Abstract

Abstract A copper backing is formed on a silver-cadmium oxide contact by first forming a bimetal strip having a thin layer of substantially pure silver and copper layer. The bimetal strip is secured at at least one end to a billet of the contact material, to retain them together during subsequent operations, with the silver surface of the bimetal strip against a surface of the billet of contact materials. The composite is then rolled to a substantial reduction of thickness, of the order of at least 50 percent, to bond the silver surface of the bimetal to the contact material. This produces a tri-layer contact with the layers fully integrated, consisting of the main contact material section, an intermediate silver layer and a copper backing layer.

Inventors

  • 👤 M Backstrom

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-01 09:49
CPC Classifications
H; H01; H01H; H01H11/00; H01H11/04; H01H11/06; H01H1/00; H01H1/02; H01H1/021; H01H1/023; H01H1/0231; Y; Y10; Y10T; Y10T29/00; Y10T29/49; Y10T29/49002; Y10T29/49117; Y10T29/49204; Y10T29/49208; Y10T29/4921

Claims Analysis

Total Claims: 5
Claim 1
Independent Claim 21 words
The process of claim 1 wherein the bimetal strip is welded at one end to the contact material prior to rolling.
Claim 2
Dependent Claim 20 words
The process of claim 1 wherein the cadmium oxide in the silver-cadmium oxide is up to about 50 weight percent.
Claim 3
Dependent Claim 18 words
The process of claim 3 wherein the cadmium oxide is about 2.5-15 weight percent of the contact material.
Claim 4
Dependent Claim 26 words
The process of claim 1 wherein the silver of the silver-copper bimetal is not more than 10 percent of the total thickness of the composite structure.
Claim 5
Dependent Claim 18 words
The process of claim 5 wherein the silver is 1-5 percent of the thickness of the composite structure.

References Cited (Backward Citations)

US3381364A Cited
US3355796A Cited
US3381365A Cited
US3462828A Cited
US3381366A Cited
US3462827A Cited
US3545067A Cited
US3392437A Cited
US3392436A Cited
US3616982A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1977-07-01 1977-12-31 1978-07-02 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1981-07-01 1981-12-31 1982-07-02 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1985-07-01 1985-12-31 1986-07-02 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag