Process for electrowinning zinc from sulfide concentrates

Assignee: Kidd Creek Mines Ltd
•
Filing: 1969-05-19
•
Granted: 1972-04-11
•
Expires: 1989-05-19
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract This disclosure is directed to leaching zinc sulfide concentrates to facilitate the production of zinc and sulphur. solution. To provide for increased recovery the copper sulfate leach The zinc sulfide is leached with a copper sulfate solution, preferably under oxidizing conditions, to produce a copper sulfide and a zinc sulfate solution. The elemental sulphur can be obtained from the copper sulfide by a subsequent oxidizing leach and the zinc metal can be obtained by electrolyzing the zinc sulfate leach may be accomplished in a staging operation to establish an excess of zinc sulfide concentrate in the initial leach step.

Inventors

  • 👤 Howard C Renken
  • 👤 Theodoor W Zegers

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-01 20:26
CPC Classifications
C; C25; C25C; C25C1/00; C25C1/16

Claims Analysis

Total Claims: 7
Claim 1
Independent Claim 18 words
The process of claim 1 wherein the mole ratio of zinc to copper is from 2:1 to 1:2.
Claim 2
Dependent Claim 32 words
The process of claim 1 wherein the mole ratio of zinc to copper is 1:1 to 1:2 and the conversion of zinc sulfide to zinc sulfate is from 40 to 80 percent.
Claim 3
Dependent Claim 136 words
The process which comprises mixing zinc sulfide ore and copper sulfate solution and an oxygen containing gas in a first pressure leaching vessel, discharging the reaction mixture to a filtering means, withdrawing the pregnant solution from the filtering means and treating said pregnant solution in a purification and electrolysis means to produce zinc metal and a spent sulfuric acid electrolyte, charging said sulfuric acid, air and the solids from said filtering means to a second pressure leaching vessel, regenerating copper sulfate solution in said second leaching vessel, recycling said copper sulfate solution to said first pressure leaching vessel, discharging the residue from said second leaching vessel to a sulphur flotation means, withdrawing sulphur from said flotation means, withdrawing unreacted zinc sulfide from said flotation means and recycling said zinc sulfide to said first pressure leaching vessel.
Claim 4
Dependent Claim 22 words
The process of claim 1 in which the amount of oxygen in said first leaching vessel is about 20 to 100 psig.
Claim 5
Dependent Claim 30 words
The process of claim 1 wherein the ratio of zinc sulfide to copper sulfate in said first pressure leaching vessel is in excess of the molar quantities needed for reaction.
Claim 6
Dependent Claim 38 words
The process of claim 1 wherein the ratio of Zn to Cu iN said first pressure leaching vessel is 1:1 to 1:2 and the conversion of zinc sulfide to zinc sulfate therein is from 40 to 80 percent.
Claim 7
Dependent Claim 31 words
The process of claim 7 wherein the charge to said second leaching vessel is unreacted zinc sulfide, a copper sulfide, and about 1 mole of sulfuric acid per mole of copper.

References Cited (Backward Citations)

US1553414A Cited
US1890934A Cited
US1937634A Cited
US3095363A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1975-04-11 1975-10-11 1976-04-11 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1979-04-11 1979-10-11 1980-04-11 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1983-04-11 1983-10-11 1984-04-11 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag