Thermoplastic blend composition

Assignee: Mitsubishi Gas Chemical Co Inc
•
Filing: 1974-04-18
•
Granted: 1976-06-15
•
Expires: 1994-04-18
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A thermoplastic blend composition having especially superior impact strength and fatigue resistance comprising 15 ro 80% by weight of a polyphenylene oxide, 16 to 75% by weight of a rubber-modified polystyrene, 2 to 15% by weight of an aromatic polycarbonate and 2 to 15% by weight of a high styrene rubber, the sum total of the proportions of these ingredients being 100% by weight.

Inventors

  • 👤 Eiichi Yonemitsu
  • 👤 Akitoshi Sugio
  • 👤 Takanari Nawata
  • 👤 Masanobu Masu
  • 👤 Masaharu Kimura
  • 👤 Norio Sayama

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-25 03:51
CPC Classifications
C; C08; C08L; C08L51/00; C08L51/04; C08L71/00; C08L71/08; C08L71/10; C08L71/12; C08L71/123; C08L69/00; Y; Y10; Y10S; Y10S525/00; Y10S525/905

Claims Analysis

Total Claims: 6
Claim 1
Independent Claim 262 words
In a thermoplastic blend composition having especially superior impact strength and fatigue resistance comprising A. 15 to 80% by weight of a polyphenylene oxide having a polymeric structure expressed by the following formula ##SPC2## wherein R 1 and R 2 are the same or different, and each represents a methyl or ethyl group, and n is a positive integer of at least 85, B. 16 to 75% by weight of a rubber-modified polystyrene having polymeric units of a conjugated diene monomer and polymeric units of an aromatic vinyl monomer, obtained by polymerizing the aromatic vinyl monomer in the presence of one member selected from the group consisting of a polymer of the conjugated diene monomer and a rubbery polymer which is a copolymer of the conjugated diene monomer and at least one monomer selected from the group consisting of ethylene, propylene, acrylonitrile and styrene, the content of said polymeric units of the conjugated diene monomer in the rubber-modified polystyrene being 2 to 15% by weight, and C. 2 to 15% by weight of an aromatic polycarbonate, the improvement wherein the composition further comprises D. 2 to 15% by weight of a high styrene rubber having polymeric units of a conjugated diene monomer and polymeric units of an aromatic vinyl monomer, obtained by copolymerizing the conjugated diene monomer and an aromatic vinyl monomer, the content of said polymeric units of the aromatic vinyl monomer in the high styrene rubber being 35 to 65% by weight, the sum total of the proportions of the components (A), (B), (C) and (D) being 100% by weight.
Claim 2
Dependent Claim 262 words
In a thermoplastic blend composition having especially superior impact strength and fatigue resistance comprising A. 15 to 80% by weight of a polyphenylene oxide having a polymeric structure expressed by the following formula ##SPC2## wherein R 1 and R 2 are the same or different, and each represents a methyl or ethyl group, and n is a positive integer of at least 85, B. 16 to 75% by weight of a rubber-modified polystyrene having polymeric units of a conjugated diene monomer and polymeric units of an aromatic vinyl monomer, obtained by polymerizing the aromatic vinyl monomer in the presence of one member selected from the group consisting of a polymer of the conjugated diene monomer and a rubbery polymer which is a copolymer of the conjugated diene monomer and at least one monomer selected from the group consisting of ethylene, propylene, acrylonitrile and styrene, the content of said polymeric units of the conjugated diene monomer in the rubber-modified polystyrene being 2 to 15% by weight, and C. 2 to 15% by weight of an aromatic polycarbonate, the improvement wherein the composition further comprises D. 2 to 15% by weight of a high styrene rubber having polymeric units of a conjugated diene monomer and polymeric units of an aromatic vinyl monomer, obtained by copolymerizing the conjugated diene monomer and an aromatic vinyl monomer, the content of said polymeric units of the aromatic vinyl monomer in the high styrene rubber being 35 to 65% by weight, the sum total of the proportions of the components (A), (B), (C) and (D) being 100% by weight.
Claim 3
Dependent Claim 30 words
The composition of claim 1 wherein the rubber-modified polystyrene contains polymeric units of at least one aromatic vinyl monomer selected from the group consisting of styrene, chlorostyrene, and α-methyl styrene.
Claim 4
Dependent Claim 55 words
The composition of claim 1 wherein the rubber-modified polystyrene contains polymeric units of a vinyl monomeric mixture in which said aromatic vinyl monomer is included in a proportion of at least 50% by weight and the other is at least one vinyl monomer selected from the group consisting of acrylonitrile, alkyl methacrylate and alkyl acrylate.
Claim 5
Dependent Claim 24 words
The composition of claim 1 wherein said conjugated diene monomer is at least one member selected from the group consisting of butadiene and isoprene.
Claim 6
Dependent Claim 29 words
A composition according to claim 1 wherein the rubber-modified polystyrene (B) is a graft polymer of polybutadiene and styrene and the high styrene rubber (D) is a styrene-butadiene copolymer.

References Cited (Backward Citations)

US3221080A Cited
US3663471A Cited
US3660531A Cited
US3801673A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1979-06-15 1979-12-15 1980-06-15 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1983-06-15 1983-12-15 1984-06-15 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1987-06-15 1987-12-15 1988-06-15 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag