Patent US3962140A successfully refreshed from Google Patents.
← Back to Patent Explorer
US3962140A Expired / Lapsed US ⏱️ 0.0 years remaining

Nickel-copper-molybdenum methanation catalyst

Assignee: Harshaw Chemical Co
•
Filing: 1975-03-10
•
Granted: 1976-06-08
•
Expires: 1995-03-10
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A supported methanation catalyst and a process for utilizing the catalyst are disclosed. The catalyst yields a product containing a major proportion of methane and some ethane. Methanation of a gaseous feed stream containing from about 10 to about 50 mole percent carbon monoxide, and from about 1.0 to about 3.0 times as much hydrogen as carbon monoxide, is effected at elevated temperature and high pressure continuously over a prolonged period of time, while a conversion of carbon monoxide in excess of 80 mole percent is maintained. Thermal stability at elevated temperature and pressure permits essentially continuous use of the catalyst for extended periods of time without time-consuming shutdowns. High conversion of gaseous feed and thermal stability of catalyst permits economical process design which utilizes a minimal recycle, if any. The supported catalyst consists essentially of a complex of oxides of nickel, copper and molybdenum which complex is reduced on the support prior to or during use. The complex of oxides consists of from about 5 to about 20 percent by weight molybdenum oxide, and from about 5 to about 40 percent by weight nickel oxide, each amount based on total catalyst, present in a weight ratio of nickel oxide to copper oxide in the range from 1:1 to about 9:1, and preferably in the range from about 1 to about 3.

Inventors

  • 👤 William R. Alcorn
  • 👤 Leonard A. Cullo

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-08 06:32
CPC Classifications
C; C10; C10K; C10K3/00; C10K3/02; C10K3/04; B; B01; B01J; B01J23/00; B01J23/70; B01J23/76; B01J23/84; B01J23/85; B01J23/88; B01J23/885; C07; C07C; C07C1/00; C07C1/02; C07C1/04; C07C1/0425; C07C1/043; C07C1/0435; C07C2523/00; C07C2523/16; C07C2523/24; C07C2523/28; C07C2523/70; C07C2523/72; C07C2523/74; C07C2523/755; C07C2523/76; C07C2523/84; C07C2523/85; C07C2523/88; C07C2523/885

Claims Analysis

Total Claims: 4
Claim 1
Independent Claim 167 words
A supported methanation catalyst for the production of gaseous hydrocarbon mixtures, composed predominantly of methane with up to about 5 percent of ethane, on a moisture-free basis, said catalyst prepared by reduction with hydrogen of a complex of oxides on a catalyst support, said complex defined by the formula Ni a Cu b Mo c O x, wherein a, b and c are numbers so chosen that when b is unity, a and c are in the range from about 1 to about 9, and x is a number determined by the valence requirements of the other elements present, wherein the support comprises at least 50 percent of the total weight of the catalyst, the remainder including from about 5% to about 20% by weight of molybdenum oxide, based on total catalyst, from about 5% to about 40% by weight of nickel oxide, and copper oxide, wherein the weight ratio of the nickel oxide to the copper oxide is in the range from about 1:1 and 9:1.
Claim 2
Dependent Claim 167 words
A supported methanation catalyst for the production of gaseous hydrocarbon mixtures, composed predominantly of methane with up to about 5 percent of ethane, on a moisture-free basis, said catalyst prepared by reduction with hydrogen of a complex of oxides on a catalyst support, said complex defined by the formula Ni a Cu b Mo c O x, wherein a, b and c are numbers so chosen that when b is unity, a and c are in the range from about 1 to about 9, and x is a number determined by the valence requirements of the other elements present, wherein the support comprises at least 50 percent of the total weight of the catalyst, the remainder including from about 5% to about 20% by weight of molybdenum oxide, based on total catalyst, from about 5% to about 40% by weight of nickel oxide, and copper oxide, wherein the weight ratio of the nickel oxide to the copper oxide is in the range from about 1:1 and 9:1.
Claim 3
Dependent Claim 26 words
The supported catalyst of claim 1 wherein the support is present in an amount from about 70% to about 95% by weight of the finished catalyst.
Claim 4
Dependent Claim 21 words
The supported catalyst of claim 1 wherein the weeight ratio of nickel oxide ot molybdenum oxide is between 0.2 and 5.

References Cited (Backward Citations)

US3854895A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1979-06-08 1979-12-08 1980-06-08 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1983-06-08 1983-12-08 1984-06-08 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1987-06-08 1987-12-08 1988-06-08 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag