Patent US3953922A successfully refreshed from Google Patents.
← Back to Patent Explorer
US3953922A Expired / Lapsed US ⏱️ 0.0 years remaining

Method of eliminating the training effect in superconducting coils by post-wind preload

Assignee: Energy Research and Development Administration ERDA
•
Filing: 1975-02-24
•
Granted: 1976-05-04
•
Expires: 1995-02-24
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract The training effect in superconducting coils is eliminated by winding the coil with a composite material that includes both a superconductor and a normal material and then applying stresses to the wound coil in the direction that electromagnetic stresses will be applied to the coil during normal use and in a magnitude greater than the calculated magnitude of the greatest electromagnetic stresses to be applied to the coil.

Inventors

  • 👤 Joseph R. Heim

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-09 11:20
CPC Classifications
H; H01; H01F; H01F6/00; H01F6/06; H01F41/00; H01F41/02; Y; Y10; Y10S; Y10S505/00; Y10S505/825; Y10S505/917; Y10S505/924; Y10T; Y10T29/00; Y10T29/49; Y10T29/49002; Y10T29/4902; Y10T29/49805

Claims Analysis

Total Claims: 8
Claim 1
Independent Claim 59 words
A method of conditioning a wound superconducting coil formed of a plurality of filaments of superconducting material in a matrix of normal conducting material comprising the step of: stressing the coil in the directions of the electromagnetic forces generated in normal use and in a magnitude greater than the magnitude of the maximum electromagnetic force generated in normal use.
Claim 2
Independent Claim 59 words
A method of conditioning a wound superconducting coil formed of a plurality of filaments of superconducting material in a matrix of normal conducting material comprising the step of: stressing the coil in the directions of the electromagnetic forces generated in normal use and in a magnitude greater than the magnitude of the maximum electromagnetic force generated in normal use.
Claim 3
Dependent Claim 47 words
The method of claim 1 wherein the step of stressing the coil comprises: inserting an expandable collet into the coil; expanding the expandable collet against the coil to strain the normal conducting material to a value of strain between 0.2% and 0.4%; and removing the expandable collet.
Claim 4
Dependent Claim 47 words
The method of claim 1 wherein the step of stressing the coil comprises: emplacing the coil in a coaxial annular cylinder; applying fluid pressure to the coaxial annular cylinder to compress the normal conducting material of the coil to a value of strain between 0.2% and 0.4%
Claim 5
Independent Claim 92 words
A method of preloading a wound superconducting solenoidal coil formed of a plurality of filaments of superconducting material in a matrix of normal conducting material comprising the steps of: placing a cylindrical mandrel coaxially within said coil, said cylindrical mandrel sized to make a close fit to said coil, said cylindrical mandrel of a material having a thermal coefficient of cubical expansion that is less than the thermal coefficient of cubical expansion of said normal conducting material; and cooling said coil containing said mandrel to cryogenic temperatures, whereby said coil is preloaded.
Claim 6
Independent Claim 92 words
A method of preloading a wound superconducting solenoidal coil formed of a plurality of filaments of superconducting material in a matrix of normal conducting material comprising the steps of: placing a cylindrical mandrel coaxially within said coil, said cylindrical mandrel sized to make a close fit to said coil, said cylindrical mandrel of a material having a thermal coefficient of cubical expansion that is less than the thermal coefficient of cubical expansion of said normal conducting material; and cooling said coil containing said mandrel to cryogenic temperatures, whereby said coil is preloaded.
Claim 7
Dependent Claim 12 words
The method of claim 4 wherein said mandrel is made of Invar.
Claim 8
Dependent Claim 22 words
The method of claim 5 wherein said step of cooling said coil comprises immersing said coil containing said mandrel in liquid nitrogen.

References Cited (Backward Citations)

US3023495A Cited
US3764401A Cited
US3859566A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1979-05-04 1979-11-03 1980-05-04 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1983-05-04 1983-11-03 1984-05-04 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1987-05-04 1987-11-03 1988-05-04 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag