided that such additional substituents do not include substituents which impair activity of hydroxy substituents.
Claim 2
Dependent Claim 208 words
Article including at least one metallic portion in intimate contact with a plastic portion, said metallic portion including at least one element which accelerates the oxidative degradation of at least a component of the said plastic portion, the said plastic portion including a polymeric composition which is at least 90 percent by weight nominally ethylenically saturated polymer, exclusive of filler, the said plastic portion containing a metal deactivator to lessen the acceleration of oxidation degradation due to the said metallic portion said metal deactivator being contained within the range of from 0.01 percent to 5.0 percent by weight based on the said polymeric composition; characterized in that the said metal deactivator is of the structure ##EQU4## in which R is a methyl grouping or higher homologue alkyl grouping, in which Ar is a single aryl ring or fused aryl ring structure, in which the indicated hydroxy substituent is in a position ortho to the ##EQU5## grouping and is the only hydroxy substituent ortho to the said ##EQU6## grouping, in which there are permitted additional substituents on any ring position of the said Ar grouping other than that occupied by the said hydroxy grouping provided that such additional substituents do not include substituents which impair activity of hydroxy substituents.
Claim 3
Dependent Claim 30 words
Article of claim 1 in which the said metal deactivator is characterized in that said hydroxy substituent ortho to said ##EQU7## grouping is the only substituent on said Ar ring.
Claim 4
Dependent Claim 17 words
Article of claim 2 in which the said polymer may be produced by the polymerization of ethylene.
Claim 5
Dependent Claim 12 words
Article of claim 1 in which the said metallic portion comprises copper.
Claim 6
Dependent Claim 20 words
Article of claim 1 in which the said plastic portion contains a thermal antioxidant in addition to the metal deactivator.
Claim 7
Dependent Claim 14 words
Article of claim 5 in which the said thermal antioxidant is a hindered phenol.
Claim 8
Dependent Claim 27 words
Article of claim 1 in which the said metal deactivator is of the structure ##EQU8## in which R is a methyl grouping or higher homologue alkyl grouping.

References Cited (Backward Citations)

US3357944A Cited
US3440210A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1979-07-20 1980-01-19 1980-07-20 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1983-07-20 1984-01-19 1984-07-20 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1987-07-20 1988-01-19 1988-07-20 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag