Patent US3797495A successfully refreshed from Google Patents.
← Back to Patent Explorer
US3797495A Expired / Lapsed US ⏱️ 0.0 years remaining

Pressure sensitive adhesive tape and disposable diaper

Assignee: Kimberly Clark Corp
•
Filing: 1973-02-01
•
Granted: 1974-03-19
•
Expires: 1993-02-01
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract Pressure sensitive adhesive tape having a backsized, reinforced fibrous backing, a pigmented, plasticized polyvinyl chloride backsize, a release coat of silicone rubber, and an aggressively tacky adhesive of a block copolymer of isoprene and styrene tackified with a polyolefin and plasticized with an extended oil. Particular utility as a disposable diaper fastener is disclosed.

Inventors

  • 👤 G Schmidt

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-23 18:11
CPC Classifications
A; A61; A61F; A61F13/00; A61F13/15; A61F13/56; A61F13/58; Y; Y10; Y10T; Y10T428/00; Y10T428/28; Y10T428/2839

Claims Analysis

Total Claims: 9
Claim 1
Independent Claim 34 words
The tape of claim 1 wherein said backing has a basis weight in the range of 50 to 120 lbs./3,000 ft.2 and is saturated with 20 to 80 parts/100 parts fiber of polyacrylate binder.
Claim 2
Dependent Claim 20 words
The tape of claim 1 wherein said backing is a unified paper including Kraft fibers beater treated with acrylonitrile rubber.
Claim 3
Dependent Claim 31 words
The tape of claim 2 wherein said backsize coating comprises the following proportions of ingredients: 100 parts polyvinyl chloride, 50 to 150 parts polyacrylate, and 30 to 195 parts titanium dioxide.
Claim 4
Dependent Claim 41 words
The tape of claim 3 wherein said backsize further includes about 20 to 65 parts of a decorative pigment per 100 parts of resin and is applied in the amount of about 10 to 25 lbs. per 3, 000 sq. ft.
Claim 5
Dependent Claim 59 words
The tape of claim 4 wherein the adhesive is applied in the amount of about 0.8 to 1.8 oz. per square yard and comprises, in parts by weight: Block copolymer - 100 parts Polyolefin tackifier - 75 to 150 parts Antioxidant - 0.5 to 3.0 parts Naphthenic oil - 10 to 75 parts Filler - 0 to 50 parts
Claim 6
Dependent Claim 109 words
A diaper tape adapted for use as fasteners with disposable diapers of the type combining an absorbent pad with a fluid pervious cover and a fluid impervious thin film backing comprising, a reinforced fibrous backing, a backsize of from 10 to 20 lbs./3,000 sq. ft. of pigmented polyvinyl chloride plasticized with a polyacrylate on one side of said backing, a release coat of from 0.1 to 1.0 lbs./3,000 sq. ft. of catalyst-cured silicone rubber over said backsize, and an adhesive on the side of said backing opposite from said backsize and release coat, said adhesive comprising an aggressively tacky block copolymer of isoprene and styrene tackified with a polyolefin.
Claim 7
Dependent Claim 105 words
An improved disposable diaper of the type having an absorbent pad with a fluid-pervious cover, a fluid-impervious thin film backing, and pressure sensitive adhesive tape fastening means, the improvement wherein said pressure sensitive adhesive tape comprises, a reinforced fibrous backing, a backsize coating of polyvinyl chloride plasticized with a polyacrylate on one side of said backing, a release coating of catalyst-cured silicone rubber over said backsize, and an adhesive coating on the side of said backing opposite from said backsize and release coatings, said adhesive comprising an aggressively tacky block copolymer of isoprene and styrene tackified with a polyolefin, and extended with a naphthenic oil.
Claim 8
Dependent Claim 44 words
The diaper of claim 8 wherein said tape backsize coating is applied in the amount of about 10 to 25 lbs./3,000 ft.2 and comprises the following proportions of ingredients: 100 parts polyvinyl chloride, 50 to 150 parts polyacrylate, and 30 to 195 parts pigment.
Claim 9
Dependent Claim 62 words
The diaper of claim 9 wherein said tape adhesive is applied in the amount of from about 0.8 oz. to 1.8 oz. per square yard and comprises, in parts by weight: Block copolymer - 100 parts Polyolefin tackifier - 75 to 150 parts Antioxidant - 0.5 to 3.0 parts Naphthenic oil - 10 to 75 parts Filler - 0 to 50 parts

References Cited (Backward Citations)

US2607711A Cited
US3161533A Cited
US3068117A Cited
US3464848A Cited
US3740366A Cited
US3630201A Cited
US3625752A Cited
US3660323A Cited
US3681190A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1977-03-18 1977-09-17 1978-03-19 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1981-03-18 1981-09-17 1982-03-19 $3760.00 Window Closed / Lapsed