Abstract

Abstract Anode shields are provided around the anode baskets in an electroforming process.

Inventors

  • 👤 Ramon D. Vanderveer
  • 👤 William P. Dugan

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-02 12:47
CPC Classifications
H; H05; H05K; H05K3/00; H05K3/22; H05K3/24; H05K3/241; C; C25; C25D; C25D1/00; C25D21/00; C25D21/12; H05K3/40; H05K3/4092; Y; Y10; Y10S; Y10S204/00; Y10S204/07

Claims Analysis

Total Claims: 8
Claim 1
Independent Claim 99 words
A method of electroforming nickel on a printed circuit board comprising the steps of: providing a bath of sulfamate nickel plating solution; immersing a printed circuit board cathode in the plating solution; immersing a titanium wire anode basket containing nickel chips in the plating solution in an operational relationship to the cathode; shielding the anode in a non-conductive plastic shield having a plurality of openings disposed in a predetermined pattern on the surface of said shield facing the cathode; and passing a current through said anode to electrodeposit nickel from said nickel chips on said printed circuit board cathode.
Claim 2
Independent Claim 99 words
A method of electroforming nickel on a printed circuit board comprising the steps of: providing a bath of sulfamate nickel plating solution; immersing a printed circuit board cathode in the plating solution; immersing a titanium wire anode basket containing nickel chips in the plating solution in an operational relationship to the cathode; shielding the anode in a non-conductive plastic shield having a plurality of openings disposed in a predetermined pattern on the surface of said shield facing the cathode; and passing a current through said anode to electrodeposit nickel from said nickel chips on said printed circuit board cathode.
Claim 3
Independent Claim 119 words
A method of electroforming nickel on a printed circuit board comprising the steps of: providing a bath of sulfamate nickel plating solution; immersing a printed circuit board cathode in the plating solution; immersing a first titanium wire anode basket containing nickel chips in the plating solution on one side of the cathode; immersing a second titanium wire anode basket containing nickel chips in the plating solution on the opposed side of the cathode; shielding the anodes in non-conductive plastic shields having a plurality of openings disposed in a predetermined pattern on the surface of said shields facing the cathode; and passing a current through the anode to electrodeposit nickel from said nickel chips on said printed circuit board cathode.
Claim 4
Independent Claim 119 words
A method of electroforming nickel on a printed circuit board comprising the steps of: providing a bath of sulfamate nickel plating solution; immersing a printed circuit board cathode in the plating solution; immersing a first titanium wire anode basket containing nickel chips in the plating solution on one side of the cathode; immersing a second titanium wire anode basket containing nickel chips in the plating solution on the opposed side of the cathode; shielding the anodes in non-conductive plastic shields having a plurality of openings disposed in a predetermined pattern on the surface of said shields facing the cathode; and passing a current through the anode to electrodeposit nickel from said nickel chips on said printed circuit board cathode.
Claim 5
Dependent Claim 46 words
The method of claim 2 wherein the openings in the first anode shield are substantially greater than the openings in the second anode shield to electroform a greater thickness of nickel on the first anode side of said cathode than on the second anode side thereof.
Claim 6
Independent Claim 234 words
A method of electroforming nickel on a printed circuit board comprising the steps of: providing a bath of sulfamate nickel plating solution; immersing a printed circuit board cathode having a redundant circuit side and an opposed true circuit side in the plating solution; immersing a first titanium wire anode basket containing nickel chips in the plating solution on the redundant circuit side of the cathode; immersing a second titanium wire anode basket containing nickel chips in the plating solution on the true circuit side of the cathode; shielding the first anode basket in a first non-conductive plastic anode shield having four substantially flat surfaces disposed around and substantially enclosing said first anode basket, said first anode shield having a plurality of vertically extending rectangular openings disposed in a predetermined pattern on the one flat surface of said first shield facing the redundant circuit side of the cathode; shielding the second anode basket in a second non-conductive plastic anode shield having four substantially flat surfaces disposed around and substantially enclosing said second anode basket, said second anode shield having a plurality of spaced circular openings disposed in a predetermined pattern on the one flat surface of said second anode shield facing the true circuit side of the cathode; and passing a current through the anodes to electrodeposit nickel on both the redundant circuit side and the true circuit side of said printed circuit board cathode.
Claim 7
Independent Claim 234 words
A method of electroforming nickel on a printed circuit board comprising the steps of: providing a bath of sulfamate nickel plating solution; immersing a printed circuit board cathode having a redundant circuit side and an opposed true circuit side in the plating solution; immersing a first titanium wire anode basket containing nickel chips in the plating solution on the redundant circuit side of the cathode; immersing a second titanium wire anode basket containing nickel chips in the plating solution on the true circuit side of the cathode; shielding the first anode basket in a first non-conductive plastic anode shield having four substantially flat surfaces disposed around and substantially enclosing said first anode basket, said first anode shield having a plurality of vertically extending rectangular openings disposed in a predetermined pattern on the one flat surface of said first shield facing the redundant circuit side of the cathode; shielding the second anode basket in a second non-conductive plastic anode shield having four substantially flat surfaces disposed around and substantially enclosing said second anode basket, said second anode shield having a plurality of spaced circular openings disposed in a predetermined pattern on the one flat surface of said second anode shield facing the true circuit side of the cathode; and passing a current through the anodes to electrodeposit nickel on both the redundant circuit side and the true circuit side of said printed circuit board cathode.
Claim 8
Dependent Claim 50 words
The method of claim 4 wherein the openings in the first anode shield are substantially greater in flat surface area than the openings in the second anode shield to electroform a greater thickness of nickel on the redundant circuit side of said cathode than on the true circuit side thereof.

References Cited (Backward Citations)

CA519197A Cited
US2559926A Cited
US3429786A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1979-05-04 1979-11-03 1980-05-04 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1983-05-04 1983-11-03 1984-05-04 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1987-05-04 1987-11-03 1988-05-04 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag