Patent US3963592A successfully refreshed from Google Patents.
← Back to Patent Explorer
US3963592A Expired / Lapsed US ⏱️ 0.0 years remaining

Method for the electrolytic production of alkali

Assignee: Occidental Chemical Corp
•
Filing: 1974-09-30
•
Granted: 1976-06-15
•
Expires: 1994-09-30
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A method whereby an alkali, such as an alkali metal hydroxide, is produced at the cathode by the electrolysis of aqueous alkali metal halide solutions and the process is operated to produce either chlorine or HCl at the anode.

Inventors

  • 👤 Olle Lindstrom

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-26 21:47
CPC Classifications
C; C25; C25B; C25B11/00; C25B11/04; C25B9/00; C25B9/70; C25B1/00; C25B1/01; C25B1/14; C25B1/16; C25B11/051

Claims Analysis

Total Claims: 3
Claim 1
Independent Claim 147 words
In the process for electrolyzing an aqueous solution of an alkali metal chloride to form an alkali metal hydroxide at the cathode and chlorine at the anode by the oxidation of chloride ions in the anolyte, the improvement which comprises introducing hydrogen gas at the anode, preferentially anodically oxidizing said hydrogen gas in the presence of a catalyst to hydrogen ions by passing said hydrogen gas through a porous anode containing the catalyst into the anolyte and reacting the thus-formed hydrogen ions with the chloride ions in the anolyte, the porous anode through which the hydrogen gas is passed being formed in two layers, said first layer being a porous sintered coarse layer of platinized titanium and said second layer being a porous sintered finer layer of titanium, the hydrogen gas being passed initially through said first layer and then through said second layer into the anolyte.
Claim 2
Dependent Claim 147 words
In the process for electrolyzing an aqueous solution of an alkali metal chloride to form an alkali metal hydroxide at the cathode and chlorine at the anode by the oxidation of chloride ions in the anolyte, the improvement which comprises introducing hydrogen gas at the anode, preferentially anodically oxidizing said hydrogen gas in the presence of a catalyst to hydrogen ions by passing said hydrogen gas through a porous anode containing the catalyst into the anolyte and reacting the thus-formed hydrogen ions with the chloride ions in the anolyte, the porous anode through which the hydrogen gas is passed being formed in two layers, said first layer being a porous sintered coarse layer of platinized titanium and said second layer being a porous sintered finer layer of titanium, the hydrogen gas being passed initially through said first layer and then through said second layer into the anolyte.
Claim 3
Dependent Claim 27 words
The process as claimed in claim 1 wherein the hydrogen gas introduced at the anode is at least partially supplied by hydrogen gas formed at the cathode.

References Cited (Backward Citations)

US3124520A Cited
US3282834A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1979-06-15 1979-12-15 1980-06-15 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1983-06-15 1983-12-15 1984-06-15 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1987-06-15 1987-12-15 1988-06-15 $7700.00 Window Closed / Lapsed