Method of improving wire adhesion to rubber
Assignee: GILS G VAN
•
Filing: 1972-08-07
•
Granted: 1974-04-09
•
Expires: 1992-08-07
Abstract
Abstract A rubber bondable metal surface is pretreated by coating it with an organic oil mixture and rubbing it with a slightly abrasive material prior to adhering the treated metal to a natural or synthetic rubber. The adhering of the metal to rubber is accomplished by merely heating the rubber to bond it to the pretreated metal or by also adding a coating of adhesive between the pretreated metal and rubber and curing the composite to bond the adhesive contacting surfaces.
Inventors
- 👤 Gils G Van
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-05 22:35
CPC Classifications
C; C08; C08J; C08J5/00; C08J5/12; C08J2321/00
Claims Analysis
Total Claims: 2
Claim 1
Independent Claim
31 words
A method of pretreating a rubber bondable metal surface as set forth in Claim 1 wherein said steps of applying said mixture and abrading said metal surface are performed substantially simultaneously.
Claim 2
Dependent Claim
30 words
A method of pretreating a rubber bondable metal surface as set forth in claim 1 wherein the chlorothane in said mixture evaporates after said step of abrading said metal surface.
References Cited (Backward Citations)
No citation records indexed.
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1977-04-08 | 1977-10-08 | 1978-04-09 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1981-04-08 | 1981-10-08 | 1982-04-09 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1985-04-08 | 1985-10-08 | 1986-04-09 | $7700.00 | Window Closed / Lapsed |