Abstract

Abstract A process for refining smelted, silver-bearing residues (i.e. mattes) wherein as a first step oxygen or oxygen-enriched-air is injected into the molten matte to slag off base metal impurities and oxidize selenium and tellurium. In a second step oxidation is continued in the presence of a flux to reduce copper content of the thus-produced silver bullion to less than about 1% by weight.

Inventors

  • 👤 Tei Stewart Sanmiya
  • 👤 Derek George Kerfoot
  • 👤 Robert Ray Matthews

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-29 10:12
CPC Classifications
C; C22; C22B; C22B11/00; C22B11/02; C22B11/021; Y; Y02; Y02P; Y02P10/00; Y02P10/20

Claims Analysis

Total Claims: 3
Claim 1
Independent Claim 233 words
A PROCESS FOR RECOVERING VALUES FROM SILVER MATTE CONTAINING GREATER THAN ABOUT 50% BY WEIGHT OF SILVER, BASE METAL FROM THE GROUP CONSISTING OF COPPER, NICKEL, LEAD AND SMALL AMOUNTS OF GOLD AND PLATINUM GROUP METALS WITH UP TO ABOUT 30% BY WEIGHT OF AT LEAST ONE ELEMENT SELECTED FROM THE GROUP CONSISTING OF SELENIUM AND TELLURIUM, COMPRISING INJECTING A GAS SELECTED FROM THE GROUP CONSISTING OF OXYGEN AND AIR ENRICHED WITH OXYGEN TO AT LEAST ABOUT 50% BY VOLUME INTO SAID SILVER MATTE HELD MOLTEN AT A TEMPRATURE OF ABOUT 1.090*C TO ABOUT 1,260*C IN THE ABSENCE OF A FLUX TO OXIDIZE AND VOLITLIZE SELENIUM AND TELURIUM SO AS TO PROVIDE A MATTE CONTAINING AT MOST ABOUT 0.6% BY WEIGHT TOTAL SELENIUM AND TELLURIUM, RECOVERING AT LEAST ONE MATERIAL SELECTED FROM THE GROUP OF OXIDIZED SELENIUM AND TELLURIUM FROM THE GASEOUS EFFLUENT FROM SAID GAS INJECTION PROCESS, CONTINUING SAID GAS INJECTION PROCESS IN THE ABSENCE OF A FLUX UNTIL THE MATTE IS CONVERTED TO BULLION CONTAINING AT LEAST ABOUT 85% BY WEIGHT OF SILVER, SKIMMING ANY BASE-METAL SLAG FROM THE SURFACE OF THE MOLTEN BULLION, ADDING A BORAX-SLICA FLUX AND CONTINUING OXIDATION WHILE THE MOLTEN BULLION IS IN CONTRACT WITH SAID BORAX-SILICA FLUX UNTIL THE COPPER CONTENT OF THE BULLION IS LESS THAN 1% BY WEIGHT TO PROVIDE A SILVER RICH BULLION CONTAINING GOLD AND PLATINUM GROUP METALS AND SUITABLE FOR ELECTROREFINING.
Claim 2
Dependent Claim 233 words
A PROCESS FOR RECOVERING VALUES FROM SILVER MATTE CONTAINING GREATER THAN ABOUT 50% BY WEIGHT OF SILVER, BASE METAL FROM THE GROUP CONSISTING OF COPPER, NICKEL, LEAD AND SMALL AMOUNTS OF GOLD AND PLATINUM GROUP METALS WITH UP TO ABOUT 30% BY WEIGHT OF AT LEAST ONE ELEMENT SELECTED FROM THE GROUP CONSISTING OF SELENIUM AND TELLURIUM, COMPRISING INJECTING A GAS SELECTED FROM THE GROUP CONSISTING OF OXYGEN AND AIR ENRICHED WITH OXYGEN TO AT LEAST ABOUT 50% BY VOLUME INTO SAID SILVER MATTE HELD MOLTEN AT A TEMPRATURE OF ABOUT 1.090*C TO ABOUT 1,260*C IN THE ABSENCE OF A FLUX TO OXIDIZE AND VOLITLIZE SELENIUM AND TELURIUM SO AS TO PROVIDE A MATTE CONTAINING AT MOST ABOUT 0.6% BY WEIGHT TOTAL SELENIUM AND TELLURIUM, RECOVERING AT LEAST ONE MATERIAL SELECTED FROM THE GROUP OF OXIDIZED SELENIUM AND TELLURIUM FROM THE GASEOUS EFFLUENT FROM SAID GAS INJECTION PROCESS, CONTINUING SAID GAS INJECTION PROCESS IN THE ABSENCE OF A FLUX UNTIL THE MATTE IS CONVERTED TO BULLION CONTAINING AT LEAST ABOUT 85% BY WEIGHT OF SILVER, SKIMMING ANY BASE-METAL SLAG FROM THE SURFACE OF THE MOLTEN BULLION, ADDING A BORAX-SLICA FLUX AND CONTINUING OXIDATION WHILE THE MOLTEN BULLION IS IN CONTRACT WITH SAID BORAX-SILICA FLUX UNTIL THE COPPER CONTENT OF THE BULLION IS LESS THAN 1% BY WEIGHT TO PROVIDE A SILVER RICH BULLION CONTAINING GOLD AND PLATINUM GROUP METALS AND SUITABLE FOR ELECTROREFINING.
Claim 3
Dependent Claim 46 words
A process as in claim 1 wherein after base-metal slag is skimmed from said bullion, oxidation is carried out while the molten bullion is in contact with soda ash flux and, thereafter, the soda ash flux is removed prior to addition of the borax silica flux.

References Cited (Backward Citations)

US486613A Cited
US597139A Cited
US918908A Cited
US1004676A Cited
US2131072A Cited
US2218250A Cited
US2775509A Cited
US2948591A Cited
US2944886A Cited
US3249399A Cited
US3627486A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1978-09-01 1979-03-03 1979-09-02 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1982-09-01 1983-03-03 1983-09-02 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1986-09-01 1987-03-03 1987-09-02 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag