Patent US3966503A successfully refreshed from Google Patents.
← Back to Patent Explorer
US3966503A Expired / Lapsed US ⏱️ 0.0 years remaining

Method for making instantaneous scarfing starts

Assignee: ESAB AB
•
Filing: 1975-01-13
•
Granted: 1976-06-29
•
Expires: 1995-01-13
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A method for making an instantaneous thermochemical start on the surface of a ferrous metal workpiece, comprising the steps of: (a) contacting a preselected spot on said surface where the reaction is to begin, with the end of a ferrous metal wire which has been heated to its ignition temperature in an oxygen atmosphere, (b) impinging a high intensity jet of oxygen gas on said surface at a point 1 to 15 cm. behind said spot, thereby causing an immediate scarfing reaction to begin and a molten puddle to form at said spot, and (c) continuing the impingement of a high intensity jet of oxygen on said puddle until the puddle has spread to a preselected width. Thereafter, the spreading oxygen stream may be left on and used to carry out the scarfing reaction, or it may be turned off and another oxygen stream may be impinged on the spread puddle at an acute angle to the work surface in order to "take over" and carry out the scarfing reaction. The type of scarfing cut sought will determine the type of scarfing oxygen stream used to "take over" the scarfing reaction from the spreading stream.

Inventors

  • 👤 Stephen August Engel

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-29 17:01
CPC Classifications
B; B23; B23K; B23K7/00; B23K7/08; B23K7/06

Claims Analysis

Total Claims: 15
Claim 1
Independent Claim 123 words
A method for making an instantaneous thermochemical start on the surface of a ferrous metal workpiece comprising the steps of: a. contacting a preselected spot on said surface where the scarfing reaction is to begin, with the end of a ferrous metal wire which has been preheated to its ignition temperature in an oxygen atmosphere, and simultaneously therewith b. impinging a high intensity jet of oxygen gas on said surface at a point about 1 to 15 cm. behind said spot, thereby causing an instantaneous scarfing reaction to begin and a molten puddle to form at said spot, and thereafter c. continuing the impingement of a high intensity jet of oxygen on said puddle until said puddle has spread to a preselected width.
Claim 2
Independent Claim 123 words
A method for making an instantaneous thermochemical start on the surface of a ferrous metal workpiece comprising the steps of: a. contacting a preselected spot on said surface where the scarfing reaction is to begin, with the end of a ferrous metal wire which has been preheated to its ignition temperature in an oxygen atmosphere, and simultaneously therewith b. impinging a high intensity jet of oxygen gas on said surface at a point about 1 to 15 cm. behind said spot, thereby causing an instantaneous scarfing reaction to begin and a molten puddle to form at said spot, and thereafter c. continuing the impingement of a high intensity jet of oxygen on said puddle until said puddle has spread to a preselected width.
Claim 3
Dependent Claim 40 words
The method of claim 1 wherein relative motion between the workpiece and the means for producing said steps is caused to take place at normal scarfing speed prior to and throughout said steps without interruption, thereby producing a flying start.
Claim 4
Dependent Claim 34 words
The method of claim 1 wherein relative motion between said workpiece and the means for producing said steps is caused to commence at normal scarfing speed upon contact of said wire with said spot.
Claim 5
Dependent Claim 20 words
The method of claim 1 wherein the starting wire is preheated by flames impinged upon the end of said wire.
Claim 6
Dependent Claim 64 words
The method of claim 2 wherein the high velocity oxygen jet defined by step (b) is directed at said point from a position such that the included angle formed by the central axis of said jet and the line of travel on the work surface is between 30° and 80°, and such that the puddle is spread parallel to the direction of relative motion.
Claim 7
Dependent Claim 61 words
The method of claim 2 wherein the high velocity oxygen jet defined by step (b) is directed at said spot from a position such that the included angle formed by the central axis of said jet and the surface of the workpiece is between 30° and 80°. and such that the puddle is spread perpendicular to the direction of relative motion.
Claim 8
Dependent Claim 24 words
The method of claim 4 wherein said flames are directed against said surface and deflected upwards by said surface to impinge on said wire.
Claim 9
Dependent Claim 36 words
The method of claim 1 which in addition contains the step of d. scarfing said surface by impinging a sheet-like stream of scarfing oxygen on the molten puddle directed at an acute angle to said surface.
Claim 10
Dependent Claim 57 words
The method of claim 8 wherein said sheet-like stream of scarfing oxygen is gradually diminished in intensity towards the edges of said stream, reaching zero intensity at the lateral edges of the orifice from which it is discharged, thereby producing an individual, fin-free spot scarfing cut whose width is less than the width of said discharge orifice.
Claim 11
Dependent Claim 80 words
The method of claim 8 wherein said sheet-like stream of scarfing oxygen is gradually diminished in intensity towards the edges of said stream, but remaining greater than zero intensity at the lateral edges of the orifice from which it is discharged, thereby producing a fin-free spot scarfing cut which will not leave excessively high ridges or deep grooves between adjacent cuts made simultaneously and in like manner, said cut having a width equal to the width of said discharge orifice.
Claim 12
Dependent Claim 35 words
The method of claim 8 wherein said sheet-like stream of scarfing oxygen is substantially uniform in intensity across the entire width of the orifice from which it is discharged, thereby producing a conventional scarfing cut.
Claim 13
Dependent Claim 24 words
The method of claim 9 wherein the width of said cut produced is equal to or greater than the width of the started puddle.
Claim 14
Dependent Claim 24 words
The method of claim 10 wherein the width of said cut produced is equal to or greater than the width of the started puddle.
Claim 15
Dependent Claim 24 words
The method of claim 11 wherein the width of said cut produced is equal to or greater than the width of the started puddle.

References Cited (Backward Citations)

US2309096A Cited
US2438344A Cited
US3658599A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1979-06-29 1979-12-29 1980-06-29 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1983-06-29 1983-12-29 1984-06-29 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1987-06-29 1987-12-29 1988-06-29 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag