Patent US3960969A successfully refreshed from Google Patents.
← Back to Patent Explorer
US3960969A Expired / Lapsed US ⏱️ 0.0 years remaining

Method for preparing an improved creosote wood preservative from a coal tar creosote by the use of caustic compounds

Assignee: Koppers Inc
•
Filing: 1975-02-07
•
Granted: 1976-06-01
•
Expires: 1995-02-07
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract An improved creosote wood preservative that has a light color and that forms a non-sticky crud deposit is prepared from a coal tar creosote. The coal tar creosote is distilled to an end temperature in the range of 395° to 410°C. at atmospheric pressure. This distillation produces a distillate and a pitch residue. The distillate is contacted with at least 1% by weight of one or more of the following caustic compounds: alkali metal alcoholates of alkali metal hydroxides to produce the improved creosote wood preservative. The pitch residue from distillation is recovered and it is utilized in the production of various pitch products or in combustion for its fuel value.

Inventors

  • 👤 Nicholas P. Greco
  • 👤 David A. Webb

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-08 21:05
CPC Classifications
B; B27; B27K; B27K3/00; B27K3/34; B27K3/44; A; A01; A01N; A01N61/00; A01N61/02; C; C10; C10C; C10C1/00; C10C1/20

Claims Analysis

Total Claims: 19
Claim 1
Independent Claim 124 words
A method of preparing an improved creosote wood preservative, having a lighter color and reduced tendency for formation of a crud deposit on treated wood, from a coal tar creosote comprising: a. distilling the coal tar creosote to an end temperature equivalent to a temperature in the range of 395° - 410°C at atmospheric pressure to produce a distillate and a pitch residue, and b. contacting the distillate with at least 1% by weight of a caustic compound selected from the group consisting of alkali metal alcoholates and alkali metal hydroxides and mixtures of alkali metal alcoholates and hydroxides at a temperature in the range from the melting temperature to the boiling temperature of the creosote whereby an improved creosote wood preservative is produced.
Claim 2
Independent Claim 124 words
A method of preparing an improved creosote wood preservative, having a lighter color and reduced tendency for formation of a crud deposit on treated wood, from a coal tar creosote comprising: a. distilling the coal tar creosote to an end temperature equivalent to a temperature in the range of 395° - 410°C at atmospheric pressure to produce a distillate and a pitch residue, and b. contacting the distillate with at least 1% by weight of a caustic compound selected from the group consisting of alkali metal alcoholates and alkali metal hydroxides and mixtures of alkali metal alcoholates and hydroxides at a temperature in the range from the melting temperature to the boiling temperature of the creosote whereby an improved creosote wood preservative is produced.
Claim 3
Dependent Claim 27 words
A method according to claim 1 wherein the coal tar creosote is distilled at a temperature of 300°C at a reduced pressure around 60 mm of mercury.
Claim 4
Dependent Claim 40 words
A method according to claim 1, wherein the coal tar creosote is refluxed to a temperature in the range of 250°C - 320°C at atmospheric pressure for a residence time of 5 - 60 minutes before the creosote is distilled.
Claim 5
Dependent Claim 14 words
A method according to claim 1 which includes recovering the pitch residue from distillation.
Claim 6
Dependent Claim 37 words
A method according to claim 1 which includes: a. adding a correction oil to the distillate before the distillate is contacted with the caustic compounds whereby anthracene, phenanthrene and carbazole are maintained in solution at low temperatures.
Claim 7
Dependent Claim 31 words
A method according to claim 1, which includes: a. adding a correction oil to the improved creosote wood preservative whereby anthracene, phenanthrene and carbazole are maintained in solution at low temperatures.
Claim 8
Dependent Claim 15 words
A method according to claim 1 wherein sodium methylate is used as the caustic compound.
Claim 9
Dependent Claim 15 words
A method according to claim 1 wherein sodium hydroxide is used as the caustic compound.
Claim 10
Dependent Claim 19 words
A method according to claim 1 which includes removing dissolved phenolate salts present in the improved creosote wood preservative.
Claim 11
Dependent Claim 19 words
A method according to claim 1 which includes removing anthracene, phenanthrene and carbazole from the improved creosote wood preservative.
Claim 12
Independent Claim 144 words
A method of preparing an improved creosote wood preservative having a lighter color and reduced tendency for formation of crud deposit on treated wood from a coal tar creosote comprising: a. refluxing the coal tar creosote to a temperature in the range of 250°-320°C at atmospheric pressure for a residence time of 5 - 60 minutes b. distilling the refluxed creosote to an end temperature of 300°C at a reduced pressure around 60 mm of mercury to produce a distillate and a pitch residue, and c. contacting the distillate with at least 1% by weight of a caustic compound selected from the group consisting of alkali metal alcoholates, alkali metal hydroxides and mixtures of alkali metal alcoholates and hydroxides at a temperature in the range from the melting temperature to the boiling temperature of the creosote whereby an improved creosote wood preservative is produced.
Claim 13
Independent Claim 144 words
A method of preparing an improved creosote wood preservative having a lighter color and reduced tendency for formation of crud deposit on treated wood from a coal tar creosote comprising: a. refluxing the coal tar creosote to a temperature in the range of 250°-320°C at atmospheric pressure for a residence time of 5 - 60 minutes b. distilling the refluxed creosote to an end temperature of 300°C at a reduced pressure around 60 mm of mercury to produce a distillate and a pitch residue, and c. contacting the distillate with at least 1% by weight of a caustic compound selected from the group consisting of alkali metal alcoholates, alkali metal hydroxides and mixtures of alkali metal alcoholates and hydroxides at a temperature in the range from the melting temperature to the boiling temperature of the creosote whereby an improved creosote wood preservative is produced.
Claim 14
Dependent Claim 36 words
A method according to claim 11 which includes adding a correction oil to the distillate before the distillate is contacted with the caustic compound whereby anthracene, phenanthrene and carbazole are maintained in solution at low temperatures.
Claim 15
Dependent Claim 30 words
A method according to claim 11 which includes adding a correction oil to the improved creosote wood preservative whereby anthracene, phenanthrene and carbazole are maintained in solution at low temperatures.
Claim 16
Dependent Claim 19 words
A method according to claim 11 which includes removing dissolved phenolate salts present in the improved creosote wood preservative.
Claim 17
Dependent Claim 19 words
A method according to claim 11 which includes removing anthracene, phenanthrene and carbazole from the improved creosote wood preservative.
Claim 18
Dependent Claim 15 words
A method according to claim 11 wherein sodium methylate is used as the caustic compound.
Claim 19
Dependent Claim 15 words
A method according to claim 11 wherein sodium hydroxide is used as the caustic compound.

References Cited (Backward Citations)

US2040100A Cited
US2044764A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1979-06-01 1979-12-01 1980-06-01 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1983-06-01 1983-12-01 1984-06-01 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1987-06-01 1987-12-01 1988-06-01 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag