Patent US3943436A successfully refreshed from Google Patents.
Patent US3888966A successfully refreshed from Google Patents.
← Back to Patent Explorer
US3888966A Expired / Lapsed US ⏱️ 0.0 years remaining

Enhanced cobalt recovery from ammoniacally leached reduced ores using cyanide, hydrazine, or hydroxylamine compounds

Assignee: Freeport Minerals Co
•
Filing: 1972-06-02
•
Granted: 1975-06-10
•
Expires: 1992-06-02
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract In an ammoniacal leaching process for the recovery of nonferrous metals, the slurry of reduced ore and ammoniacal solution in the leaching-washing circuit is treated with nitrogenous compounds selected from the group consisting of hydrazine and soluble salts thereof, hydroxylamine and soluble salts thereof, hydrogen cyanide and soluble cyanide salts. These compounds enhance the solubilization of ore cobalt values into the liquid phase of the slurry, thereby enabling the recovery of additional amounts of cobalt which would otherwise be lost with the ore tailings.

Inventors

  • 👤 David James Miller

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-08 16:02
CPC Classifications
C; C22; C22B; C22B23/00; C22B23/04; C22B23/0407; C22B23/0446; C22B3/00; C22B3/20; C22B3/26; C22B3/33; Y; Y02; Y02P; Y02P10/00; Y02P10/20

Claims Analysis

Total Claims: 14
Claim 1
Independent Claim 175 words
IN A REDUCED AMMONICAL LEACHING PROCESS FOR THE RECOVERY OF NICKEL AND COBALT VALUES FROM AN ORE WHICH COMPRISES TREATING A SLURRY CONSISTING OF (A) A SOLID PHASE COMPRISING A REDUCED COBALT CONTAINING ORE AND (B) A LIQUID PHASE COMPRISING AN AQUEOUS AMMONICAL SOLUTION HAVING A PH ABOVE 7, WITH A GAS CONTAINING ELEMENTAL OXYGEN IN AT LEAST ONE LEACHING STAGE TO SOLUBILIZE NICKEL AND COBALT VALUES OF THE ORE IN THE LIQUID PHASE OF THE SLURRY, AND THEN WASHING THE SLURRY WITH AN AMMONIACAL WASHING SOLUTION IN AT LEAST ONE WASHING STAGE, WITHOUT PASSING A GAS CONTAINING ELEMENTAL OXYGEN THROUGH THE SLURRY DURING THE WASHING STAGE, TO RECOVER A PRODUCT LIQUOR CONTAINING THE SOLUBILIZED NICKEL AND COBALT VALUES: THE IMPROVEMENT FOR ENHANCHING THE SOLUBILITY OF THE COBALT VALUES OF THE ORE IN THE LIQUID PHASE OF THE SLURRY WHICH COMPRISES PROVIDING IN THE SLURRY, DURING THE WASHING STAGE, A NITROGENOUS COMPOUND SELECTED FROM THE GROUP CONSISTING OF HYDRAZINE AND A SOLUBLE SALT OF HYDRAZINE, WHEREIN THE AMOUNT OF THE COMPOUND IN THE SLURRY IS
Claim 2
Dependent Claim 175 words
IN A REDUCED AMMONICAL LEACHING PROCESS FOR THE RECOVERY OF NICKEL AND COBALT VALUES FROM AN ORE WHICH COMPRISES TREATING A SLURRY CONSISTING OF (A) A SOLID PHASE COMPRISING A REDUCED COBALT CONTAINING ORE AND (B) A LIQUID PHASE COMPRISING AN AQUEOUS AMMONICAL SOLUTION HAVING A PH ABOVE 7, WITH A GAS CONTAINING ELEMENTAL OXYGEN IN AT LEAST ONE LEACHING STAGE TO SOLUBILIZE NICKEL AND COBALT VALUES OF THE ORE IN THE LIQUID PHASE OF THE SLURRY, AND THEN WASHING THE SLURRY WITH AN AMMONIACAL WASHING SOLUTION IN AT LEAST ONE WASHING STAGE, WITHOUT PASSING A GAS CONTAINING ELEMENTAL OXYGEN THROUGH THE SLURRY DURING THE WASHING STAGE, TO RECOVER A PRODUCT LIQUOR CONTAINING THE SOLUBILIZED NICKEL AND COBALT VALUES: THE IMPROVEMENT FOR ENHANCHING THE SOLUBILITY OF THE COBALT VALUES OF THE ORE IN THE LIQUID PHASE OF THE SLURRY WHICH COMPRISES PROVIDING IN THE SLURRY, DURING THE WASHING STAGE, A NITROGENOUS COMPOUND SELECTED FROM THE GROUP CONSISTING OF HYDRAZINE AND A SOLUBLE SALT OF HYDRAZINE, WHEREIN THE AMOUNT OF THE COMPOUND IN THE SLURRY IS
Claim 3
Dependent Claim 195 words
In a reduced ammoniacal leaching process for the recovery of nickel and cobalt values from an ore which comprises treating a slurry consisting of (a) a solid phase comprising a reduced cobalt containing ore and (b) a liquid phase comprising an aqueous ammoniacal solution having a pH above 7, with a gas containing elemental oxygen in at least one leaching stage to solubilize nickel and cobalt values of the ore in the liquid phase of the slurry, and then washing the slurry with an ammoniacal washing solution in at least one washing stage, without passing a gas containing elemental oxygen through the slurry during the washing stage, to recover a product liquor containing the solubilized nickel and cobalt values: the improvement for enhancing the solubility of the cobalt values of the ore in the liquid phase of the slurry which comprises providing in the slurry, during the washing stage, a nitrogenous compound selected from the group consisting of hydroxylamine and a soluble salt of hydroxylamine, wherein the amount of compound in the slurry is sufficient to provide a hydroxylamine content, expressed as NH2OH, of from about 0.01 to 10% of the total weight of slurry.
Claim 4
Dependent Claim 195 words
In a reduced ammoniacal leaching process for the recovery of nickel and cobalt values from an ore which comprises treating a slurry consisting of (a) a solid phase comprising a reduced cobalt containing ore and (b) a liquid phase comprising an aqueous ammoniacal solution having a pH above 7, with a gas containing elemental oxygen in at least one leaching stage to solubilize nickel and cobalt values of the ore in the liquid phase of the slurry, and then washing the slurry with an ammoniacal washing solution in at least one washing stage, without passing a gas containing elemental oxygen through the slurry during the washing stage, to recover a product liquor containing the solubilized nickel and cobalt values: the improvement for enhancing the solubility of the cobalt values of the ore in the liquid phase of the slurry which comprises providing in the slurry, during the washing stage, a nitrogenous compound selected from the group consisting of hydroxylamine and a soluble salt of hydroxylamine, wherein the amount of compound in the slurry is sufficient to provide a hydroxylamine content, expressed as NH2OH, of from about 0.01 to 10% of the total weight of slurry.
Claim 5
Dependent Claim 199 words
In a reduced ammoniacal leaching process for the recovery of nickel and cobalt values from an ore which comprises treating a slurry consisting of (a) a solid phase comprising a reduced cobalt containing ore and (b) a liquid phase comprising an aqueous ammoniacal solution having a pH above 7, with a gas containing elemental oxygen in at least one leaching stage to solubilize nickel and cobalt values of the ore in the liquid phase of the slurry, and then washing the slurry with an ammoniacal washing solution in at least one washing stage, without passing a gas containing elemental oxygen through the slurry during the washing stage, to recover a product liquor containing the solubilized nickel and cobalt values: the improvement for enhancing the solubility of the cobalt values of the ore in the liquid phase of the slurry which comprises providing in the slurry, during the washing stage, a nitrogenous compound selected from the group consisting of hydrazine and a soluble salt of hydrazine, said compound being provided in an amount effective to enhance the solubility of the cobalt values of the ore in the liquid phase of the slurry, without subjecting the slurry to a reductive carbonylation.
Claim 6
Dependent Claim 199 words
In a reduced ammoniacal leaching process for the recovery of nickel and cobalt values from an ore which comprises treating a slurry consisting of (a) a solid phase comprising a reduced cobalt containing ore and (b) a liquid phase comprising an aqueous ammoniacal solution having a pH above 7, with a gas containing elemental oxygen in at least one leaching stage to solubilize nickel and cobalt values of the ore in the liquid phase of the slurry, and then washing the slurry with an ammoniacal washing solution in at least one washing stage, without passing a gas containing elemental oxygen through the slurry during the washing stage, to recover a product liquor containing the solubilized nickel and cobalt values: the improvement for enhancing the solubility of the cobalt values of the ore in the liquid phase of the slurry which comprises providing in the slurry, during the washing stage, a nitrogenous compound selected from the group consisting of hydrazine and a soluble salt of hydrazine, said compound being provided in an amount effective to enhance the solubility of the cobalt values of the ore in the liquid phase of the slurry, without subjecting the slurry to a reductive carbonylation.
Claim 7
Dependent Claim 199 words
In a reduced ammoniacal leaching process for the recovery of nickel and cobalt values from an ore which comprises treating a slurry consisting of (a) a solid phase comprising a reduced cobalt containing ore and (b) a liquid phase comprising an aqueous ammoniacal solution having a pH above 7, with a gas containing elemental oxygen in at least one leaching stage to solubilize nickel and cobalt values of the ore in the liquid phase of the slurry, and then washing the slurry with an ammoniacal washing solution in at least one washing stage, withhout passing a gas containing elemental oxygen through the slurry during the washing stage, to recover a product liquor containing the solubilized nickel and cobalt values: the improvement for enhancing the solubility of the cobalt values of the ore in the liquid phase of the slurry which comprises providing in the slurry, during the washing stage, a nitrogenous compound selected from the group consisting of hydroxylamine anD a soluble salt of hydroxylamine, said compound being provided in an amount effective to enhance the solubility of the cobalt values of the ore in the liquid phase of the slurry, without subjecting the slurry to a reductive carbonylation.
Claim 8
Dependent Claim 199 words
In a reduced ammoniacal leaching process for the recovery of nickel and cobalt values from an ore which comprises treating a slurry consisting of (a) a solid phase comprising a reduced cobalt containing ore and (b) a liquid phase comprising an aqueous ammoniacal solution having a pH above 7, with a gas containing elemental oxygen in at least one leaching stage to solubilize nickel and cobalt values of the ore in the liquid phase of the slurry, and then washing the slurry with an ammoniacal washing solution in at least one washing stage, withhout passing a gas containing elemental oxygen through the slurry during the washing stage, to recover a product liquor containing the solubilized nickel and cobalt values: the improvement for enhancing the solubility of the cobalt values of the ore in the liquid phase of the slurry which comprises providing in the slurry, during the washing stage, a nitrogenous compound selected from the group consisting of hydroxylamine anD a soluble salt of hydroxylamine, said compound being provided in an amount effective to enhance the solubility of the cobalt values of the ore in the liquid phase of the slurry, without subjecting the slurry to a reductive carbonylation.
Claim 9
Dependent Claim 191 words
In a reduced ammoniacal leaching process for the recovery of nickel and cobalt values from an ore which comprises treating a slurry consisting of (a) a solid phase comprising a reduced cobalt containing ore and (b) a liquid phase comprising an aqueous ammoniacal solution having a pH above 7, with a gas containing elemental oxygen in at least one leaching stage to solubilize nickel and cobalt values of the ore in the liquid phase of the slurry, and then washing the slurry with an ammoniacal washing solution in at least one washing stage, without passing a gas containing elemental oxygen through the slurry during the washing stage, to recover a product liquor containing the solubilized nickel and cobalt values: the improvement for enhancing the solubility of the cobalt values of the ore in the liquid phase of the slurry which comprises providing in the slurry, during the washing stage, a nitrogenous compound selected from the group consisting of hydrazine and a soluble salt of hydrazine, said compound being provided in an amount effective to enhance the solubility of the cobalt values of the ore in the liquid phase of the slurry.
Claim 10
Dependent Claim 191 words
In a reduced ammoniacal leaching process for the recovery of nickel and cobalt values from an ore which comprises treating a slurry consisting of (a) a solid phase comprising a reduced cobalt containing ore and (b) a liquid phase comprising an aqueous ammoniacal solution having a pH above 7, with a gas containing elemental oxygen in at least one leaching stage to solubilize nickel and cobalt values of the ore in the liquid phase of the slurry, and then washing the slurry with an ammoniacal washing solution in at least one washing stage, without passing a gas containing elemental oxygen through the slurry during the washing stage, to recover a product liquor containing the solubilized nickel and cobalt values: the improvement for enhancing the solubility of the cobalt values of the ore in the liquid phase of the slurry which comprises providing in the slurry, during the washing stage, a nitrogenous compound selected from the group consisting of hydrazine and a soluble salt of hydrazine, said compound being provided in an amount effective to enhance the solubility of the cobalt values of the ore in the liquid phase of the slurry.
Claim 11
Dependent Claim 53 words
The process of claim 5 wherein the washing step employs a plurality of countercurrent washing stages to counter-currently wash the slurry wherein the ammoniacal washing solution is first fed to the final washing stage, in which the nitrogenous compound is provided in the slurry by adding the compound to the ammoniacal washing solution.
Claim 12
Dependent Claim 191 words
In a reduced ammoniacal leaching process for the recovery of nickel and cobalt values from an ore which comprises treating a slurry consisting of (a) a solid phase comprising a reduced cobalt containing ore and (b) a liquid phase comprising an aqueous ammoniacal solution having a pH above 7, with a gas containing elemental oxygen in at least one leaching stage to solubilize nickel and cobalt values of the ore in the liquid phase of the slurry, and then washing the slurry with an ammoniacal washing solution in at least one washing stage, without passing a gas containing elemental oxygen through the slurry during the washing stage, to recover a product liquor containing the solubilized nickel and cobalt values: the improvement for enhancing the solubility of the cobalt values of the ore in the liquid phase of the slurry which comprises providing in the slurry, during the washing stage, a nitrogenous compound selected from the group consisting of hydroxylamine and a soluble salt of hydroxylamine, said compound being provided in an amount effective to enhance the solubility of the cobalt values of the ore in the liquid phase of the slurry.
Claim 13
Dependent Claim 191 words
In a reduced ammoniacal leaching process for the recovery of nickel and cobalt values from an ore which comprises treating a slurry consisting of (a) a solid phase comprising a reduced cobalt containing ore and (b) a liquid phase comprising an aqueous ammoniacal solution having a pH above 7, with a gas containing elemental oxygen in at least one leaching stage to solubilize nickel and cobalt values of the ore in the liquid phase of the slurry, and then washing the slurry with an ammoniacal washing solution in at least one washing stage, without passing a gas containing elemental oxygen through the slurry during the washing stage, to recover a product liquor containing the solubilized nickel and cobalt values: the improvement for enhancing the solubility of the cobalt values of the ore in the liquid phase of the slurry which comprises providing in the slurry, during the washing stage, a nitrogenous compound selected from the group consisting of hydroxylamine and a soluble salt of hydroxylamine, said compound being provided in an amount effective to enhance the solubility of the cobalt values of the ore in the liquid phase of the slurry.
Claim 14
Dependent Claim 53 words
The process of claim 7 wherein the washing step employs a plurality of countercurrent washing stages to counter-currently wash the slurry wherein the ammoniacal washing solution is first fed to the final washing stage, in which the nitrogenous compound is provided in the slurry by adding the compound to the ammoniacal washing solution.

References Cited (Backward Citations)

US911254A Cited
US1164141A Cited
US2621107A Cited
US2711956A Cited
US2902345A Cited
US2928732A Cited
US3141765A Cited
US3272738A Cited
US3403020A Cited
US3347662A Cited
US3437476A Cited
US3753686A Cited
US3684491A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1978-06-09 1978-12-09 1979-06-10 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1982-06-09 1982-12-09 1983-06-10 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1986-06-09 1986-12-09 1987-06-10 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag