Abstract
Abstract Flexing abrasion resistance and anti-fibrillation of acrylic synthetic fibers are improved by wet-spinning a solution of acrylonitrile polymer in an inorganic solvent through spinnerette orifices while maintaining the linear velocity ratio of the freeextrusion above 1 and the jet-stretch ratio above 1.5.
Inventors
- 👤 Mitsunori Sato
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-08 15:51
CPC Classifications
D; D01; D01F; D01F6/00; D01F6/02; D01F6/18; D01F6/28; D01F6/38
Claims Analysis
Total Claims: 3
Claim 1
Independent Claim
87 words
A METHOD OF PRODUCING ACRYLIC SYNTHETIC FIBERS WHICH COMPRISES EXTRUDING A SPINNING SOLUTION OF AN ACRYLONITRILE POLYMER CONTAINING AT LEAST 80 PERCENT BY WEIGHT OF COMBINED ACRYLONITRILE, DISSOLVED IN A RHODANIDE AS SOLVENT TO PRODUCE A SOLVENT CONCENTRATION OF 40-70 PERCENT BY WEIGHT, THROUGH SPINNERETTE ORIFICES INTO A COAGULATION BATH, CONTAINING A CONCENTRATION OF THE RHODANIDE WHICH IS 40-70 PERCENT OF THE CONCENTRATION OF THE RHODANIDE IN THE SPINNING SOLUTION, WHILE MAINTAINING A LINEAR VELOCITY RATIO OF THE FREE-EXTRUSION ABOVE 1 AND A JET-STREACH RATIO ABOVE 1.5.
Claim 2
Independent Claim
87 words
A METHOD OF PRODUCING ACRYLIC SYNTHETIC FIBERS WHICH COMPRISES EXTRUDING A SPINNING SOLUTION OF AN ACRYLONITRILE POLYMER CONTAINING AT LEAST 80 PERCENT BY WEIGHT OF COMBINED ACRYLONITRILE, DISSOLVED IN A RHODANIDE AS SOLVENT TO PRODUCE A SOLVENT CONCENTRATION OF 40-70 PERCENT BY WEIGHT, THROUGH SPINNERETTE ORIFICES INTO A COAGULATION BATH, CONTAINING A CONCENTRATION OF THE RHODANIDE WHICH IS 40-70 PERCENT OF THE CONCENTRATION OF THE RHODANIDE IN THE SPINNING SOLUTION, WHILE MAINTAINING A LINEAR VELOCITY RATIO OF THE FREE-EXTRUSION ABOVE 1 AND A JET-STREACH RATIO ABOVE 1.5.
Claim 3
Dependent Claim
43 words
The method as claimed in claim 1, wherein the fibers are removed from the coagulation bath and introduced into a second coagulation bath containing a concentration of the rhodanide which is 20-35 percent of the concentration of the rhodanide in the spinning solution.
References Cited (Backward Citations)
US2094099A
Cited
US2975024A
Cited
US3073669A
Cited
US3412191A
Cited
US3673053A
Cited
US3689621A
Cited
US3706828A
Cited
US3676540A
Cited
US3760053A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1978-05-19 | 1978-11-18 | 1979-05-20 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1982-05-19 | 1982-11-18 | 1983-05-20 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1986-05-19 | 1986-11-18 | 1987-05-20 | $7700.00 | Window Closed / Lapsed |