Patent EP0447639B1 successfully refreshed from Google Patents.
Patent US3676401A successfully refreshed from Google Patents.
← Back to Patent Explorer
US3676401A Expired / Lapsed US ⏱️ 0.0 years remaining

Environmentally disintegratable plastic compositions comprising copolymers of ethylene and carbon monoxide and a degradation accelerator

Assignee: Eastman Kodak Co
•
Filing: 1970-10-30
•
Granted: 1972-07-11
•
Expires: 1990-10-30
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract Compositions comprising (1) a copolymer of ethylene and 0.1 percent to 18 percent by weight of carbon monoxide, said percentage range being the proportion of carbon monoxide in the copolymer, and (2) an ultraviolet light degradable amount of an organometallic compound or salt of a common metal, e.g., ferricine, cobalt acetyl acetonate, etc., whereby film, articles of manufacture and especially packaging means, upon exposure to ultraviolet rays emitted by the sun are capable of accelerated deterioration thereby causing such materials including packaging means to decompose forming dust or flakes which may become embedded in the soil or carried away by rain water under those circumstances where they are thrown away out of doors so as to be exposed to natural environmental conditions.

Inventors

  • 👤 James William Henry

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-24 23:23
CPC Classifications
C; C08; C08K; C08K5/00; C08K5/04; C08K5/09; C08K5/098; B; B65; B65D; B65D65/00; B65D65/38; B65D65/46; B65D65/466; B65D81/00; B65D81/24; B65D81/30; C08G; C08G67/00; C08G67/02; C08K5/0008; C08K5/0033; C08K5/56; C08L; C08L23/00; C08L23/02; C08L23/04; C08L23/08; C08L23/0846; Y; Y10; Y10S; Y10S220/00; Y10S220/30; Y10S260/00; Y10S260/43; Y10S428/00; Y10S428/913

Claims Analysis

Total Claims: 14
Claim 1
Independent Claim 192 words
from about 0.001 percent to about 5 percent by weight based on total polymer weight of an organometallic compound selected from the group consisting of copper oxalate, nickel sebacate, metal salts of monocarboxylic acids of the formula R''COO wherein R'' is a hydrocarbon radical containing from one to 17 carbon atoms and the metal is selected from the group consisting of copper, cobalt, iron and nickel; metal acetylacetonate complexes of CH3COCH2OCOCH3 wherein the metal is selected from the group consisting of copper, cobalt, iron, manganese, chromium, vanadium and nickel; metal alkylacetoacetate complexes of CH3COCH2COOR'''' wherein the R'''' group contains from 2 to 20 carbons and the metal is selected from the group consisting of copper, cobalt, iron, manganese, nickel and zinc; metal complexes of N,N''-salicylidene ethylene diamine wherein the metal is selected from the group consisting of copper, cobalt, vanadium and manganese; metal 8-hydroxy quinolinates wherein the metal is selected from the group consisting of copper, cobalt, zinc, vanadium and manganese; chromic chloride complex with stearic or oleic acid; cobaltic chloride complex with oleic acid; and copper dust, said organometallic compound content being sufficient to accelerate degradation upon exposure to ultraviolet light.
Claim 2
Dependent Claim 15 words
The composition of claim 1 wherein the amount of carbon monoxide is about 6-12 percent.
Claim 3
Dependent Claim 52 words
The composition of claim 1 wherein the amount of carbon monoxide is sufficient whereby packaging means in the form of film or a molded article is capable of disintegration upon exposure to ultraviolet light emitted by the sun within a time period in the range between about 4 days and 2 weeks.
Claim 4
Dependent Claim 11 words
The composition of claim 1 wherein the organometallic compound is ferricine.
Claim 5
Dependent Claim 13 words
The composition of claim 1 wherein the organometallic compound is cobalt acetyl acetonate.
Claim 6
Dependent Claim 31 words
The composition of claim 2 containing about 1 percent by weight of cobalt acetyl acetonate and the amount of carbon monoxide is 8 percent based on the weight of the copolymer.
Claim 7
Dependent Claim 13 words
The composition of claim 1 wherein the sAlt is a salt of iron.
Claim 8
Dependent Claim 13 words
The composition of claim 1 wherein the salt is a salt of copper.
Claim 9
Dependent Claim 13 words
The composition of claim 1 wherein the salt is a salt of manganese.
Claim 10
Dependent Claim 15 words
The composition of claim 1 wherein the amount of carbon monoxide is about 0.5 percent.
Claim 11
Dependent Claim 15 words
The composition of claim 1 wherein the amount of carbon monoxide is about 1 percent.
Claim 12
Dependent Claim 15 words
The composition of claim 1 wherein the amount of carbon monoxide is about 6 percent.
Claim 13
Dependent Claim 15 words
The composition of claim 1 wherein the amount of carbon monoxide is about 8 percent.
Claim 14
Dependent Claim 15 words
The composition of claim 1 wherein the amount of carbon monoxide is about 12 percent.

References Cited (Backward Citations)

US2495286A Cited
US3274158A Cited
US3083184A Cited
GB1128793A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1975-07-11 1976-01-10 1976-07-11 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1979-07-11 1980-01-10 1980-07-11 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1983-07-11 1984-01-10 1984-07-11 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag