Abstract

Abstract The process of making a nailable, lightweight, fireproof and waterproof construction slab includes: A. COMBINING Portland cement, perlite, glass fiber, cellulose pulp, slaked lime and water to form an aqueous admixture, and B. FORMING AND CURING THE SLAB FROM SAID ADMIXTURE, SAID CURING INCLUDING SUBJECTING THE FORMED SLAB TO PRESSURIZATION TO SQUEEZE WATER THEREFROM.

Inventors

  • 👤 G Jakel

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-27 18:17
CPC Classifications
C; C04; C04B; C04B28/00; C04B28/02; C04B28/04; B; B28; B28B; B28B1/00; B28B1/08; B28B1/10; B28B11/00; B28B11/08; B28B11/10; B28B5/00; B28B5/02; B28B5/021; B28B5/022; B28B5/04

Claims Analysis

Total Claims: 10
Claim 1
Independent Claim 190 words
IN THE PROCESS OF MAKING A LIGHTWEIGHT, FREPROOF AND WATERPROOF CONSTRUCTION SLAB, HTE STEPS THAT INCLUDE: A. COMBINING PORTLAND CEMENT, PERILTE, GLASS FIBER, CELLULOSE PULP, A SUB-MIX AND WATER TO FORM AN AQUEOUS ADMIXTURE, AND B. FORMING THE CURING THE SLAB FROM SAID ADMIXTURE, SAID FORMING INCLUDING SUBJECTING THE FORMED SLAB TO PRESSURIZATION TO SQUEEZE WATER THEREFROM, C. SAID SUB-MIX HAVING BEEN PARELIMINARILY PREPARED BY COMBINING QUICK LIME AND WATER TO FORM A MIX REACTING EXOTHERMICALLY, AND ADDING FATTY MATERIAL TO THE REACTING MIX, AND IN THE RELATIVE AMOUNTS BETWEEN 45 AND 55 POUNDS OF QUICK LIME BETWEEN 25 AND 30 GALLONS OF WATER BETWEEN 1.5 AND 2.5 GALLONS OF FATTY MATERIAL D. THE CONSTITUENTS OF THE ADMIXTURE BEING PRESENT IN THE RELATIVE AMOUNT: BETWEEN ABOUT 180 AND 195 POUNDS OF CEMENT BETWEEN ABOUT 72 AND 90 POUNDS OF PERLITE BETWEEN ABOUT 38 AND 46 GALLONS OF AQUEOUS CELLULOSE PULP CONTAINING SAID GLASS FIBER, AND BETWEEN ABOUT 7 AND 9 GALLONS OF SAID SUB-MIX E. THE PULP AND GLASS FIBER BEING PRESENT IN THE RELATIVE AMOUNTS: BETWEEN 40 AND 48 POUNDS OF CELLULOSE BETWEEN AND 4 POUNDS OF GLASS FIBER.
Claim 2
Dependent Claim 190 words
IN THE PROCESS OF MAKING A LIGHTWEIGHT, FREPROOF AND WATERPROOF CONSTRUCTION SLAB, HTE STEPS THAT INCLUDE: A. COMBINING PORTLAND CEMENT, PERILTE, GLASS FIBER, CELLULOSE PULP, A SUB-MIX AND WATER TO FORM AN AQUEOUS ADMIXTURE, AND B. FORMING THE CURING THE SLAB FROM SAID ADMIXTURE, SAID FORMING INCLUDING SUBJECTING THE FORMED SLAB TO PRESSURIZATION TO SQUEEZE WATER THEREFROM, C. SAID SUB-MIX HAVING BEEN PARELIMINARILY PREPARED BY COMBINING QUICK LIME AND WATER TO FORM A MIX REACTING EXOTHERMICALLY, AND ADDING FATTY MATERIAL TO THE REACTING MIX, AND IN THE RELATIVE AMOUNTS BETWEEN 45 AND 55 POUNDS OF QUICK LIME BETWEEN 25 AND 30 GALLONS OF WATER BETWEEN 1.5 AND 2.5 GALLONS OF FATTY MATERIAL D. THE CONSTITUENTS OF THE ADMIXTURE BEING PRESENT IN THE RELATIVE AMOUNT: BETWEEN ABOUT 180 AND 195 POUNDS OF CEMENT BETWEEN ABOUT 72 AND 90 POUNDS OF PERLITE BETWEEN ABOUT 38 AND 46 GALLONS OF AQUEOUS CELLULOSE PULP CONTAINING SAID GLASS FIBER, AND BETWEEN ABOUT 7 AND 9 GALLONS OF SAID SUB-MIX E. THE PULP AND GLASS FIBER BEING PRESENT IN THE RELATIVE AMOUNTS: BETWEEN 40 AND 48 POUNDS OF CELLULOSE BETWEEN AND 4 POUNDS OF GLASS FIBER.
Claim 3
Dependent Claim 14 words
The method of claim 1 wherein the slab is formed as a tapered shingle.
Claim 4
Dependent Claim 10 words
The product slab formed by the process of claim 1.
Claim 5
Dependent Claim 12 words
The process of claim 1 wherein said fatty material consists of tallow.
Claim 6
Dependent Claim 21 words
The process of claim 1 wherein chloride salts of potassium and calcium and calcium nitrate are also combined in the admixture.
Claim 7
Dependent Claim 16 words
The product slab in the form of a shingle formed by the process of claim 1.
Claim 8
Dependent Claim 15 words
The process of claim 1 wherein an air entraining agent is combined in the admixture.
Claim 9
Dependent Claim 22 words
The process of claim 1 wherein the admixture also contains between 4 and 8 ounces of air entraining agent, in relative amount.
Claim 10
Dependent Claim 28 words
The process of claim 1 wherein the admixture also contains salts of copper and calcium, said salts consisting of chloride salts of copper and calcium and calcium nitrate.

References Cited (Backward Citations)

US1961525A Cited
US3137614A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1977-10-14 1978-04-15 1978-10-15 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1981-10-14 1982-04-15 1982-10-15 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1985-10-14 1986-04-15 1986-10-15 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag