Patent US3954577A successfully refreshed from Google Patents.
← Back to Patent Explorer
US3954577A Expired / Lapsed US ⏱️ 0.0 years remaining

Electrochemical preparation of aluminum bromide

Assignee: Texaco Inc
•
Filing: 1974-11-27
•
Granted: 1976-05-04
•
Expires: 1994-11-27
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract Aluminum bromide is prepared by an electrochemical process in a cell with an aluminum anode, employing as the electrolyte, a solution of hydrogen bromide in an aprotic solvent capable of dissolving both hydrogen bromide and aluminum bromide. After initiation of the reaction with an electric current, the reaction proceeds without additional electrical power. The product is a solution of aluminum bromide and may also include solid aluminum bromide if the amount produced exceeds the solubility limit of the solvent.

Inventors

  • 👤 Stephen A. Levine

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-06 13:31
CPC Classifications
C; C25; C25B; C25B1/00; C25B1/01; C25B1/24

Claims Analysis

Total Claims: 19
Claim 1
Independent Claim 82 words
An electrolytic process for the preparation of aluminum bromide which comprises providing an electrochemical cell with an aluminum anode, a cathode which is not attacked by hydrogen bromide, aluminum bromide or bromine and an electrolyte consisting essentially of hydrogen bromide in a solvent capable of dissolving hydrogen bromide and aluminum bromide, said electrolyte having below 100 ppm of water, and passing an electric current through the cell in order to initiate a reaction, whereby there is obtained a solution of aluminum bromide.
Claim 2
Dependent Claim 82 words
An electrolytic process for the preparation of aluminum bromide which comprises providing an electrochemical cell with an aluminum anode, a cathode which is not attacked by hydrogen bromide, aluminum bromide or bromine and an electrolyte consisting essentially of hydrogen bromide in a solvent capable of dissolving hydrogen bromide and aluminum bromide, said electrolyte having below 100 ppm of water, and passing an electric current through the cell in order to initiate a reaction, whereby there is obtained a solution of aluminum bromide.
Claim 3
Dependent Claim 41 words
A process according to claim 1 wherein the electrolyte is a solution of hydrogen bromide in an aprotic solvent, said solvent having a boiling point above about 25° C and capable of dissolving at least 5% by weight of hydrogen bromide.
Claim 4
Dependent Claim 17 words
A process according to claim 2 in which the electrolyte is a saturated solution of hydrogen bromide.
Claim 5
Dependent Claim 12 words
A process according to claim 2 in which the solvent is dimethylformamide.
Claim 6
Dependent Claim 12 words
A process according to claim 2 in which the solvent is cyclohexane.
Claim 7
Dependent Claim 21 words
A process according to claim 1 in which the aluminum electrode is composed of at least 90% by weight of aluminum.
Claim 8
Dependent Claim 17 words
A process according to claim 6 in which the aluminum electrode is composed of substantially pure aluminum.
Claim 9
Dependent Claim 28 words
A process according to claim 1 in which the cathode is composed of a material selected from the group consisting of platinum, palladium, rhenium, graphite and glassy carbon.
Claim 10
Dependent Claim 14 words
A process according to claim 8 in which the cathode is composed of platinum.
Claim 11
Dependent Claim 97 words
An electrolytic process for the preparation of aluminum bromide which comprises providing an electrochemical cell with an aluminum anode composed of at least 90% by weight of aluminum, a cathode which is not attacked by hydrogen bromide, aluminum bromide or bromine, and an electrolyte comprising a solution of 5% or more by weight hydrogen bromide in an aprotic solvent having a boiling point above 25° C., said electrolyte having below 100 ppm of water, and passing an electric current through the cell in order to initiate a reaction, whereby there is obtained a solution of aluminum bromide.
Claim 12
Dependent Claim 97 words
An electrolytic process for the preparation of aluminum bromide which comprises providing an electrochemical cell with an aluminum anode composed of at least 90% by weight of aluminum, a cathode which is not attacked by hydrogen bromide, aluminum bromide or bromine, and an electrolyte comprising a solution of 5% or more by weight hydrogen bromide in an aprotic solvent having a boiling point above 25° C., said electrolyte having below 100 ppm of water, and passing an electric current through the cell in order to initiate a reaction, whereby there is obtained a solution of aluminum bromide.
Claim 13
Dependent Claim 17 words
A process according to claim 10 in which the electrolyte is a saturated solution of hydrogen bromide.
Claim 14
Dependent Claim 23 words
A process according to claim 10 in which there is obtained a saturated solution of aluminum bromide and solid aluminum bromide as product.
Claim 15
Dependent Claim 134 words
An electrolytic process for the preparation of aluminum bromide which comprises the steps of (1) providing an electrochemical cell with an aluminum electrode composed of at least 90% by weight of aluminum, a platinum electrode and an electrolyte consisting essentially of at least 5% by weight of hydrogen bromide in an aprotic solvent capable of dissolving hydrogen bromide and aluminum bromide, said electrolyte having below 100 ppm of water, (2) initially making the aluminum electrode the cathode and the platinum electrode the anode, (3) passing an electric current through the cell in order to reduce any aluminum oxide on the surface of the aluminum electrode, (4) reversing the polarity of the electrodes, and (5) passing an electric current through the cell to initiate a reaction, whereby there is obtained a solution of aluminum bromide.
Claim 16
Dependent Claim 134 words
An electrolytic process for the preparation of aluminum bromide which comprises the steps of (1) providing an electrochemical cell with an aluminum electrode composed of at least 90% by weight of aluminum, a platinum electrode and an electrolyte consisting essentially of at least 5% by weight of hydrogen bromide in an aprotic solvent capable of dissolving hydrogen bromide and aluminum bromide, said electrolyte having below 100 ppm of water, (2) initially making the aluminum electrode the cathode and the platinum electrode the anode, (3) passing an electric current through the cell in order to reduce any aluminum oxide on the surface of the aluminum electrode, (4) reversing the polarity of the electrodes, and (5) passing an electric current through the cell to initiate a reaction, whereby there is obtained a solution of aluminum bromide.
Claim 17
Dependent Claim 28 words
A process according to claim 13 wherein the electrolyte is a saturated solution of hydrogen bromide in a aprotic solvent having a boiling point above about 25° C.
Claim 18
Dependent Claim 17 words
A process according to claim 14 in which the aluminum electrode is composed of substantially pure aluminum.
Claim 19
Dependent Claim 12 words
A process according to claim 14 in which the solvent is dimethylformamide.

References Cited (Backward Citations)

US3113911A Cited
US3240687A Cited
US3330746A Cited
US3347761A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1979-05-04 1979-11-03 1980-05-04 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1983-05-04 1983-11-03 1984-05-04 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1987-05-04 1987-11-03 1988-05-04 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag